# US 2018/0022977 A1 · Thermal conductive silicone composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0022977 A1
- Document ID: US20180022977A1
- Status: Published application
- Kind: A1
- Application number: 15/550,863
- Filed: 2016-02-08
- Published: 2018-01-25
- Earliest claimed: 2015-03-02
- Assignees: Shin-Etsu Chemical Co., Ltd.
- Applicants: Shin-Etsu Chemical Co., Ltd.
- Inventors: Kenichi TSUJI
- Web page: https://patentgrep.com/patent/US20180022977A1

## CPC

- C09K 5/14: Solid materials, e.g. powdery or granular
- C08K 3/08: Metals
- C08K 3/22: of metals
- C08L 83/04: Polysiloxanes
- C09K 5/10: Liquid materials
- C08G 77/12: containing silicon bound to hydrogen
- C08G 77/18: to alkoxy or aryloxy groups
- C08G 77/20: containing silicon bound to unsaturated aliphatic groups
- C08K 2003/0812: {Aluminium}
- C08K 2003/2296: {of zinc}
- C08K 2201/003: Additives being defined by their diameter
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2205/03: containing three or more polymers in a blend
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

Provided is a thermal conductive silicone composition exhibiting no peeling of a heat dissipation grease and capable of maintaining a low thermal resistance, even under a severe condition. The thermal conductive silicone composition contains: (A) an organopolysiloxane having at least two alkenyl groups in one molecule and exhibiting a kinetic viscosity of 10 to 100,000 mm2/s at 25° C.; (B) a one-terminal-trifunctional hydrolyzable methylpolysiloxane; (C) an aluminum powder; (D) a zinc oxide powder; (E) an organohydrogenpolysiloxane; (F) an organohydrogenpolysiloxane other than the component (E); and (G) a platinum-based catalyst for hydrosilylation, wherein when a liquid obtained by mixing and dispersing the composition in toluene which is twice the amount of the composition has been sieved, a residue of not more than 5 ppm will be observed if using a 250 mesh sieve, and a residue of not less than 200 ppm will be observed if using a 440 mesh sieve.

## Claims

### Claim 1

A thermal conductive silicone composition comprising:
(A) an organopolysiloxane having at least two alkenyl groups in one molecule and exhibiting a kinetic viscosity of 10 to 100,000 mm2/s at 25° C.;
(B) a one-terminal-trifunctional hydrolyzable methylpolysiloxane that is in an amount of 50 to 130 parts by mass per 100 parts by mass of the component (A), and is represented by a general formula (1):
wherein R1 represents an alkyl group having 1 to 6 carbon atoms, and a represents an integer of 5 to 100;
(C) an aluminum powder having an average particle diameter of 7 to 16 μm;
(D) a zinc oxide powder having an average particle diameter of not larger than 2 μm, the components (C) and (D) being present in an amount at which a mass ratio {component (C)+component (D)}/{component (A)+component (B)} becomes 8.0 to 14.0, and at which a mass ratio between the components (C) and (D) {component (C)/component (D)} becomes 3.0 to 6.0;
(E) an organohydrogenpolysiloxane represented by a general formula (2):
wherein R2 represents an alkyl group having 1 to 6 carbon atoms, and b represents an integer of 5 to 100;
(F) an organohydrogenpolysiloxane other than the component (E), having at least two silicon atom-bonded hydrogen atoms in one molecule, the components (E) and (F) being present in an amount at which a value of {total number of silicon atom-bonded hydrogen atoms in components (E) and (F)}/{number of alkenyl groups in component (A)} becomes 0.5 to 1.5, and at which a ratio {number of silicon atom-bonded hydrogen atoms in component (E)}/{number of silicon atom-bonded hydrogen atoms in component (F)} becomes 0.6 to 5.0; and
(G) a platinum-based catalyst for hydrosilylation that is in an amount at which platinum atoms are present in an amount of 0.1 to 500 ppm on mass basis with respect to the component (A), wherein
when a liquid obtained by mixing and dispersing the composition in toluene which is twice the amount of the composition has been sieved, a residue of not more than 5 ppm is observed if using a 250 mesh sieve (mesh size of 63 μm), and a residue of not less than 200 ppm is observed if using a 440 mesh sieve (mesh size of 32 μm).

### Claim 2 (depends on 1)

The thermal conductive silicone composition according to claim 1, further comprising:
(H) a reaction control agent that is selected from an acetylene compound, a nitrogen compound, an organic phosphorous compound, an oxime compound and an organic chloro compound, and is in an amount of 0.1 to 5% on mass basis with respect to the component (A).

### Claim 3 (depends on 1)

A heat dissipation material comprising the thermal conductive silicone composition as set forth in claim 1.

### Claim 4 (depends on 1, 3)

The heat dissipation material according to claim 3, wherein a cured product obtained by pressurizing the thermal conducive silicone composition as set forth in claim 1 under 0.15 MPa at room temperature for 15 min and then performing heating and curing at 150° C. for 90 min, has a thickness of 35 to 60 μm at room temperature.

### Claim 5 (depends on 2)

A heat dissipation material comprising the thermal conductive silicone composition as set forth in claim 2.

### Claim 6 (depends on 2, 5)

The heat dissipation material according to claim 5, wherein a cured product obtained by pressurizing the thermal conducive silicone composition as set forth in claim 2 under 0.15 MPa at room temperature for 15 min and then performing heating and curing at 150° C. for 90 min, has a thickness of 35 to 60 μm at room temperature.