# US 2018/0023211 A1 · Nanoparticle deposition in porous and on planar substrates

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0023211 A1
- Document ID: US20180023211A1
- Status: Published application
- Kind: A1
- Application number: 15/654,152
- Filed: 2017-07-19
- Published: 2018-01-25
- Earliest claimed: 2016-07-20
- Assignees: Trustees of Boston University
- Applicants: The Trustees of Boston University
- Inventors: Uday B. PAL; Soumendra BASU; Paul GASPER; Yanchen LU; Srikanth GOPALAN
- Web page: https://patentgrep.com/patent/US20180023211A1

## CPC

- C25D 17/10: Electrodes {, e.g. composition, counter electrode}
- C23C 14/0021: {Reactive sputtering or evaporation}
- C23C 14/02: Pretreatment of the material to be coated (C23C14/04 takes precedence)
- C23C 14/046: {Coating cavities or hollow spaces, e.g. interior of tubes; Infiltration of porous substrates}
- C23C 14/083: {of refractory metals or yttrium}
- C23C 14/18: on other inorganic substrates
- C23C 14/228: {Gas flow assisted PVD deposition}
- C25D 7/006: {Nanoparticles}
- H01M 4/8853: {Electrodeposition}
- H01M 4/8867: {Vapour deposition}
- H01M 4/8882: {Heat treatment, e.g. drying, baking}
- H01M 4/9066: {of metal-ceramic composites or mixtures, e.g. cermets}
- H01M 8/00: Fuel cells; Manufacture thereof
- H01M 2008/1293: {Fuel cells with solid oxide electrolytes}
- Y02E 60/50: Fuel cells
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method of preparing a metal nanoparticle on a surface includes subjecting a metal source to a temperature and a pressure in a carrier gas selected to provide a vapor metal species at a vapor pressure in the range of about 10−4 to about 10−11 atm; contacting the vapor metal species with a heated substrate; and depositing the metal as a nanoparticle on the substrate.

## Claims

### Claim 1

A method of preparing a metal nanoparticle in or on a surface comprising:
subjecting a metal source to a temperature and a pressure in a carrier gas selected to provide a vapor metal species at a vapor pressure in the range of about 10−4 to about 10−11 atm;
contacting the vapor metal species with a heated substrate; and
depositing the metal as a nanoparticle on the substrate.

### Claim 2 (depends on 1)

The method of claim 1, wherein the metal vapor species are deposited thermally as a nanoparticle.

### Claim 3 (depends on 1)

The method of claim 1, wherein the metal vapor species are deposited electrolytically as a nanoparticle.

### Claim 4 (depends on 1)

The method of claim 1, wherein the metal species comprises one or more of vaporized metal, metal oxyhydroxides and metal hydroxides.

### Claim 5 (depends on 1)

The method of claim 1, wherein the substrate is porous.

### Claim 6 (depends on 1)

The method of claim 1, wherein the carrier gas comprises water vapor.

### Claim 7 (depends on 2)

The method of claim 2, wherein thermally depositing comprises heating the metal source at a first higher temperature and maintaining the substrate at a second lower substrate, wherein the vapor metal species decompose on contacting the substrate to deposit the metal nanoparticles.

### Claim 8 (depends on 3)

The method of claim 3, wherein electrolytically depositing comprises applying a voltage at the substrate to reduce the vapor metal species to metal.

### Claim 9 (depends on 1)

The method of claim 1, wherein the substrate is a porous anode of a solid oxide fuel cell.

### Claim 10 (depends on 1)

The method of claim 1, wherein the substrate is a solid support of a heterogeneous catalyst.

### Claim 11

A method of depositing metal nanoparticles in a porous electrode of a solid oxide fuel cell, comprising:
heating a metal source to a first temperature selected to vaporize the metal source;
flowing a carrier gas over the heated metal source, wherein the carrier gas interacts with the vaporized metal and forms a metallic species gas phase having a vapor pressure in the range of about 10−4 to about 10−11 atm;
directing the metallic species gas towards a surface of a solid oxide fuel cell, wherein the surface comprises a porous electrode of the solid oxide fuel cell, and wherein the solid oxide fuel cell is independently heated to a second temperature that is less than the first temperature; and
decomposing the metallic species to deposit nanoparticles of the source metal.

