# US 2018/0023194 A1 · Process for coating an article and coating produced thereby

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0023194 A1
- Document ID: US20180023194A1
- Status: Published application
- Kind: A1
- Application number: 15/543,781
- Filed: 2015-11-03
- Published: 2018-01-25
- Earliest claimed: 2015-01-15
- Assignees: BOEHLERIT GmbH & Co.KG.
- Applicants: BOEHLERIT GmbH & Co.KG.
- Inventors: Reinhard PITONAK; Arno KOEPF; Ronald WEISSENBACHER
- Web page: https://patentgrep.com/patent/US20180023194A1

## CPC

- C23C 16/45523: {Pulsed gas flow or change of composition over time}
- C23C 16/0272: {Deposition of sub-layers, e.g. to promote the adhesion of the main coating}
- C23C 16/029: {Graded interfaces}
- C23C 16/34: Nitrides {(C23C16/303 takes precedence)}
- C23C 28/044: {coatings specially adapted for cutting tools or wear applications}
- C23C 28/048: {with layers graded in composition or physical properties}
- C23C 30/005: {on hard metal substrates}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

The invention relates to a process for coating an article (1), wherein a coating (2) having one or more coating layers (3, 4, 5) is applied to the article (1), wherein at least one coating layer (5) is formed essentially from aluminium, titanium and nitrogen, wherein the coating layer (5) has, at least in some regions, adjoining lamellae of different chemical composition and is deposited from a gas phase comprising at least one aluminium precursor and at least one titanium precursor. According to the invention, by setting a molar ratio of aluminium to titanium, the lamellae of different chemical composition are each formed with a cubic structure, it being possible for aluminium and titanium to be partly replaced by other metals and for nitrogen to be partly replaced by oxygen and/or carbon with retention of the cubic structure. The invention further relates to a correspondingly produced coating (2).

## Claims

### Claim 1

A method for coating an object (1), wherein a coating (2) having one or more coating layers (3, 4, 5) is applied to the object (1), wherein at least one coating layer (5) is formed essentially from aluminum, titanium and nitrogen, wherein the coating layer (5) comprises, at least in some regions, mutually adjoining lamellae of varying chemical composition and is deposited from a gas phase having at least one aluminum precursor and at least one titanium precursor, characterized in that, by adjustment of a molar ratio of aluminum to titanium, the lamellae of varying chemical composition are each formed with a cubic structure, wherein with the preservation of the cubic structure, aluminum and titanium can be partially replaced by other metals, and nitrogen can be partially replaced by oxygen and/or carbon.

### Claim 2 (depends on 1)

The method according to claim 1, characterized in that, for the deposition of the at least one coating layer (5) of essentially aluminum, titanium and nitrogen, a molar Al/Ti ratio in the gas phase is, at least temporarily, limited to maximally 3.0, preferably maximally 2.0, in particular maximally 1.5.

### Claim 3 (depends on 1)

The method according to claim 1, characterized in that the lamellae are deposited with a lamellar periodicity of less than 20 nm, preferably 3 nm to 17 nm, in particular 5 nm to 15 nm.

### Claim 4 (depends on 1)

The method according to claim 1, characterized in that the at least one coating layer (5) of essentially aluminum, titanium and nitrogen is deposited with an average composition of AlxTi1-xN and from a gas phase containing aluminum trichloride, titanium tetrachloride and ammonia.

### Claim 5 (depends on 4)

The method according to claim 4, characterized in that the at least one coating layer (5) of essentially aluminum, titanium and nitrogen is deposited with an average composition of AlxTi1-xN with 0.70≦x≦0.90, preferably 0.75≦x≦0.85.

### Claim 6 (depends on 1)

The method according to claim 1, characterized in that the at least one coating layer (5) of essentially aluminum, titanium and nitrogen is deposited at a pressure of 10 mbar to 80 mbar, in particular 20 mbar to 50 mbar.

