# US 2018/0022640 A1 · Ion exchangeable glass, glass ceramics and methods for making the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0022640 A1
- Document ID: US20180022640A1
- Status: Published application
- Kind: A1
- Application number: 15/706,044
- Filed: 2017-09-15
- Published: 2018-01-25
- Earliest claimed: 2013-08-30
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Matthew John Dejneka; Qiang Fu; Timothy Michael Gross; Xiaoju Guo; Sumalee Likitvanichkul; John Christopher Mauro
- Web page: https://patentgrep.com/patent/US20180022640A1

## CPC

- C03C 10/0009: {containing silica as main constituent}
- C03B 32/02: Thermal crystallisation, e.g. for crystallising glass bodies into glass-ceramic articles {(C03B27/012 takes precedence)}
- C03C 3/091: containing aluminium
- C03C 3/097: containing phosphorus, niobium or tantalum
- C03C 3/112: containing fluorine
- C03C 4/005: {for opaline glass}
- C03C 4/02: for coloured glass
- C03C 10/00: Devitrified glass ceramics, i.e. glass ceramics having a crystalline phase dispersed in a glassy phase and constituting at least 50% by weight of the total composition
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 2204/00: Glasses, glazes or enamels with special properties
- Y10T 428/315: Surface modified glass [e.g., tempered, strengthened, etc.]
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Glass-ceramics and precursor glasses that are crystallizable to glass-ceramics are disclosed. The glass-ceramics of one or more embodiments include rutile, anatase, armalcolite or a combination thereof as the predominant crystalline phase. Such glasses and glass-ceramicsmay include compositions of, in mole %: SiO2 in the range from about 45 to about 75; Al2O3 in the range from about 4 to about 25; P2O5 in the range from about 0 to about 10; MgO in the range from about 0 to about 8; R2O in the range from about 0 to about 33; ZnO in the range from about 0 to about 8; ZrO2 in the range from about 0 to about 4; B2O3 in the range from about 0 to about 12, and one or more nucleating agents in the range from about 0.5 to about 12. In some glass-ceramic articles, the total crystalline phase includes up to 20% by weight of the glass-ceramic article.

## Claims

### Claim 1

A glass-ceramic article comprising:
a predominant crystalline phase comprising anatase, rutile, or a combination thereof; and a composition, in mol %, comprising:
SiO2 in the range from about 45 to about 75;
Al2O3 in the range from about 4 to about 25;
P2O5 in the range from about 0 to about 10;
MgO in the range from about 0 to about 8;
R2O in the range from about 0 to about 33;
ZnO in the range from about 0 to about 8;
ZrO2 in the range from about 0 to about 4;
TiO2 in the range from about 0.5 to about 12; and
B2O3 in the range from about 0 to about 12,
wherein R2O comprises one or more of Na2O, Li2O and K2O.

### Claim 2 (depends on 1)

The glass-ceramic article of claim 1, wherein (R2O—Al2O3) is in the range from about −4 to about 4.

### Claim 3 (depends on 1)

The glass-ceramic article of claim 1, wherein the composition comprises, in mol %, Li2O in the range from about 0 to about 12;
Na2O in the range from about 4 to about 20; and
K2O in the range from about 0 to about 2.

### Claim 4 (depends on 1)

The glass-ceramic article of claim 1, wherein the composition comprises, in mol %, any one or more of B2O3 in the range from about 2 to about 10, and P2O5 in the range from about 0.1 to about 10.

### Claim 5 (depends on 1)

The glass-ceramic article of claim 1 further comprising a total crystalline phase of up to 20% by weight.

### Claim 6 (depends on 1)

The glass-ceramic article of claim 1, further comprising a compressive stress layer extending from a surface of the glass-ceramic article to a depth of the compressive stress layer, the compressive stress layer comprising a compressive stress of about 200 MPa or greater and the depth of compressive stress layer of about 15 μm or greater.

### Claim 7 (depends on 6)

The glass-ceramic article of claim 6, further exhibiting a Vickers indentation crack initiation load of about 10 kgf or greater.

