# US 2018/0023165 A1 · Method for vitrification of arsenic and antimony

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0023165 A1
- Document ID: US20180023165A1
- Status: Published application
- Kind: A1
- Application number: 15/216,048
- Filed: 2016-07-21
- Published: 2018-01-25
- Earliest claimed: 2016-07-21
- Assignees: Dundee Sustainable Technologies Inc.
- Applicants: Dundee Sustainable Technologies Inc.
- Inventors: Jean-Marc Lalancette; David Lemieux; Khalil Nasrallah; Gabriel Garcia Curiel; Romain Barbaroux
- Web page: https://patentgrep.com/patent/US20180023165A1

## CPC

- B09B 3/29: involving a melting or softening step
- B09B 3/27: Binding by sodium silicate, e.g. cement or water glass
- C03C 1/002: {Use of waste materials, e.g. slags}
- C03C 3/062: with less than 40% silica by weight
- C03C 3/078: containing an oxide of a divalent metal, e.g. an oxide of zinc
- C03C 3/087: containing calcium oxide, e.g. common sheet or container glass
- C22B 1/11: Removing sulfur, phosphorus or arsenic other than by roasting
- C22B 30/02: Obtaining antimony
- C22B 30/04: Obtaining arsenic {(extraction of metal compounds by leaching in organic solutions C22B3/16; treatment or purification of solutions by adsorption on solids C22B3/24, by liquid-liquid extraction C22B3/26, by ion-exchange extraction C22B3/42)}
- B09B: DISPOSAL OF SOLID WASTE NOT OTHERWISE PROVIDED FOR
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS

## Abstract

A method for vitrification of arsenic and antimony, comprising substituting oxygen to sulfur on thiosalts, incorporating resulting sodium arsenate and sodium antimonate into a sodium silicate glass-forming mixture and vitrifying the sodium silicate glass-forming mixture into a resulting glass sequestering the arsenic and antimony.

## Claims

### Claim 1

Method for vitrification of arsenic and antimony, comprising substituting oxygen to sulfur on thiosalts, incorporating resulting sodium arsenate and sodium antimonate into a sodium silicate glass-forming mixture and vitrifying the sodium silicate glass-forming mixture into a resulting glass sequestering the arsenic and the antimony.

### Claim 2 (depends on 1)

The method of claim 1, wherein said substituting oxygen to sulfur on thiosalts is done by air or oxygen, at a temperature in a range between about 200° C. and 400° C.

### Claim 3 (depends on 1)

The method of claim 1, wherein the sodium silicate glass-forming mixture comprises silica in a range between 40 and 75%, sodium oxide in a range between 10 and 25% w/w and ferric oxide in a range between 8 and 20% w/w.

### Claim 4 (depends on 1)

The method of claim 1, wherein the sodium silicate glass-forming mixture comprises silica in a range between 40 and 75%, sodium oxide in a range between 10 and 25% w/w, and at least one of: ferric oxide in a range between 7 and 20% w/w, calcium oxide in a range between 1 and 10% w/w, magnesium oxide in a range between 0.1 and 2% w/w, aluminium oxide in a range between 0.1 and 2% w/w, potassium oxide in a range between 0.1 and 2% w/w and titanium oxide in a range between 0.1 and 2% w/w, alone or combined, in a total proportion in a range between about 5 and 20 w/w %.

### Claim 5 (depends on 1)

The method of claim 1, wherein said vitrifying the sodium silicate glass-forming mixture comprises heating the sodium silicate glass-forming mixture at a temperature in a range between about 1000° C. and about 1200° C. under atmospheric pressure.

### Claim 6 (depends on 1)

The method of claim 1, wherein the resulting glass comprises arsenic in a range between 1 and 20 w/w % and antimony in a range between 1 and 10 w/w %.

### Claim 7 (depends on 1)

The method of claim 1, wherein the resulting glass comprises arsenic in a range between 1 and 20 w/w %, antimony in a range between 1 and 10 w/w % and ferric oxide in a range between 7 and 20% w/w.

### Claim 8

A method for sequestering arsenic and antimony of As/Sb-bearing sulfurated ores or concentrates, comprising oxidation of the arsenic and antimony in the As/Sb-bearing sulfurated ores or concentrates, and vitrification.

### Claim 9 (depends on 8)

The method of claim 8, wherein said oxidation is performed at a temperature in the range between 200 and 400° C., the method yielding a sodium silicate glass incorporating up to 20 w/w % arsenic, and up to 10 w/w % of antimony.

### Claim 10 (depends on 8)

The method of claim 8, yielding a sodium silicate glass incorporating from 1 to 20 w/w % arsenic, from 1 to 10 w/w % of antimony and from 7 to 20 w/w % iron oxide, with amounts of at least one of: SiO2, Na2O, As2O3/As2O5, Sb2O3/Sb2O5.