# US 2018/0022636 A1 · Ion-exchanged glass of high surface compression and shallow depth of layer with high resistance to radial crack formation from vickers indentation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0022636 A1
- Document ID: US20180022636A1
- Status: Published application
- Kind: A1
- Application number: 15/692,433
- Filed: 2017-08-31
- Published: 2018-01-25
- Earliest claimed: 2011-07-01
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Jonathan David Pesansky; Chandan Kumar Saha; Trevor E. Wilantewicz
- Web page: https://patentgrep.com/patent/US20180022636A1

## CPC

- C03C 3/097: containing phosphorus, niobium or tantalum
- C03C 3/083: containing aluminium oxide or an iron compound
- C03C 3/085: containing an oxide of a divalent metal
- C03C 3/087: containing calcium oxide, e.g. common sheet or container glass
- C03C 3/091: containing aluminium
- C03C 3/093: containing zinc or zirconium
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- Y10T 29/49863: with prestressing of part
- Y10T 428/315: Surface modified glass [e.g., tempered, strengthened, etc.]
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Disclosed are alkali aluminosilicate glasses having unexpected resistance to indentation cracking. The glasses obtain this high resistance as a result of a high level of surface compression accompanied by a shallow depth of layer. The advantaged glasses show greater resistance to radial crack formation from Vickers indentation than glasses with the same compressive stress, but higher depths of layer.

## Claims

### Claim 1

A glass article comprising:
about 40 mol % to about 70 mol % SiO2;
about 11 mol % to about 25 mol % Al2O3;
at least 4 mol % to about 15 mol.% P2O5;
less than about 1 mol % B2O3; and
from 13 mol % to about 25 mol % Na2O.

### Claim 2 (depends on 1)

The glass article of claim 1, wherein:
0.6<[M2O3(mol %)/RxO(mol %)]<1.4; or i.
1.3<[(P2O5+R2O)/M2O3]≦2.3, ii.
where M2O3=Al2O3+B2O3, RxO is the sum of monovalent and divalent cation oxides present in the glass composition, and R2O is the sum of monovalent cation oxides present in the glass composition.

### Claim 3 (depends on 1)

The glass article of claim 1, wherein the glass article is ion-exchange strengthened with a compressive stress from about 600 to about 1200 MPa at a depth of layer from about 10 to about 40 μm and an indentation fracture threshold from about 10 to about 50 kg.

### Claim 4 (depends on 1)

The glass article of claim 1, wherein the glass article satisfies one or more of:
0.6<[M2O3(mol %)/RxO(mol %)]<1.4;
0.6<[M2O3(mol %)/RxO(mol %)]<1;
1.3<[(P2O5+R2O)/M2O3]≦2.3; and
1.5<[(P2O5+R2O)/M2O3]≦2.0.

### Claim 5 (depends on 1)

The glass article of claim 1, wherein the glass article comprises less than 1 mol % K2O or the monovalent and divalent cation oxides are selected from the group consisting of Li2O, Na2O, K2O, Rb2O, Cs2O, MgO, CaO, SrO, BaO, and ZnO.

### Claim 6 (depends on 1)

A method of ion exchanging a glass article having a layer under compressive stress, the layer extending from a surface of the glass article to a depth of layer, comprising:
providing the glass article of claim 1; and
ion exchanging the glass article in a bath at a temperature of up to about 410° C. for from about 15 minutes to about 24 hours to form the layer, wherein the compressive stress of the layer is from about 600 MPa to about 1200 MPa and the depth of layer is from about 10 μm to about 40 μm.

### Claim 7 (depends on 1)

A method of making a device comprising a glass article having a layer under compressive stress, the layer extending from a surface of the glass article to a depth of layer, comprising:
providing the glass article of claim 1;
ion exchanging the glass article in a bath at a temperature of up to about 410° C. for from about 15 minutes to about 24 hours to form the layer, wherein the compressive stress of the layer is from about 600 MPa to about 1200 MPa and the depth of layer is from about 10 μm to about 40 μm; and
incorporating the glass article into a device.

### Claim 8

A glass article comprising:
about 50 mol % to about 65 mol % SiO2;
about 14 mol % to about 20 mol % Al2O3;
0 mol % to less than about 1 mol % B2O3;
about 4 mol % to about 10 mol % P2O5; and
from 14 mol % to about 20 mol % Na2O.

### Claim 9 (depends on 8)

The glass article of claim 8, wherein:
0.6<[M2O3(mol %)/RxO(mol %)]<1.4; or i.
1.3<[(P2O5+R2O)/M2O3]≦2.3, ii.
where M2O3=Al2O3+B2O3, RxO is the sum of monovalent and divalent cation oxides present in the glass composition, and R2O is the sum of monovalent cation oxides present in the glass composition.

### Claim 10 (depends on 8)

The glass article of claim 8, wherein the glass article is ion-exchange strengthened with a compressive stress from about 600 to about 1200 MPa at a depth of layer from about 10 to about 40 μm and an indentation fracture threshold from about 10 to about 50 kg.

### Claim 11 (depends on 8)

The glass article of claim 8, wherein the glass article satisfies one or more of:
0.6<[M2O3(mol %)/RxO(mol %)]<1.4;
0.6<[M2O3(mol %)/RxO(mol %)]<1;
1.3<[(P2O5+R2O)/M2O3]≦2.3; and
1.5<[(P2O5+R2O)/M2O3]≦2.0.

### Claim 12 (depends on 8)

The glass of claim 8, wherein the glass comprises less than 1 mol % K2O or the monovalent and divalent cation oxides are selected from the group consisting of Li2O, Na2O, K2O, Rb2O, Cs2O, MgO, CaO, SrO, BaO, and ZnO.

### Claim 13 (depends on 8)

A method of ion exchanging a glass article having a layer under compressive stress, the layer extending from a surface of the glass article to a depth of layer, comprising:
providing the glass article of claim 8; and
ion exchanging the glass article in a bath at a temperature of up to about 410° C. for from about 15 minutes to about 24 hours to form the layer, wherein the compressive stress of the layer is from about 600 MPa to about 1200 MPa and the depth of layer is from about 10 μm to about 40 μm.

### Claim 14 (depends on 8)

A method of making a device comprising a glass article having a layer under compressive stress, the layer extending from a surface of the glass article to a depth of layer, comprising:
providing the glass article of claim 8;
ion exchanging the glass article in a bath at a temperature of up to about 410° C. for from about 15 minutes to about 24 hours to form the layer, wherein the compressive stress of the layer is from about 600 MPa to about 1200 MPa and the depth of layer is from about 10 μm to about 40 μm; and
incorporating the glass article into a device.