# US 2018/0022634 A1 · Glass for laser processing and method for producing perforated glass using same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0022634 A1
- Document ID: US20180022634A1
- Status: Published application
- Kind: A1
- Application number: 15/550,257
- Filed: 2016-02-03
- Published: 2018-01-25
- Earliest claimed: 2015-02-13
- Assignees: Nippon Sheet Glass Co., Ltd.
- Applicants: Nippon Sheet Glass Company, Limited
- Inventors: Teruhide INOUE; Koichi SAKAGUCHI; Hirotaka KOYO
- Web page: https://patentgrep.com/patent/US20180022634A1

## CPC

- C03C 3/091: containing aluminium
- B23K 26/0006: {taking account of the properties of the material involved (B23K26/32, B23K26/40 take precedence)}
- B23K 26/0622: by shaping pulses
- B23K 26/352: for surface treatment
- B23K 26/382: by boring
- B23K 26/53: for modifying or reforming the material inside the workpiece, e.g. for producing break initiation cracks
- C03C 3/093: containing zinc or zirconium
- C03C 3/095: containing rare earths
- C03C 15/00: Surface treatment of glass, not in the form of fibres or filaments, by etching (etching or surface-brightening compositions, in general C09K13/00)
- C03C 23/0025: {by a laser beam}
- B23K 2101/40: Semiconductor devices
- B23K 2103/54: {Glass}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

The present invention provides a glass composition that allows holes with a circular contour and a smooth inner wall to be formed by a collective micro-hole-forming process using a combination of modified portion formation by ultraviolet laser irradiation and etching, the glass composition being adapted for practical continuous production. The present invention relates to a glass for laser processing, the glass having a glass composition including, in mol %: 45.0%≦SiO2≦70.0%; 2.0%≦B2O3≦20.0%; 3.0%≦Al2O3≦20.0%; 0.1%≦CuO≦2.0%; 0%≦TiO2≦15.0%; and 0%≦ZnO≦9.0%, wherein a relationship of 0≦Li2O+Na2O+K2O<2.0% is satisfied.

## Claims

### Claim 1

A glass for laser processing, the glass having a glass composition comprising, in mol %:
45.0%≦SiO2≦70.0%;
2.0%≦B2O3≦20.0%;
3.0%≦Al2O3≦20.0%;
0.1%≦CuO≦2.0%;
0%≦TiO2≦15.0%; and
0%≦ZnO≦9.0%,
wherein a relationship of 0≦Li2O+Na2O+K2O<2.0% is satisfied.

### Claim 2 (depends on 1)

The glass for laser processing according to claim 1, wherein a relationship of 55.0%≦SiO2+B2O3≦80.0% is satisfied.

### Claim 3 (depends on 1)

The glass for laser processing according to claim 1, wherein a relationship of 6.0%≦MgO+CaO+SrO+BaO≦25.0% is satisfied.

### Claim 4 (depends on 1)

The glass for laser processing according to claim 1, wherein a relationship of 5.0≦Al2O3/CuO≦60.0 is satisfied.

### Claim 5 (depends on 1)

The glass for laser processing according to claim 1, further comprising, as a coloring component, an oxide of at least one metal selected from the group consisting of Fe, Ce, Bi, W, Mo, Co, Mn, Cr, and V.

### Claim 6 (depends on 1)

The glass for laser processing according to claim 1, wherein
the glass composition comprises, in mol %:
45.0%≦SiO2≦68.0%;
2.0%≦B2O3≦20.0%;
3.0%≦Al2O3≦20.0%; and
0.1%≦CuO≦2.0%,
the glass composition is substantially free of TiO2 and ZnO, and
the following relationships are satisfied:
58.0%≦SiO2+B2O3≦80.0%;
8.0%≦MgO+CaO+SrO+BaO≦20.0%;
0≦Li2O+Na2O+K2O<2.0%; and
6.0≦Al2O3/CuO≦60.0.

### Claim 7 (depends on 1)

The glass for laser processing according to claim 1, wherein
the glass composition comprises, in mol %:
50.0%≦SiO2≦68.0%;
6.0%≦B2O3≦18.0%;
7.0%≦Al2O3≦18.0%;
0.1%≦CuO≦1.8%; and
1.0%≦TiO2≦10.0%,
the glass composition is substantially free of ZnO, and
the following relationships are satisfied:
58.0%≦SiO2+B2O3≦80.0%;
8.0%≦MgO+CaO+SrO+BaO≦20.0%;
0≦Li2O+Na2O+K2O<2.0%;
6.0≦Al2O3/CuO≦60.0; and
0≦TiO2/CuO≦20.0.

### Claim 8 (depends on 1)

The glass for laser processing according to claim 1, wherein
the glass composition comprises, in mol %:
50.0%≦SiO2≦68.0%;
6.0%≦B2O3≦18.0%;
7.0%≦Al2O3≦18.0%;
0.1%≦CuO≦1.8%; and
1.0%≦ZnO≦9.0%,
the glass composition is substantially free of TiO2, and
the following relationships are satisfied:
58.0%≦SiO2+B2O3≦80.0%;
8.0%≦MgO+CaO+SrO+BaO≦20.0%;
0≦Li2O+Na2O+K2O<2.0%; and
6.0≦Al2O3/CuO≦60.0.

### Claim 9 (depends on 1)

The glass for laser processing according to claim 1, wherein the glass composition further comprises, in mol %:
2.0%≦MgO≦10.0%;
1.0%≦CaO≦10.0%;
1.0%≦SrO≦10.0%; and
0≦BaO≦6.0%.

### Claim 10 (depends on 1)

The glass for laser processing according to claim 1, wherein the glass composition further comprises, in mol %:
3.0%≦MgO≦8.5%;
2.0%≦CaO≦6.5%;
2.0%≦SrO≦6.5%; and
0≦BaO≦6.0%.

### Claim 11 (depends on 1)

The glass for laser processing according to claim 1, having a coefficient of thermal expansion of 60×10−7/° C. or less.

### Claim 12 (depends on 1)

The glass for laser processing according to claim 1, having an absorption coefficient α of 2 to 40/cm.

### Claim 13 (depends on 1)

A method for producing a perforated glass, comprising the steps of:
(i) irradiating an area of the glass for laser processing according to claim 1 with a laser pulse focused by a lens, thereby forming a modified portion in the irradiated area; and
(ii) etching at least the modified portion using an etchant, thereby forming a hole in the glass for laser processing.