# US 2018/0024161 A1 · Scanning probe microscope and method for measuring local electrical potential fields

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0024161 A1
- Document ID: US20180024161A1
- Status: Published application
- Kind: A1
- Application number: 15/550,036
- Filed: 2016-01-18
- Published: 2018-01-25
- Earliest claimed: 2015-02-13
- Assignees: Forschungszentrum Juelich GmbH
- Applicants: Forschungszentrum Juelich GmbH
- Inventors: Frank Stefan Tautz; Ruslan Temirov; Christian Wagner; Matthew Felix Blishen Green
- Web page: https://patentgrep.com/patent/US20180024161A1

## CPC

- G01Q 60/30: Scanning potential microscopy
- G01Q 60/42: Functionalisation
- G01Q: SCANNING-PROBE TECHNIQUES OR APPARATUS; APPLICATIONS OF SCANNING-PROBE TECHNIQUES, e.g. SCANNING PROBE MICROSCOPY [SPM]

## Abstract

A scanning probe microscope includes a tip. A quantum dot is applied to the tip.

## Claims

### Claim 1

A scanning probe microscope comprising:
a tip,
wherein a quantum dot is applied to the tip.

### Claim 2 (depends on 2)

The scanning probe microscope according to claim 2, wherein the quantum dot is a substance.

### Claim 3 (depends on 2)

The scanning probe microscope according to claim 2, wherein the substance is an organic, metal-organic, or inorganic substance.

### Claim 4 (depends on 2)

The scanning probe microscope according to claim 2, wherein the substance is a molecule or a spatially restricted arrangement of material.

### Claim 5 (depends on 4)

The scanning probe microscope according to claim 4, wherein the spatially restricted arrangement of material is ordered on an atomic or molecular level, or is not ordered.

### Claim 6 (depends on 4)

The scanning probe microscope according to claim 4, wherein the spatially restricted arrangement of material is a nanocrystal, an ordered or nonordered cluster, a nanotube, a carbon nanotube or a lithographic structure.

### Claim 7 (depends on 6)

The scanning probe microscope according to claim 6, wherein the nanocrystal is a metal cluster, a metal cluster having shells made of organic ligands, a doped or undoped semiconductor nanostructure, a nanowire or a nanocrystal or cluster made of molecules.

### Claim 8 (depends on 4)

The scanning probe microscope according to claim 4, wherein the molecule is an organic, bio-organic, inorganic, or metal-organic molecule.

### Claim 9 (depends on 1)

The scanning probe microscope according to claim 1, wherein the quantum dot is a device.

### Claim 10 (depends on 9)

The scanning probe microscope according to claim 9, wherein the device includes micro-scale or nano-scale electrodes and a material.

### Claim 11 (depends on 10)

The scanning probe microscope according to claim 10, wherein the material is a doped semiconductor, graphene, silicon, or a two-dimensional material.

### Claim 12 (depends on 9)

The scanning probe microscope according to claim 9, wherein the device is a lithographically structured material.

### Claim 13 (depends on 12)

The scanning probe microscope according to claim 12, wherein the device is integrated in the tip of the scanning probe microscope.

### Claim 14 (depends on 1)

The scanning probe microscope according to claim 1, wherein an electrically insulating layer or a chemical bond through which electrodes can tunnel is located between the quantum dot and the tip.

### Claim 15 (depends on 1)

The scanning probe microscope according to claim 1, wherein the scanning probe microscope is an atomic-force microscope.

### Claim 16

A method for measuring a local electrical potential field, the method comprising:
guiding a quantum dot is guided, by a tip to which it is applied to a site at which the local electrical potential field is measured, and
measuring a critical voltage at which a charge of the quantum dot changes.

### Claim 17 (depends on 16)

The method according to claim 16, wherein the quantum dot is guided, by the tip to which it is applied, to a reference site at which there is no local electrical potential field to be measured, and the critical voltage at which the charge of the quantum dot changes is measured, and in that, by comparing the critical voltages at the reference site and at the site at which the local electrical potential field is measured, the local electrical potential field at said site is measured.

### Claim 18 (depends on 16)

The method according to claim 16, wherein the local electrical potential field is measured quantitatively by way of the shielding factor, the gating efficiency, and the sensitivity factor.

### Claim 19 (depends on 16)

The method according to claim 16, wherein the measured local electrical potential field is calibrated by way of a known electrical potential field in a reference structure.

### Claim 20 (depends on 16)

The method according to claim 16, wherein an electrical memory element is read.

### Claim 21 (depends on 16)

The method according to claim 16, wherein the local electrical potential field is measured without contact.

### Claim 22 (depends on 16)

The method according to claim 16, wherein the local electrical potential field is measured above an insulating sample.

### Claim 23 (depends on 16)

The methods according to claim 16, wherein the charge change in the quantum dot is determined by way of a force change that is measured by measuring the frequency shift in the amplitude-modulated dynamic mode of an atomic-force microscope, by changing the cantilever deflection in the static mode of an atomic-force microscope, or by measuring the energy dissipation in the amplitude-modulated dynamic mode of an atomic-force microscope.

### Claim 24 (depends on 16)

The method according to claim 16, wherein two different charge changes in the quantum dot, the critical voltages of which are dependent on the distance between the tip and the sample surface to different extents, are measured in order to separate the topography signal from the electrical potential field signal.

### Claim 25 (depends on 16)

The method according to claim 16, wherein a two-dimensional or three-dimensional image of the local electrical potential field is taken by repeating the measurement at various points in the half-space above the sample surface.

### Claim 26 (depends on 16)

The method according to claim 16, wherein the applied voltage is adjusted to a fixed value close to the critical voltage at which the charge of the quantum dot changes, and the standard operating mode of an atomic-force microscope is used to produce an image while the half-space region to be investigated above the sample is scanned.

### Claim 27 (depends on 26)

The method according to claim 26, wherein there is a clear relationship between the atomic-force microscope signal and the critical voltage, and the atomic-force microscope signal is interpreted directly as a variation of the critical voltage.

### Claim 28 (depends on 26)

The method according to claim 26, wherein lines in a two-dimensional image, along which the change in the atomic-force microscope signal is greatest, are interpreted as lines of constant electrical potential.

### Claim 29 (depends on 26)

The method according to claim 26, wherein the set voltage is adjusted together with the distance between the tip and the sample surface according to the change in the critical voltage, and in that surfaces in a three-dimensional image, along which the change in the atomic-force microscope signal is greatest, are interpreted as surfaces of constant electrical potential.

### Claim 30 (depends on 16)

The method according to claim 16, wherein the applied voltage, as a manipulated variable, is held continuously at the critical value at which the charge of the quantum dot changes, while the half-space above the sample surface is scanned.

### Claim 31 (depends on 8)

The scanning probe microscope according to claim 8, wherein the molecule is a metal complex, a metallocene, an aromatic molecule, a condensed aromatic molecule, or an aliphatic molecule, or a derivative thereof, with or without a heteroatom.

### Claim 32 (depends on 8)

The scanning probe microscope according to claim 8, wherein the molecule is 3,4,9,10-perylenetetracarboxylic dianhydride.