# US 2018/0023158 A1 · High-strength heavy-walled stainless steel seamless tube or pipe and method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0023158 A1
- Document ID: US20180023158A1
- Status: Published application
- Kind: A1
- Application number: 15/549,514
- Filed: 2015-02-20
- Published: 2018-01-25
- Earliest claimed: 2015-02-20
- Assignees: Jfe Steel Corporation
- Applicants: JFE Steel Corporation
- Inventors: Shunsuke Sasaki; Tatsuro Katsumura; Yasushi Kato
- Web page: https://patentgrep.com/patent/US20180023158A1

## CPC

- C21D 9/08: for tubular bodies or pipes
- B21B 3/02: Rolling special iron alloys {, e.g. stainless steel}
- B21B 19/04: Rolling basic material of solid, i.e. non-hollow, structure; Piercing {, e.g. rotary piercing mills}
- C21D 1/25: Hardening, combined with annealing between 300 degrees Celsius and 600 degrees Celsius, i.e. heat refining ("Vergüten")
- C21D 6/004: {containing Cr and Ni}
- C21D 6/005: {containing Mn}
- C21D 6/007: {containing Co}
- C21D 7/12: by expanding tubular bodies
- C21D 8/10: during manufacturing of tubular bodies
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/42: with copper
- C22C 38/44: with molybdenum or tungsten
- C22C 38/46: with vanadium
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C22C 38/54: with boron
- C22C 38/58: with more than 1.5% by weight of manganese
- C21D 1/18: Hardening (C21D1/02 takes precedence); Quenching with or without subsequent tempering (quenching devices C21D1/62)
- C21D 2211/001: Austenite
- C21D 2211/005: Ferrite
- C21D 2211/008: Martensite
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- B21B: ROLLING OF METAL (auxiliary operations used in connection with metal-working operations covered in B21, see B21C; bending by rolling B21D; manufacture of particular objects, e.g. screws, wheels, rings, barrels, balls, by rolling B21H; pressure welding by means of a rolling mill B23K20/04)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A high-strength heavy-walled stainless steel seamless tube or pipe exhibiting excellent low-temperature toughness is characterized by having a chemical composition containing Cr: 15.5% to 18.0% and a steel microstructure containing a ferritic phase and a martensitic phase, wherein the maximum value of the areas of the ferrite grains in the steel microstructures in a circumferential direction cross section and an L direction (rolling direction) cross section of the steel tube or pipe is 3,000 μm2 or less and the content of ferrite grains having areas of 800 μm2 or less is 50% or more on an area fraction basis, where, when adjacent ferrite grains are present in the steel microstructure and the crystal misorientation between one ferrite grain and the other ferrite grain is 15° or more, the adjacent grains are assumed to be grains different from each other.

## Claims

### Claim at position 1

-5. (canceled)

### Claim 6

A high-strength heavy-walled stainless steel seamless tube or pipe with excellent low-temperature toughness,
comprising a chemical composition containing, on a percent by mass basis, Cr: 15.5% to 18.0% and a steel microstructure containing a ferritic phase and a martensitic phase,
wherein a maximum value of areas of ferrite grains in the steel microstructures in a circumferential direction cross section and an L direction (rolling direction) cross section of the steel tube or pipe is 3,000 μm2 or less and content of ferrite grains having areas of 800 μm2 or less is 50% or more on an area fraction basis, where, when adjacent ferrite grains are present in the steel microstructure and crystal misorientation between one ferrite grain and another ferrite grain is 15° or more, the adjacent grains are grains different from each other.

### Claim 7 (depends on 6)

The high-strength heavy-walled stainless steel seamless tube or pipe according to claim 6, wherein the chemical composition further contains, on a percent by mass basis, C: 0.050% or less, Si: 1.00% or less, Mn: 0.20% to 1.80%, Ni: 1.5% to 5.0%, Mo: 1.0% to 3.5%, V: 0.02% to 0.20%, N: 0.01% to 0.15%, O: 0.006% or less, and the remainder composed of Fe and incidental impurities.

### Claim 8 (depends on 7)

The high-strength heavy-walled stainless steel seamless tube or pipe according to claim 7, wherein the chemical composition further contains, on a percent by mass basis, at least one group selected from Group A to Group D:
Group A: Al: 0.002% to 0.050%,
Group B: at least one selected from Cu: 3.5% or less, W: 3.5% or less, and REM: 0.3% or less,
Group C: at least one selected from Nb: 0.2% or less, Ti: 0.3% or less, and Zr: 0.2% or less,
Group D: at least one selected from Ca: 0.01% or less and B: 0.01% or less.

### Claim 9 (depends on 6)

The high-strength heavy-walled stainless steel seamless tube or pipe according to claim 6, wherein the maximum value of the areas of the ferrite grains in the steel microstructures in a circumferential direction cross section and an L direction (rolling direction) cross section of the steel tube or pipe is 3,000 μm2 or less and the content of ferrite grains having areas of 800 μm2 or less is 50% or more on an area fraction basis.

### Claim 10

A method of manufacturing a high-strength heavy-walled stainless steel seamless tube or pipe, comprising: heating a steel, performing piercing the steel to produce a hollow base steel, and subjecting the hollow base steel to elongating rolling, wherein a hot working temperature of the elongating rolling is 700° C. to 1,200° C., and the steel microstructure of the hollow base steel at the hot working temperature contains 35% or more of austenite on an area fraction basis.

### Claim 11 (depends on 7)

The high-strength heavy-walled stainless steel seamless tube or pipe according to claim 7, wherein the maximum value of the areas of the ferrite grains in the steel microstructures in a circumferential direction cross section and an L direction (rolling direction) cross section of the steel tube or pipe is 3,000 μm2 or less and the content of ferrite grains having areas of 800 μm2 or less is 50% or more on an area fraction basis.

### Claim 12 (depends on 8)

The high-strength heavy-walled stainless steel seamless tube or pipe according to claim 8, wherein the maximum value of the areas of the ferrite grains in the steel microstructures in a circumferential direction cross section and an L direction (rolling direction) cross section of the steel tube or pipe is 3,000 μm2 or less and the content of ferrite grains having areas of 800 μm2 or less is 50% or more on an area fraction basis.