# US 2018/0023705 A1 · Metal gasket

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0023705 A1
- Document ID: US20180023705A1
- Status: Published application
- Kind: A1
- Application number: 15/538,640
- Filed: 2015-12-03
- Published: 2018-01-25
- Earliest claimed: 2014-12-22
- Assignees: Nok Corporation
- Applicants: NOK Corporation
- Inventors: Takeshi WATANABE; Ryoko SAITO; Isao TANJI; Shinya NAKAOKA
- Web page: https://patentgrep.com/patent/US20180023705A1

## CPC

- F16J 15/064: {the packing combining the sealing function with other functions}
- F16J 15/08: with exclusively metal packing
- F16J 15/0818: {Flat gaskets}
- H05K 5/06: Hermetically-sealed casings {(specially adapted for small components H05K5/0095)}
- F16J 2015/085: {without fold over}
- F16J 2015/0856: {with a non-metallic coating or strip}
- F16J 2015/0868: {Aspects not related to the edges of the gasket}
- F16J: PISTONS {(specially adapted for dampers F16F9/32)}; CYLINDERS; SEALINGS
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS

## Abstract

The present invention addresses the problem of providing: a metal gasket capable of limiting the loss of axial bolt fastening force even if a peripheral creased section is formed as an anti-saline intrusion measure; and a metal gasket, which has relatively small curved sections with a radius of curvature of not more than 20 mm on the outer edge and which is capable of limiting loss of axial bolt fastening force even when a peripheral creased section is formed over the entire perimeter of the metal gasket as an anti-saline intrusion measure. Said problem is solved by a metal gasket, which is disposed between the abutting surfaces of two members and has, on a metal base plate: bolt holes into which bolts are inserted; a bead that is to the inside of the bolt holes and is for sealing between the abutting surfaces; and a peripheral creased section configured by bending the perimeter of the metal base plate in one direction so that no gap in which saline can accumulate is formed between the abutting surfaces. The peripheral creased section has areas formed by gradually changing bend length in the gasket circumferential direction so that loss of axial bolt fastening force when compressed by bolts is limited.

## Claims

### Claim 1

A metal gasket to be disposed between abutting surfaces of two members, the metal gasket comprising:
a metal base plate including a bolt hole through which a bolt is inserted, a bead section for sealing a space between the abutting surfaces on a more internal circumferential side than the bolt hole, and a peripheral creased section formed by folding a perimeter of the metal base plate in one direction to prevent formation of a gap in which saline accumulates between the abutting surfaces, wherein
the peripheral creased section includes a region with a folding length gradually changing in a gasket circumferential direction to suppress loss of a bolt fastening axial force in compression with the bolt, wherein the peripheral creased section is not formed in vicinity of the bolt hole, but formed in the perimeter of the metal base plate except the vicinity of the bolt hole.

### Claim 2

(canceled)

### Claim 3 (depends on 1)

The metal gasket according to claim 1, wherein the folding length of the peripheral creased section is formed to gradually change in the gasket circumferential direction to become shorter toward the vicinity of the bolt hole in which the peripheral creased section is not formed.

### Claim 4 (depends on 1)

The metal gasket according to claim 1, wherein, in the perimeter of the metal base plate in which the peripheral creased section is not formed, a recognition projection to recognize whether the gasket is attached is formed, the recognition projection extending outward and sideward from the space between the abutting surfaces.

### Claim 5 (depends on 1)

The metal gasket according to claim 1, wherein the folding length of the peripheral creased section falls within a range of 0.3 mm to 5.0 mm.

### Claim 6 (depends on 1)

The metal gasket of claim 1, wherein the peripheral creased section is formed over an entire perimeter of the metal base plate, and has the folding length and a folding height that are formed to gradually change in the gasket circumferential direction such that the folding length becomes longer and the folding height becomes shorter toward the bolt hole, and wherein an end edge on an internal circumferential side of the peripheral creased section is disposed to contact the bolt hole or extend across the bolt hole.

### Claim 7

(canceled)

### Claim 8 (depends on 6)

The metal gasket according to claim 6, wherein, in the peripheral creased section in vicinity of the bolt hole, a recognition projection to recognize whether the gasket is attached, the recognition projection extending outward and sideward from the space between the abutting surfaces.

### Claim 9 (depends on 1)

The metal gasket according to claim 1, further comprising:
at least one curved section with a radius of curvature of 20 mm or less in an outer edge of the metal base plate, wherein
the peripheral creased section is formed over an entire perimeter of the metal base plate, and has a folding width in vicinity of the curved section that gradually changes in the gasket circumferential direction.

### Claim 10 (depends on 9)

The metal gasket according to claim 9, wherein the folding width of the peripheral creased section is formed to gradually change in the gasket circumferential direction such that the folding width becomes wider toward the curved section from the outer edge of the metal base plate.

### Claim 11 (depends on 9)

The metal gasket according to claim 9 wherein the folding width of the peripheral creased section is formed to gradually change in the gasket circumferential direction such that the folding width becomes wider toward the bolt hole from the curved section of the metal base plate.

### Claim 12 (depends on 6)

The metal gasket according to claim 6 wherein the folding width of the peripheral creased section falls within a range of 0.3 mm to 30.0 mm.

### Claim 13 (depends on 1)

The metal gasket according to claim 1 wherein surfaces of the metal base plate are covered with a rubber-like elastic member.