# US 2018/0022637 A1 · Ion exchangeable glass with high crack initiation threshold

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0022637 A1
- Document ID: US20180022637A1
- Status: Published application
- Kind: A1
- Application number: 15/696,831
- Filed: 2017-09-06
- Published: 2018-01-25
- Earliest claimed: 2011-11-16
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Timothy Michael Gross
- Web page: https://patentgrep.com/patent/US20180022637A1

## CPC

- C03C 3/097: containing phosphorus, niobium or tantalum
- C03C 3/083: containing aluminium oxide or an iron compound
- C03C 3/085: containing an oxide of a divalent metal
- C03C 3/087: containing calcium oxide, e.g. common sheet or container glass
- C03C 4/02: for coloured glass
- C03C 14/006: {the non-glass component being in the form of microcrystallites, e.g. of optically or electrically active material}
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 3/04: containing silica
- C03C 3/062: with less than 40% silica by weight
- C03C 3/064: containing boron
- C03C 3/091: containing aluminium
- C03C 3/093: containing zinc or zirconium
- C03C 4/18: for ion-sensitive glass
- C03C 21/00: Treatment of glass, not in the form of fibres or filaments, by diffusing ions or metals in the surface
- C03C 2204/00: Glasses, glazes or enamels with special properties
- Y10T 428/265: 1 mil or less
- Y10T 428/315: Surface modified glass [e.g., tempered, strengthened, etc.]
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Alkali aluminosilicate glasses that are resistant to damage due to sharp impact and capable of fast ion exchange are provided. The glasses comprise at least 4 mol % P2O5 and, when ion exchanged, have a Vickers indentation crack initiation load of at least about 7 kgf.

## Claims

### Claim at position 1

1-55. (canceled)

### Claim 56

An alkali aluminosilicate glass comprising MgO; from about 40 mol % to about 70 mol % SiO2; from about 11 mol % to about 25 mol % Al2O3; from about 4 mol % to about 15 mol % P2O5; from about 13 mol % to about 20 mol % Na2O; less than 1 mol % B2O3; and 0 mol % K2O, wherein:
i. the alkali aluminosilicate glass is free of Li2O; and
ii. 1.3<[(P2O5+R2O)/M2O3]≦2.3, where M2O3=Al2O3+B2O3 and R2O is the sum of monovalent cation oxides present in the alkali aluminosilicate glass.

### Claim 57 (depends on 56)

The alkali aluminosilicate glass of claim 56, wherein the alkali aluminosilicate glass comprises from about 50 mol % to about 65 mol % SiO2; from about 14 mol % to about 20 mol % Al2O3; from about 4 mol % to about 10 mol % P2O5; and from about 14 mol % to about 20 mol % Na2O.

### Claim 58 (depends on 56)

The alkali aluminosilicate glass of claim 56, wherein the glass satisfies:
1.5<[(P2O5+R2O)/M2O3]≦2.0.

### Claim 59 (depends on 56)

The alkali aluminosilicate glass of claim 56, wherein the alkali aluminosilicate glass comprises 0 mol % B2O3.

### Claim 60 (depends on 56)

The alkali aluminosilicate glass of claim 56, wherein the monovalent cation oxides are selected from the group consisting of Na2O, Rb2O, and Cs2O.

### Claim 61 (depends on 57)

The alkali aluminosilicate glass of claim 57, wherein the alkali aluminosilicate glass comprises 0 mol % B2O3.

### Claim 62 (depends on 56)

The alkali aluminosilicate glass of claim 56, wherein the alkali aluminosilicate glass has a potassium/sodium interdiffusion coefficient of at least about 2.4×10−10 cm2/s at 410° C.

### Claim 63 (depends on 69)

The alkali aluminosilicate glass of claim 69, wherein the potassium/sodium interdiffusion coefficient is in a range from about 2.4×10−10 cm2/s up to about 1.5×10−9 cm2/s at 410° C.

### Claim 64 (depends on 56)

An electronic device comprising the alkali aluminosilicate glass of claim 56.

### Claim 65

An alkali aluminosilicate glass comprising MgO; from about 40 mol % to about 70 mol % SiO2; from about 11 mol % to about 25 mol % Al2O3; from about 4 mol % to about 15 mol % P2O5; from about 13 mol % to about 20 mol % Na2O; less than 1 mol % B2O3; and 0 mol % K2O, wherein:
i. the alkali aluminosilicate glass is ion exchanged to a depth of layer of at least about 10 μm;
ii. the alkali aluminosilicate glass is free of Li2O; and
iii. 1.3<[(P2O5+R2O)/M2O3]≦2.3, where M2O3=Al2O3+B2O3 and R2O is the sum of monovalent cation oxides present in the alkali aluminosilicate glass.

### Claim 66 (depends on 65)

The alkali aluminosilicate glass of claim 65, wherein the alkali aluminosilicate glass comprises from about 50 mol % to about 65 mol % SiO2; from about 14 mol % to about 20 mol % Al2O3; from about 4 mol % to about 10 mol % P2O5; and from about 14 mol % to about 20 mol % Na2O.

### Claim 67 (depends on 65)

The alkali aluminosilicate glass of claim 65, wherein the glass satisfies:
1.5<[(P2O5+R2O)/M2O3]≦2.0.

### Claim 68 (depends on 65)

The alkali aluminosilicate glass of claim 65, wherein the alkali aluminosilicate glass has a potassium/sodium interdiffusion coefficient of at least about 2.4×10−10 cm2/s at 410° C.

### Claim 69 (depends on 68)

The alkali aluminosilicate glass of claim 68, wherein the potassium/sodium interdiffusion coefficient is in a range from about 2.4×10−10 cm2/s up to about 1.5×10−9 cm2/s at 410° C.

### Claim 70 (depends on 65)

The alkali aluminosilicate glass of claim 65, wherein the glass has a compressive layer extending from a surface of the glass to the depth of layer, and wherein the compressive layer is under a compressive stress of at least about 300 MPa.

### Claim 71 (depends on 65)

The alkali aluminosilicate glass of claim 65, wherein the ion exchanged glass has a Vickers indentation crack initiation load of at least about 7 kgf.

### Claim 72 (depends on 71)

The alkali aluminosilicate glass of claim 71, wherein the ion exchanged glass has a Vickers indentation crack initiation load of at least about 12 kgf.

### Claim 73 (depends on 65)

An electronic device comprising the alkali aluminosilicate glass of claim 65.