### Claim 7 (depends on 1)

The method according to claim 1, characterized in that the at least one coating layer (5) of essentially aluminum, titanium and nitrogen is deposited at a temperature of approximately 750° C. to 850° C.

### Claim 8 (depends on 1)

The method according to claim 1, characterized in that the at least one coating layer (5) of essentially aluminum, titanium and nitrogen is deposited with a thickness of 1 μm to 20 μm, in particular 3 μm to 8 μm.

### Claim 9 (depends on 1)

The method according to claim 1, characterized in that the at least one coating layer (5) of essentially aluminum, titanium and nitrogen is deposited epitaxially.

### Claim 10 (depends on 1)

The method according to claim 1, characterized in that an object (1) made of a hard metal is coated, in particular a cutting insert such as an indexed cutting plate.

### Claim 11 (depends on 1)

The method according to claim 1, characterized in that, a multi-layer coating (2) is deposited on the object (1), wherein as a first coating layer (3) a bonding layer of TiN, preferably with a thickness of less than 1.0 μm, is deposited.

### Claim 12 (depends on 1)

The method according to claim 1, characterized in that the at least one coating layer (5) of essentially aluminum, titanium and nitrogen is deposited on a coating layer (4) of TiCN.

### Claim 13 (depends on 11)

The method according to claim 11, characterized in that, in the deposition of a first coating layer (3) and subsequent deposition of each additional coating layer (4, 5), a deposition temperature is respectively lowered or maintained.

### Claim 14 (depends on 1)

The method according to claim 1, characterized in that the at least one coating layer (5) of essentially aluminum, titanium and nitrogen is, preferably all coating layers (3, 4, 5) are, deposited by means of a CVD method.

### Claim 15

A coating (2) which is applied to an object (1) by means of a CVD method, wherein the coating (2) comprises one or more coating layers (3, 4, 5) and wherein at least one coating layer (5) is formed essentially from aluminum, titanium and nitrogen and, at least in some regions, comprises mutually adjoining lamellae of varying chemical composition, characterized in that the lamellae of varying chemical composition are each formed with a cubic structure, wherein with the preservation of the cubic structure, aluminum and titanium can be partially replaced by other metals, and nitrogen can be replaced by oxygen and/or carbon.

### Claim 16 (depends on 15)

The coating (2) according to claim 15, characterized in that the lamellae are formed with a lamellar periodicity of less than 20 nm, preferably 3 nm to 17 nm, in particular 5 nm to 15 nm.

### Claim 17 (depends on 15)

The coating (2) according to claim 15, characterized in that the at least one coating layer (5) of essentially aluminum, titanium and nitrogen has with an average composition of AlxTi1-xN with 0.70≦x≦0.90, preferably 0.75≦x≦0.85.

### Claim 18 (depends on 15)

The coating (2) according to claim 15, characterized in that the at least one coating layer (5) of essentially aluminum, titanium and nitrogen has a thickness of 1 μm to 20 μm, in particular 3 μm to 8 μm.

### Claim 19 (depends on 15)

The coating (2) according to claim 15, characterized in that the at least one coating layer (5) of essentially aluminum, titanium and nitrogen is grown epitaxially.

### Claim 20 (depends on 15)

The coating (2) according to claim 15, characterized in that the coating (2) has a multi-layer structure.

### Claim 21 (depends on 20)

The coating (2) according to claim 20, characterized in that a first coating layer (3) is provided as a bonding layer on the object (1), wherein the first coating layer (3) is preferably formed from TiN with a thickness of less than 1.0 μm.

### Claim 22 (depends on 20)

The coating according to claim 20, characterized in that the at least one coating layer (5) of essentially aluminum, titanium and nitrogen is deposited on a coating layer (4) of TiCN.

### Claim 23 (depends on 15)

An object (1), in particular a cutting tool such as a cutting plate, having a coating (2) according to claim 15.