### Claim 12 (depends on 11)

The method of claim 11, wherein the electrode is an anode.

### Claim 13 (depends on 12)

The method of claim 12, wherein the anode further comprises an electronic oxide or mixed electronic ionic conductor (MIEC).

### Claim 14 (depends on 12)

The method of claim 12, wherein the deposited metal has particle density in the range of 10 to 100 per μm2, and/or the TPB is in the range of 5-100 μm/μm3, and/or the particle volume is in the range of 0.1 to 10 nm3/nm2.

### Claim 15 (depends on 11)

The method of claim 11, wherein the nanoparticles deposit at the triple phase boundary of the porous electrode.

### Claim 16 (depends on 11)

The method of claim 11, further comprising:
prior to deposition, heating the solid oxide fuel cell under reducing conditions, wherein nickel oxide present in the anode is reduced to nickel.

### Claim 17 (depends on 16)

The method of claim 16, wherein the nanoparticles deposit within pores of the porous substrate.

### Claim 18 (depends on 16)

The method of claim 16, wherein the carrier gas comprises water vapor.

### Claim 19 (depends on 16)

The method of claim 16, wherein the metal nanoparticles deposit in an anode active layer (AAL).

### Claim 20

A method of depositing metal nanoparticles in a porous electrode of a solid oxide fuel cell, comprising:
heating a metal source to a first temperature selected to vaporize the metal source;
flowing a carrier gas over the heated metal source, wherein the carrier gas interacts with the vaporized metal and forms a metallic species gas phase having a vapor pressure in the range of about 10−4 to about 10−11 atm, wherein the metallic species comprises oxygen;
directing the metallic species gas towards a surface of a solid oxide fuel cell, wherein the surface comprises a porous electrode of the solid oxide fuel cell, and wherein the solid oxide fuel cell is independently heated to a second temperature that is selected to maintain the metallic species in the gas phase; and
applying an electric bias to the electrode to extract oxygen from the metallic species and to deposit the metal as nanoparticles.

### Claim 21 (depends on 20)

The method of claim 20, wherein the electrode is an anode.

### Claim 22 (depends on 21)

The method of claim 21, wherein the anode further comprises an electronic oxide or mixed electronic ionic conductor (MIEC).

### Claim 23 (depends on 22)

The method of claim 22, wherein the electronic oxide or mixed electronic ionic conductor (MIEC) is located in the anode active layer (AAL).

### Claim 24 (depends on 20)

The method of claim 20, wherein the deposited metal has particle density in the range of 10 to 100 per μm2, and/or the TPB is in the range of 5-100 μm/μm3, and/or the particle volume is in the range of 0.1 to 10 nm3/nm2.

### Claim 25 (depends on 20)

The method of claim 20, further comprising:
prior to deposition, heating the solid oxide fuel cell under reducing conditions, wherein nickel oxide present in the anode is reduced to nickel.

### Claim 26 (depends on 20)

The method of claim 20, wherein the metal nanoparticles deposit in an anode active layer (AAL).

### Claim 27 (depends on 20)

The method of claim 20, wherein the nanoparticles deposit at the triple phase boundary of the porous electrode.

### Claim 28

A solid oxide fuel cell, comprising:
a porous metal oxide cathode;
a metal oxide electrolyte; and
a porous nickel/electronic metal oxide anode, the anode comprising nickel-nanoparticles deposited at least at the triple phase boundary of the anode.

### Claim 29 (depends on 28)

The fuel cell of claim 28, wherein the anode further comprises an electronic oxide or mixed electronic ionic conductor (MIEC) in contact with the nickel nanoparticles.

### Claim 30 (depends on 29)

The fuel cell of claim 29, further comprising a layer of an electronic oxide over the nickel nanoparticles.