# US 2018/0023348 A1 · Polycrstalline diamond structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0023348 A1
- Document ID: US20180023348A1
- Status: Published application
- Kind: A1
- Application number: 15/696,335
- Filed: 2017-09-06
- Published: 2018-01-25
- Earliest claimed: 2011-05-10
- Assignees: Element Six Abrasives S.A.
- Applicants: Element Six Abrasives S.A.
- Inventors: Nedret Can; Thembinkosi Shabalala
- Web page: https://patentgrep.com/patent/US20180023348A1

## CPC

- E21B 10/567: with preformed cutting elements mounted on a distinct support, e.g. polycrystalline inserts
- B24D 3/008: {Abrasive bodies without external bonding agent}
- B24D 3/34: characterised by additives enhancing special physical properties, e.g. wear resistance, electric conductivity, self-cleaning properties
- B24D 99/005: {Segments of abrasive wheels}
- E21B 10/55: with preformed cutting elements
- E21B 10/5735: {Interface between the substrate and the cutting element}
- E21C 35/183: with inserts or layers of wear-resisting material {(drill bits with wear-resistant parts E21B10/46)}
- E21C 35/1837: {characterised by the shape}
- E21B: EARTH OR ROCK DRILLING; OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR A SLURRY OF MINERALS FROM WELLS
- B24D: TOOLS FOR GRINDING, BUFFING OR SHARPENING (abrading-bodies specially designed for tumbling apparatus, e.g. abrading-balls B24B31/14; honing tools B24B33/08; lapping tools B24B37/11)
- E21C: MINING OR QUARRYING

## Abstract

A PCD structure comprises a first region and a second region adjacent the first region, the second region being bonded to the first region by intergrowth of diamond grains; the first region comprising a plurality of alternating strata or layers, each stratum or layer having a thickness in the range of around 5 to 300 microns. The second region comprises a plurality of strata or layers, one or more strata or layers in the second region having a thickness greater than the thicknesses of the individual strata or layers in the first region. The alternating layers or strata in the first region comprise first layers or strata alternating with second layers or strata, the first layers or strata being in a state of residual compressive stress and the second layers or strata being in a state of residual tensile stress.

## Claims

### Claim 1

A PCD structure comprising a first region and a second region adjacent the first region, the second region being bonded to the first region by intergrowth of diamond grains; the first region comprising a plurality of alternating strata or layers, each stratum or layer having a thickness in the range of around 5 to 300 microns; the second region comprising a plurality of strata or layers, one or more strata or layers in the second region having a thickness greater than the thicknesses of the individual strata or layers in the first region, wherein the alternating layers or strata in the first region comprise first layers or strata alternating with second layers or strata, the first layers or strata being in a state of residual compressive stress and the second layers or strata being in a state of residual tensile stress.

### Claim 2 (depends on 1)

A PCD structure according to claim 1, wherein each stratum or layer in the first region has a thickness in the range of around 30 to 300 microns.

### Claim 3 (depends on 1)

A PCD structure according to claim 1, wherein the strata or layers in the first region have a thickness or thicknesses in the range of around 30 to 200 microns.

### Claim 4

A PCD structure according to any one of the preceding claims, wherein the strata or layers in the second region have a thickness of greater than around 200 microns.

### Claim 5

A PCD structure according to any one of the preceding claims, wherein the first region comprises two or more different average diamond grain sizes.

### Claim 6

A PCD structure according to any one of the preceding claims, wherein the first region comprises three of more different average diamond grain sizes.

### Claim 7

A PCD structure comprising a first region and a second region adjacent the first region, the second region being bonded to the first region by intergrowth of diamond grains; the first region comprising a plurality of alternating strata or layers, each layer or stratum in the first region having a thickness in the range of around 5 to 300 microns; the first region comprising two or more different average diamond grain sizes.

### Claim 8

A PCD structure comprising a first region and a second region adjacent the first region, the second region being bonded to the first region by intergrowth of diamond grains; the first region comprising a plurality of alternating strata or layers, each stratum or layer having a thickness in the range of around 5 to 300 microns.

### Claim 9 (depends on 5, 6, 7, 8)

A PCD structure according to any one of claims 5 to 8, wherein each stratum or layer in the first and/or second region has a substantially uniform diamond grain size distribution throughout said stratum or layer.

### Claim 10

A PCD structure according to any one of the preceding claims, wherein the first region comprises an external working surface forming the initial working surface of the PCD structure in use.

### Claim 11 (depends on 7, 8, 9, 10)

A PCD structure according to any one of claims 7 to 10, wherein each stratum or layer in the first region has a thickness in the range of around 30 to 300 microns.

