# US 2018/0022890 A1 · Ester-based compound, composition comprising the same, method for preparing the same and resin composition comprising the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0022890 A1
- Document ID: US20180022890A1
- Status: Published application
- Kind: A1
- Application number: 15/546,185
- Filed: 2016-05-12
- Published: 2018-01-25
- Earliest claimed: 2015-05-14
- Assignees: LG Chem, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: Hyun Kyu KIM; Mi Yeon LEE; Jeong Ju MOON; Joo Ho KIM; Seok Ho JEONG
- Web page: https://patentgrep.com/patent/US20180022890A1

## CPC

- C08K 5/12: of cyclic polycarboxylic acids
- C07C 69/82: Terephthalic acid esters
- C08K 5/0016: {Plasticisers}
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS

## Abstract

The present invention relates to an ester-based plasticizer composition, a method for preparing the same and a resin composition comprising the same. The ester-based plasticizer composition according to one embodiment of the present invention is a novel terephthalate-based ester compound for a plasticizer prepared by transesterification. When the ester-based plasticizer composition used in a resin composition, it is capable of providing excellent properties such as migration resistance and volatility resistance as well as excellent resistance for stress, tensile strength and elongation rate.

## Claims

### Claim 1

An ester-based compound represented by the following Chemical Formula 1:
wherein, in Chemical Formula 1, R is a butyl group or an isobutyl group.

### Claim 2

A plasticizer composition comprising an ester-based compound represented by the following Chemical Formula 1:
wherein, in Chemical Formula 1, R is a butyl group or an isobutyl group.

### Claim 3

An ester-based plasticizer composition comprising an ester-based compound represented by the following Chemical Formula 1, an ester-based compound represented by the following Chemical Formula 2 and an ester-based compound represented by the following Chemical Formula 3, wherein each R in the following Chemical Formulae 1 and 2 is the same as each other:
wherein, in Chemical Formula 1, R is a butyl group or an isobutyl group;
wherein, in Chemical Formula 2, Rs are a butyl group or an isobutyl group;

### Claim 4 (depends on 3)

The ester-based plasticizer composition of claim 3, wherein the ester-based plasticizer composition comprises 0.5% by weight to 70% by weight of the ester-based compound represented by Chemical Formula 1, 0.5% by weight to 50% of the ester-based compound represented by Chemical Formula 2 and 0.5% by weight to 85% by weight of the ester-based compound represented by Chemical Formula 3 based on the total weight of the ester-based plasticizer composition.

### Claim 5 (depends on 3)

The ester-based plasticizer composition of claim 3, wherein the ester-based plasticizer composition comprises 10% by weight to 50% by weight of the ester-based compound represented by Chemical Formula 1, 0.5% by weight to 50% by weight of the ester-based compound represented by Chemical Formula 2 and 35% by weight to 80% by weight of the ester-based compound represented by Chemical Formula 3 based on the total weight of the ester-based plasticizer composition.

### Claim 6 (depends on 3)

The ester-based plasticizer composition of claim 3, wherein a mixing ratio by weight of a sum of the ester-based compound represented by Chemical Formula 2 and the ester-based compound represented by Chemical Formula 3, and the ester-based compound represented by Chemical Formula 1 is from 95:5 to 30:70.

### Claim 7 (depends on 3)

The ester-based plasticizer composition of claim 3, which is an ether-free plasticizer.

### Claim 8 (depends on 3)

A method for preparing the ester-based plasticizer composition of claim 3, the method comprising conducting transesterification of an ester-based compound represented by the following Chemical Formula 3 and an alcohol represented by the following Chemical Formula 4:
wherein, in Chemical Formula 4, R is a butyl group or an isobutyl group.

### Claim 9 (depends on 8)

The method for preparing the ester-based plasticizer composition of claim 8, wherein a molar ratio of the compound represented by Chemical Formula 3 and the alcohol represented by Chemical Formula 4 is from 1:0.005 to 1:5.

### Claim 10 (depends on 8)

The method for preparing the ester-based plasticizer composition of claim 8, wherein the alcohol represented by Chemical Formula 4 is added in an amount of 0.1 parts by weight to 89.9 parts by weight based on 100 parts by weight of the compound represented by Chemical Formula 3.

### Claim 11 (depends on 8)

The method for preparing the ester-based plasticizer composition of claim 8, wherein the transesterification is conducted at a temperature from 120° C. to 190° C.

### Claim 12 (depends on 8)

The method for preparing the ester-based plasticizer composition of claim 8, wherein the transesterification is a noncatalytic reaction.

### Claim 13 (depends on 8)

The method for preparing the ester-based plasticizer composition of claim 8, the method further comprises removing the unreacted alcohol represented by Chemical Formula 4 and reaction byproducts by distillation after conducting the transesterification.

### Claim 14 (depends on 8)

The method for preparing the ester-based plasticizer composition of claim 8, wherein part of the compound represented by Chemical Formula 3 is converted to a compound represented by the following Chemical Formula 1 and a compound represented by the following Chemical Formula 2 by the transesterification:
wherein, in Chemical Formula 1, R is a butyl group or an isobutyl group;
wherein, in Chemical Formula 2, Rs are a butyl group or an isobutyl group.

### Claim 15 (depends on 8)

The method for preparing the ester-based plasticizer composition of claim 8, wherein the compound represented by the Chemical Formula 3 is prepared by conducting esterification of a compound represented by the following Chemical Formula 5 and an alcohol represented by the following Chemical Formula 6 in the presence of a catalyst:

### Claim 16 (depends on 15)

The method for preparing the ester-based plasticizer composition of claim 15, wherein the esterification is conducted at a temperature from 80° C. to 270° C.

### Claim 17 (depends on 15)

The method for preparing the ester-based plasticizer composition of claim 15, wherein the catalyst is an organic metal catalyst comprising a Sn-based or a Ti-based, an acid catalyst comprising a sulfonic acid-based or a sulfuric acid-based, or a mixed catalyst thereof.

### Claim 18 (depends on 15)

The method for preparing the ester-based plasticizer composition of claim 15, wherein a molar ratio of the compound represented by Chemical Formula 5 and the alcohol represented by Chemical Formula 6 is from 1:1 to 1:7.

### Claim 19 (depends on 15)

The method for preparing the ester-based plasticizer composition of claim 15, wherein the alcohol represented by Chemical Formula 6 comprises at least one isomer.

### Claim 20

A resin composition comprising 5 parts by weight to 100 parts by weight of the ester-based plasticizer composition of claim based on 100 parts by weight of a resin comprising at least one selected from the group consisting of ethylene vinyl acetate, polyethylene, polypropylene, polyvinyl chloride, polystyrene, polyurethane, thermoplastic elastomers and polylactic acid.

### Claim 21

(canceled)