# US 2018/0023182 A1 · Manufacturing method for deposition mask, metal plate used for producing deposition mask, and manufacturing method for said metal sheet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0023182 A1
- Document ID: US20180023182A1
- Status: Published application
- Kind: A1
- Application number: 15/548,897
- Filed: 2016-02-05
- Published: 2018-01-25
- Earliest claimed: 2015-02-10
- Assignees: Dai Nippon Printing Co., Ltd.
- Applicants: Dai Nippon Printing Co., Ltd.
- Inventors: Chikao IKENAGA; Hiroaki NAKAYAMA; Kazunari IKEDA; Chiaki HATSUTA; Utako OOUCHI
- Web page: https://patentgrep.com/patent/US20180023182A1

## CPC

- C23C 14/042: {using masks}
- C21D 1/74: Methods of treatment in inert gas, controlled atmosphere, vacuum or pulverulent material
- C21D 6/001: {containing Ni (C21D6/004 takes precedence)}
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C22C 38/40: with nickel
- C23C 14/04: Coating on selected surface areas, e.g. using masks
- C23C 14/58: After-treatment
- C23F 1/00: Etching metallic material by chemical means (manufacture of printing surfaces B41C; manufacture of printed circuits H05K)
- C23F 1/02: Local etching
- C23F 1/04: Chemical milling
- C23F 1/28: for etching iron group metals
- G01N 23/2273: Measuring photoelectron spectrum, e.g. electron spectroscopy for chemical analysis [ESCA] or X-ray photoelectron spectroscopy [XPS]
- H05B 33/10: Apparatus or processes specially adapted to the manufacture of electroluminescent light sources
- H10K 71/166: {using selective deposition, e.g. using a mask}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C23F: NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE (working metal by laser beams B23K26/00; desurfacing by applying flames B23K7/00; working of metal by electro-erosion B23H; producing decorative effects by removing surface material, e.g. by engraving, by etching, B44C1/22; electrolytic etching or polishing C25F); INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- H05B: ELECTRIC HEATING; ELECTRIC LIGHT SOURCES NOT OTHERWISE PROVIDED FOR; CIRCUIT ARRANGEMENTS FOR ELECTRIC LIGHT SOURCES, IN GENERAL
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES

## Abstract

The present invention provides a metal sheet, on a first surface of which a resist pattern having a narrow width can be stably provided. This manufacturing method for a metal sheet includes a preparation step of preparing a sheet material comprising an iron alloy that contains nickel. When a composition analysis of the first surface of the metal sheet obtained from the sheet material is performed using X-ray photoelectron spectroscopy, the ratio A1/A2 obtained by the result of the X-ray photoelectron spectroscopy does not exceed 0.4, where A1 is the sum of the peak area value of nickel oxide and the peak area value of nickel hydroxide, and A2 is the sum of the peak area value of iron oxide and the peak area value of iron hydroxide.

## Claims

### Claim at position 1

1-13. (canceled)

### Claim 14

A manufacturing method for a metal plate used for manufacturing a deposition mask having a plurality of through-holes formed therein, the method comprising a preparation step of preparing a plate member made of an iron alloy containing nickel,
wherein:
when a composition analysis of a first surface of the metal plate obtained from the plate member is performed by using an X-ray photoelectron spectroscopy, a ratio A1/A2 obtained by the result of the X-ray photoelectron spectroscopy is 0.4 or less, where A1 is a sum of a peak planar dimension value of nickel oxide and a peak planar dimension value of nickel hydroxide, and A2 is a sum of a peak planar dimension value of iron oxide and a peak planar dimension value of iron hydroxide; and
in the composition analysis of the first surface of the metal plate by means of the X-ray photoelectron spectroscopy, an incident angle of an X-ray emitted to the metal plate on the first surface is 45 degrees, and an acceptance angle of photoelectrons discharged from the metal plate is 90 degrees.

### Claim 15 (depends on 14)

The manufacturing method for a metal plate according to claim 14, further comprising an annealing step of annealing the plate member to obtain the metal plate.

### Claim 16 (depends on 15)

The manufacturing method for a metal plate according to claim 15, the plate member is annealed in the annealing step so that the ratio A1/A2 is 0.4 or less.

### Claim 17 (depends on 15)

The manufacturing method for a metal plate according to claim 15, wherein
the annealing step is performed in an irreducible atmosphere or an inert gas atmosphere.

### Claim 18 (depends on 15)

The manufacturing method for a metal plate according to claim 15, wherein
the annealing step is performed in an inert gas atmosphere including nitrogen gas.