### Claim 12 (depends on 7, 8, 9, 10, 11)

A PCD structure according to any one of claims 7 to 11, wherein the second region has a thickness greater than the thickness of the individual strata or layers in the first region.

### Claim 13 (depends on 7, 8)

A PCD structure according to any one of claim 7 or 8, wherein the second region comprises a plurality of layers or strata.

### Claim 14 (depends on 13)

A PCD structure according to claim 13, wherein the layers or strata in the second region comprise diamond grains of a predetermined average grain size.

### Claim 15 (depends on 14)

A PCD structure according to claim 14, wherein the predetermined average grain size of the diamond grains in the second region is one of the average grain sizes of the diamond grains in the mix of diamond grains in the first region.

### Claim 16 (depends on 7, 8, 9, 10, 11, 12, 13, 14, 15)

A PCD structure according to any one of claims 7 to 15, wherein the alternating layers or strata comprise first layers or strata alternating with second layers or strata, the first layers or strata being in a state of residual compressive stress and the second layers or strata being in a state of residual tensile stress

### Claim 17

A PCD structure according to any one of the preceding claims, wherein the alternating layers or strata comprise first layers or strata alternating with second layers or strata, the first layers or strata being formed of a diamond mix having three or more different average diamond grain sizes and the second layers or strata being formed of a diamond mix having the same three or more average diamond grain sizes, wherein the first strata or layers in the first region have a different ratio of diamond grain sizes in said mix from the second strata or layers in the first region.

### Claim 18 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16)

A PCD structure according to any one of claims 1 to 16, wherein the alternating layers or strata comprise first layers or strata alternating with second layers or strata, the first layers or strata being formed of a diamond mix having a first average grain size or sizes and the second layers or strata being formed of a diamond mix having a second average grain size or sizes.

### Claim 19

A PCD structure according to any one of the preceding claims, wherein layers or strata in the first region and/or the second region comprise one or more of:
up to 20 wt % nanodiamond additions in the form of nanodiamond powder grains;
salt systems;
borides or metal carbides of at least one of Ti, V, or Nb; or
at least one of the metals Pd or Ni.

### Claim 20

A PCD structure according to any one of the preceding claims, wherein the PCD structure has a longitudinal axis, the layers or strata in the first region and/or the second region lying in a plane substantially perpendicular to the plane through which the longitudinal axis of the PCD structure extends.

### Claim 21

A PCD structure according to any one of the preceding claims, wherein the layers or strata are substantially planar, curved, bowed or domed.

### Claim 22 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17, 18, 19, 20)

A PCD structure according to any one of claims 1 to 20, wherein the PCD structure has a longitudinal axis, the layers or strata in the first region and/or the second region lying in a plane at an angle to the plane through which the longitudinal axis of the PCD structure extends.

### Claim 23

A PCD structure according to any one of the preceding claims, wherein the volume of the first region is greater than the volume of the second region.

### Claim 24

A PCD structure according to any one of the preceding claims, wherein one or more of the strata or layers intersect a working surface or side surface of the PCD structure.

### Claim 25

A PCD structure according to any one of the preceding claims, wherein each strata or layer is formed of one or more respective PCD grades having a TRS of at least 1,000 MPa; the PCD grade or grades in adjacent strata or layers having a different coefficient of thermal expansion (CTE).

### Claim 26 (depends on 25)

A PCD structure according to claim 25, wherein one or more of the strata or layers comprise a PCD grade or grades having a CTE of at least 3×10−6 mm/° C.

### Claim 27

A PCD element as claimed in any of the preceding claims, wherein at least a portion of the first region is substantially free of a catalyst material for diamond, said portion forming a thermally stable region.

### Claim 28 (depends on 27)

A PCD element as claimed in claim 27, wherein the thermally stable region extends a depth of at least 50 microns from a surface of the PCD structure.

### Claim 29 (depends on 27, 28)

A PCD element as claimed in any one of claim 27 or 28, wherein the thermally stable region comprising at most 2 weight percent of catalyst material for diamond.

### Claim 30

A PCD element for a rotary shear bit for boring into the earth, or for a percussion drill bit, comprising a PCD structure as claimed in any one of the preceding claims bonded to a cemented carbide support body.

### Claim 31 (depends on 30)

A drill bit or a component of a drill bit for boring into the earth, comprising a PCD element as claimed in claim 30.

### Claim 32

A PCD structure substantially as hereinbefore described with reference to any one embodiment as that embodiment is illustrated in the accompanying drawings.