### Claim 8

A glass-ceramic article comprising:
a predominant crystalline phase comprising anatase, rutile, or a combination thereof,
wherein the glass-ceramic article is formed from a precursor glass having a liquidus viscosity of about 10 kP or greater.

### Claim 9 (depends on 8)

The glass-ceramic article of claim 8, wherein the predominant crystalline phase comprises crystals having a minor dimension of about 1000 nm or less and wherein the crystals comprise a major dimension and an aspect ratio the major dimension to the minor dimension of about 2 or greater.

### Claim 10 (depends on 8)

The glass-ceramic article of claim 8, wherein the combined amount of anatase and rutile is less than about 12 wt. %, of the glass-ceramic article.

### Claim 11 (depends on 8)

The glass-ceramic article of claim 8, further comprising a color presented in CIELAB color space coordinates determined from specular reflectance measurements selected from any one of:
CIE a* in the range from about −2 to about 8, CIE b* in the range from about −7 to about 30, and CIE L* in the range from about 85 to about 100; and
CIE a* in the range from about −1 to about 0, CIE b* in the range from about −8 to about −3, and CIE L* in the range from about 80 to about 100.

### Claim 12 (depends on 8)

The glass-ceramic article of claim 8, further exhibiting a Vickers indentation crack initiation load of about 10 kgf or greater.

### Claim 13

An aluminosilicate glass precursor comprising a composition, in mol %, comprising:
SiO2 in the range from about 45 to about 75;
Al2O3 in the range from about 4 to about 25;
P2O5 in the range from about 0 to about 10;
MgO in the range from about 0 to about 8;
R2O in the range from about 0 to about 33;
ZnO in the range from about 0 to about 8;
ZrO2 in the range from about 0 to about 4;
TiO2 in the range from about 0.5 to about 12; and
B2O3 in the range from about 0 to about 12,
wherein R2O comprises one or more of Na2O, Li2O and K2O.

### Claim 14 (depends on 13)

The aluminosilicate glass precursor of claim 13, wherein the composition comprises, in mol %,
Li2O in the range from about 0 to about 12;
Na2O in the range from about 4 to about 20; and
K2O in the range from about 0 to about 2.

### Claim 15 (depends on 13)

The aluminosilicate glass precursor of claim 13, wherein the composition exhibits a liquidus viscosity of about 10 kilopoise (kP) or greater.

### Claim 16 (depends on 13)

The aluminosilicate glass precursor of claim 13, wherein the composition exhibits a liquidus temperature of less than about 1400° C.

### Claim 17

A method of making a glass-ceramic article having a predominant crystalline phase including anatase, rutile, or a combination thereof, the method comprising:
melting a batch for, and forming a glass article having a composition comprising, in mol %,
SiO2 in the range from about 45 to about 75;
Al2O3 in the range from about 4 to about 25;
P2O5 in the range from about 0 to about 10;
MgO in the range from about 0.01 to about 8;
R2O in the range from about 0 to about 33;
ZnO in the range from about 0 to about 8;
ZrO2 in the range from about 0 to about 4
TiO2 in the range from about 0.5 to about 12,and
B2O3 in the range from about 0 to about 12,
wherein R2O comprises one or more of Na2O, Li2O and K2O, and
wherein the glass article exhibits a liquidus viscosity of about 10 kilopoise (kP) or greater and a liquidus temperature of less than about 1400° C. during formation of the glass article;
ceramming the glass article at a temperature between about 50° C. greater than an annealing temperature of the glass article and about 1100° C. for a period of time to cause the generation of a glass-ceramic article which includes a predominant crystalline phase comprising anatase, rutile, or a combination thereof; and
cooling the glass-ceramic article to room temperature.

### Claim 18 (depends on 17)

The method of claim 17, further comprising subjecting the glass-ceramic article to ion exchange treatment to achieve a compressive stress layer within the glass-ceramic article having a compressive stress of about 200 MPa or greater, wherein the compressive stress layer extends from a surface of the glass article into the glass article at a depth of the compressive stress layer of about 15 μm or greater.

### Claim 19 (depends on 1)

An electronic or portable computing device comprising the glass-ceramic article of claim 1.

### Claim 20 (depends on 8)

An electronic or portable computing device comprising the glass-ceramic article of claim 8.