### Claim 19 (depends on 14)

The manufacturing method for a metal plate according to claim 14, wherein
the preparation step includes a rolling step of rolling a base metal made of an iron alloy containing nickel.

### Claim 20 (depends on 14)

The manufacturing method for a metal plate according to claim 14, wherein
the preparation step includes a foil creating step of creating a plating film by using a plating liquid including a solution containing a nickel compound and a solution containing an iron compound.

### Claim 21 (depends on 14)

The manufacturing method for a metal plate according to claim 14, wherein
a thickness of the metal plate is 85 μm or less.

### Claim 22 (depends on 14)

The manufacturing method for a metal plate according to claim 14, wherein
a thickness of the metal plate is 20 μm or less.

### Claim 23 (depends on 14)

The manufacturing method for a metal plate according to claim 14, wherein
the ratio A1/A2 is 0.3 or less.

### Claim 24 (depends on 14)

The manufacturing method for a metal plate according to claim 14, wherein
the metal plate obtained by the plate member is for manufacturing the deposition mask by exposing and developing a dry film attached to the first surface of the metal plate to form a first resist pattern, and by etching an area of the first surface of the metal plate to form the plurality of through-holes, the area being not covered with the first resist pattern.

### Claim 25

A metal plate used for manufacturing a deposition mask having a plurality of through-holes formed therein,
wherein:
when a composition analysis of a first surface of the metal plate is performed by using an X-ray photoelectron spectroscopy, a ratio A1/A2 obtained by the result of the X-ray photoelectron spectroscopy is 0.4 or less, where A1 is a sum of a peak planar dimension value of nickel oxide and a peak planar dimension value of nickel hydroxide, and A2 is a sum of a peak planar dimension value of iron oxide and a peak planar dimension value of iron hydroxide; and
in the composition analysis of the first surface of the metal plate by means of the X-ray photoelectron spectroscopy, an incident angle of an X-ray emitted to the metal plate on the first surface is 45 degrees, and an acceptance angle of photoelectrons discharged from the metal plate is 90 degrees.

### Claim 26 (depends on 25)

The metal plate according to claim 25, wherein
a thickness of the metal plate is 85 μm or less.

### Claim 27 (depends on 25)

The metal plate according to claim 25, wherein
a thickness of the metal plate is 20 μm or less.

### Claim 28 (depends on 25)

The metal plate according to claim 25, wherein
the metal plate is for manufacturing the deposition mask by exposing and developing a dry film attached to the first surface of the metal plate to form a first resist pattern, and by etching an area of the first surface of the metal plate to form the plurality of through-holes, the area being not covered with the first resist pattern.

### Claim 29 (depends on 25)

The metal plate according to claim 25, wherein
the ratio A1/A2 is 0.3 or less.

### Claim 30

A manufacturing method for a deposition mask having a plurality of through-holes formed therein, the method comprising:
a step of preparing a metal plate;
a first resist pattern forming step of forming a first resist pattern on a first surface of the metal plate; and
an etching step of etching an area of the first surface of the meal plate, the area being not covered with the first resist pattern, so that first recesses to define the through-holes are formed in the first surface of the metal plate;
wherein:
when a composition analysis of a first surface of the metal plate is performed by using an X-ray photoelectron spectroscopy, a ratio A1/A2 obtained by the result of the X-ray photoelectron spectroscopy is 0.4 or less, where A1 is a sum of a peak planar dimension value of nickel oxide and a peak planar dimension value of nickel hydroxide, and A2 is a sum of a peak planar dimension value of iron oxide and a peak planar dimension value of iron hydroxide; and
in the composition analysis of the first surface of the metal plate by means of the X-ray photoelectron spectroscopy, an incident angle of an X-ray emitted to the metal plate on the first surface is 45 degrees, and an acceptance angle of photoelectrons discharged from the metal plate is 90 degrees.

### Claim 31 (depends on 30)

The manufacturing method for a deposition mask according to claim 30, wherein
a thickness of the metal plate is 85 μm or less.

### Claim 32 (depends on 30)

The manufacturing method for a deposition mask according to claim 30, wherein
a thickness of the metal plate is 20 μm or less.

### Claim 33 (depends on 30)

The manufacturing method for a deposition mask according to claim 30, wherein
the first resist pattern forming step includes a step of attaching a dry film to the first surface of the metal plate, and a step of exposing and developing the dry film to form the first resist pattern.

### Claim 34 (depends on 30)

The manufacturing method for a metal plate according to claim 30, wherein
the ratio A1/A2 is 0.3 or less.