# US 2018/0022895 A1 · Polymeric piezoelectric film and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0022895 A1
- Document ID: US20180022895A1
- Status: Published application
- Kind: A1
- Application number: 15/550,154
- Filed: 2016-01-28
- Published: 2018-01-25
- Earliest claimed: 2015-02-13
- Assignees: Mitsui Chemicals, Inc.
- Applicants: Mitsui Chemicals, Inc.
- Inventors: Keisuke SATO; Katsuki ONISHI; Hiroaki TSUSHIMA; Kazuhiro TANIMOTO; Toshihisa KITAGAWA
- Web page: https://patentgrep.com/patent/US20180022895A1

## CPC

- C08K 5/29: Compounds containing {one or more} carbon-to-nitrogen double bonds
- C08L 67/04: Polyesters derived from hydroxycarboxylic acids, e.g. lactones (C08L67/06 takes precedence)
- H10N 30/098: Forming organic materials
- H10N 30/857: Macromolecular compositions
- C08F 2500/01: High molecular weight, e.g. >800,000 Da.
- G01N 25/4866: {by using a differential method}
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)

## Abstract

A polymeric piezoelectric film, including a helical chiral polymer (A) having a weight average molecular weight of from 50,000 to 1,000,000 and optical activity, in which, in the film: a crystallinity given by a DSC method is from 20% to 80%; a standardized molecular orientation MORc is from 3.5 to 15.0 when a reference thickness measured by a microwave transmission-type molecular orientation meter is 50 μm; and when a direction parallel to a phase difference streak is a direction X, a direction perpendicular to the direction X and parallel to a main plane of a film is a direction Y, and the phase difference streak is evaluated by an evaluation method A, per a length of 1,000 mm in the direction Y, a number of phase difference streaks with an evaluation value of 60 or more is 0, and a sum of the evaluation values of phase difference streaks with an evaluation value of 20 or more is 1000 or less.

## Claims

### Claim 1

A polymeric piezoelectric film, comprising a helical chiral polymer (A) having a weight average molecular weight of from 50,000 to 1,000,000 and optical activity, wherein, in the film:
a crystallinity given by a DSC method is from 20% to 80%;
a standardized molecular orientation MORc is from 3.5 to 15.0 when a reference thickness measured by a microwave transmission-type molecular orientation meter is 50 μm; and
when a direction parallel to a phase difference streak is a direction X, a direction perpendicular to the direction X and parallel to a main plane of a film is a direction Y, and the phase difference streak is evaluated by an evaluation method A, per a length of 1,000 mm in the direction Y, a number of phase difference streaks with an evaluation value of 60 or more is 0, and a sum of evaluation values of phase difference streaks with an evaluation value of 20 or more is 1000 or less,
the evaluation method A comprising:
(a) with respect to the direction Y, acquiring in-plane phase difference data of a film at intervals of 0.143 mm to obtain an in-plane phase difference profile;
(b) performing fast Fourier transformation on the obtained in-plane phase difference profile, removing low frequency components using 0.273/mm as a cutoff frequency, and then performing inverse Fourier transformation;
(c) calculating slopes of two adjacent points with respect to the in-plane phase difference profile after inverse Fourier transformation and converting the slopes into a slope profile; and
(d) taking a height from a bottom point of a valley of the obtained slope profile to an apex of a mountain adjacent to the valley as an evaluation value of a phase difference streak.

### Claim 2 (depends on 1)

The polymeric piezoelectric film according to claim 1, wherein, when evaluated by the evaluation method A, per a length of 1,000 mm in the direction Y, a number of phase difference streaks with an evaluation value of 40 or more is 0, and a sum total of evaluation values of phase difference streaks with an evaluation value of 20 or more is 200 or less.

### Claim 3 (depends on 1)

The polymeric piezoelectric film according to claim 1, wherein, when evaluated by the evaluation method A, per a length of 1,000 mm in the direction Y, a number of phase difference streaks with an evaluation value of 20 or more is 0, and a sum total of evaluation values of phase difference streaks with an evaluation value of 20 or more is 0.

### Claim 4 (depends on 1)

The polymeric piezoelectric film according to claim 1, wherein internal haze for visible light is 50% or less, and a piezoelectric constant d14 measured by a stress-charge method at 25° C. is 1 pC/N or more.

### Claim 5 (depends on 1)

The polymeric piezoelectric film according to claim 1, wherein internal haze for visible light is 13% or less.

### Claim 6 (depends on 1)

The polymeric piezoelectric film according to claim 1, wherein the helical chiral polymer (A) is a polylactic acid-type polymer having a main chain containing a repeating unit represented by the following Formula (1):

### Claim 7 (depends on 1)

The polymeric piezoelectric film according to claim 1, wherein a content of the helical chiral polymer (A) is 80% by mass or more.

### Claim 8 (depends on 1)

The polymeric piezoelectric film according to claim 1, wherein a product of the standardized molecular orientation MORc and the crystallinity is from 75 to 700.

### Claim 9 (depends on 1)

The polymeric piezoelectric film according to claim 1, wherein internal haze for visible light is 1.0% or less.

### Claim 10 (depends on 1)

The polymeric piezoelectric film according to claim 1, the film containing from 0.01 parts by mass to 10 parts by mass of a stabilizer having one or more functional groups selected from the group consisting of a carbodiimide group, an epoxy group, and an isocyanate group, the stabilizer having a weight average molecular weight of 200 to 60,000 (B) based on 100 parts by mass of the helical chiral polymer (A).

### Claim 11 (depends on 1)

A method of manufacturing the polymeric piezoelectric film according to claim 1, the method comprising: extruding a composition containing the helical chiral polymer (A) from a T-die having a lip tip edge radius of from 0.001 mm to 0.100 mm at an extrusion temperature of from 200° C. to 230° C. to form the composition into a film; and stretching the formed film.