# US 2018/0022954 A1 · Process for preparing latex functionalized with phosphorus acid and photoinitiator groups

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0022954 A1
- Document ID: US20180022954A1
- Status: Published application
- Kind: A1
- Application number: 15/656,010
- Filed: 2017-07-21
- Published: 2018-01-25
- Earliest claimed: 2016-07-22
- Applicants: Rohm and Haas Company; Dow Global Technologies LLC
- Inventors: Matthew Belowich; Meghan Koback; Jordan Stracke; Joseph Tanzer
- Web page: https://patentgrep.com/patent/US20180022954A1

## CPC

- C08F 220/14: Methyl esters {, e.g. methyl (meth)acrylate}
- C08F 265/06: Polymerisation of acrylate or methacrylate esters on to polymers thereof
- C08F 275/00: Macromolecular compounds obtained by polymerising monomers on to polymers of monomers containing phosphorus, selenium, tellurium or a metal as defined in group C08F30/00
- C08L 33/12: Homopolymers or copolymers of methyl methacrylate
- C09D 133/12: Homopolymers or copolymers of methyl methacrylate
- C09D 151/003: {grafted on to macromolecular compounds obtained by reactions only involving unsaturated carbon-to-carbon bonds (C09D151/04, C09D151/06 take precedence)}
- C08L 2201/52: Aqueous emulsion or latex, e.g. containing polymers of a glass transition temperature (Tg) below 20°C
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

The present invention is a process for preparing a stable aqueous dispersion of polymer particles comprising structural units of a phosphorus acid monomer or a salt thereof and structural units of a photoinitiator monomer. Gloss retention of paints containing the latex prepared by the process of the present invention are improved over paints that do not have photoinitiator chemically bound to the latex particles.

## Claims

### Claim 1

A process comprising forming, by way of multistage emulsion polymerization, a stable aqueous dispersion of acrylic-based polymer particles functionalized with from 0.2 to 5 weight percent structural units of a phosphorus acid monomer and from 0.05 to 10 weight percent structural units of a photoinitiator monomer based on the weight of the polymer particles, which structural units of the phosphorus acid monomer and the photoinitator monomer arise from copolymerization of a phosphorus acid monomer and a photoinitiator monomer in the same stage.

### Claim 2 (depends on 1)

The process of claim 1 wherein the multistage emulsion polymerization is a 2-stage reaction, wherein first stage monomers comprise the photoinitiator monomer; the phosphorus acid monomer; methyl methacrylate or styrene or a combination thereof; one or more acrylates selected from the group consisting of ethyl acrylate, butyl acrylate, 2-propylheptyl acrylate, and 2-ethylhexyl acrylate; and a carboxylic acid monomer or a salt thereof, are copolymerized in a first stage;
wherein methyl methacrylate or styrene or a combination thereof; one or more acrylates selected from the group consisting of ethyl acrylate, butyl acrylate, 2-propylheptyl acrylate, and 2-ethylhexyl acrylate; and a carboxylic acid monomer or a salt thereof, are copolymerized in a second stage;
wherein the second stage optionally includes the photoinitiator monomer or the phosphorus acid monomer or both, with the proviso that the ratio of photoinitator monomer in the first stage to photoinitiator monomer in the second stage is greater than 2:1, and the ratio of phosphorus acid monomer in the first stage to phosphorus acid monomer in the second stage is greater than 2:1;
wherein ratio of stage one monomers to stage two monomers is in the range of 20:80 to 50:50.

### Claim 3 (depends on 2)

The process of claim 2 wherein in the first stage, from 0.1 to 5 weight percent of the photoinitiator monomer, from 0.5 to 3 weight percent of the phosphorus acid monomer, from 40 to 50 weight percent methyl methacrylate, from 15 to 25 weight percent butyl acrylate, from 23 to 33 weight percent 2-ethylhexyl acrylate, and 0.05 to 2 weight percent methacrylic acid or a salt thereof, are copolymerized, wherein all weights are based on the weight of first stage monomers;
wherein in the second stage, from 40 to 50 weight percent methyl methacrylate, from 15 to 25 weight percent butyl acrylate, from 23 to 33 weight percent 2-ethylhexyl acrylate, from 0.05 to 2 weight percent methacrylic acid or a salt thereof, wherein all weights are based on the weight of second stage monomers;
wherein from 0.2 to 5 weight percent ureido methacrylate is copolymerized in either the first or the second stage;
wherein the second stage monomers optionally include the photoinitiator monomer or the phosphorus acid monomer or both, with the proviso that the ratio of photoinitiator monomer in the first stage to photoinitiator monomer in the second stage is greater than 10:1, and the ratio of phosphorus acid monomer in the first stage to phosphorus acid monomer in the second stage is greater than 10:1.

### Claim 4 (depends on 3)

The process of claim 3 wherein ratio of stage one monomers to stage two monomers is in the range of 25:75 to 40:60, the ratio of photoinitiator monomer in the first stage to photoinitiator monomer in the second stage is greater than 100:1, and the ratio of phosphorus acid monomer in the first stage to phosphorus acid monomer in the second stage is greater than 100:1.

### Claim 5 (depends on 4)

The process of claim 4 wherein the second stage monomers comprise no photoinitiator monomer or phosphorus acid monomer.

### Claim 6 (depends on 1)

The process of claim 1 wherein the multistage emulsion polymerization is a 2-stage reaction, wherein first stage monomers comprise methyl methacrylate or styrene or a combination thereof; one or more acrylates selected from the group consisting of ethyl acrylate, butyl acrylate, 2-propylheptyl acrylate, and 2-ethylhexyl acrylate; and a carboxylic acid monomer or a salt thereof are copolymerized in a first stage;
wherein the photoinitiator monomer; the phosphorus acid monomer; methyl methacrylate or styrene or a combination thereof; one or more acrylates selected from the group consisting of ethyl acrylate, butyl acrylate, 2-propylheptyl acrylate, and 2-ethylhexyl acrylate; and a carboxylic acid monomer or a salt thereof are copolymerized in a second stage; and
wherein the first stage optionally includes the photoinitiator monomer or the phosphorus acid monomer or both, with the proviso that the ratio of photoinitator monomer in the first stage to photoinitiator monomer in the second stage is greater than 2:1, and the ratio of phosphorus acid monomer in the first stage to phosphorus acid monomer in the second stage is greater than 2:1.

### Claim 7 (depends on 6)

The process of claim 6 wherein in the first stage, from 40 to 50 weight percent methyl methacrylate, from 15 to 25 weight percent butyl acrylate, from 23 to 33 weight percent 2-ethylhexyl acrylate, and 0.05 to 2 weight percent methacrylic acid or a salt thereof, all weights based on the weight of first stage monomers, are copolymerized;
wherein in the second stage, from 0.1 to 5 weight percent of the photoinitiator monomer, from 0.5 to 3 weight percent of the phosphorus acid monomer, from 40 to 50 weight percent methyl methacrylate, from 15 to 25 weight percent butyl acrylate, from 23 to 33 weight percent 2-ethylhexyl acrylate, from 0.05 to 2 weight percent methacrylic acid or a salt thereof;
wherein the first stage monomers optionally include the photoinitiator monomer or the phosphorus acid monomer or both, with the proviso that the ratio of photoinitiator monomer in the second stage to photoinitiator monomer in the first stage is greater than 10:1 and the ratio of phosphorus acid monomer in the second stage to phosphorus acid monomer in the first stage is greater than 10:1;
wherein from 0.2 to 5 weight percent ureido methacrylate is copolymerized in either the first or the second stage; and
wherein the ratio of stage two monomers to stage one monomers is in the range of 20:80 to 50:50.

### Claim 8 (depends on 7)

The process of claim 7 wherein ratio of stage one monomers to stage two monomers is in the range of 25:75 to 40:60, the ratio of photoinitiator monomer in the first stage to photoinitiator monomer in the second stage is greater than 100:1, and the ratio of phosphorus acid monomer in the first stage to phosphorus acid monomer in the second stage is greater than 100:1.

### Claim 9 (depends on 7)

The process of claim 7 wherein the first stage monomers comprise no photoinitiator monomer or phosphorus acid monomer.