# US 2018/0022610 A1 · Method for Manufacturing Graphene Composite Film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0022610 A1
- Document ID: US20180022610A1
- Status: Published application
- Kind: A1
- Application number: 15/679,223
- Filed: 2017-08-17
- Published: 2018-01-25
- Earliest claimed: 2015-12-29
- Assignees: I-Shou University
- Applicants: I-Shou University
- Inventors: Chiung-Fang Lin
- Web page: https://patentgrep.com/patent/US20180022610A1

## CPC

- C01B 32/184: Preparation
- B01F 31/80: Mixing by means of high-frequency vibrations above one kHz, e.g. ultrasonic vibrations
- B29D 7/01: Films or sheets
- C01B 39/02: Crystalline aluminosilicate zeolites; Isomorphous compounds thereof; Direct preparation thereof; Preparation thereof starting from a reaction mixture containing a crystalline zeolite of another type, or from preformed reactants; After-treatment thereof
- H01B 1/16: the conductive material comprising metals or alloys
- H01B 1/18: the conductive material comprising carbon-silicon compounds, carbon or silicon
- B29K 2995/0041: Crystalline
- C01B 2204/04: Specific amount of layers or specific thickness
- C01B 2204/22: Electronic properties
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- B01F: MIXING, e.g. DISSOLVING, EMULSIFYING OR DISPERSING (mixing paints B44D3/06)
- B29D: PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCES IN A PLASTIC STATE (making granules B29B9/00; making preforms B29B11/00)
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

A method for manufacturing a graphene composite film includes preparing a zeolite suspension containing zeolite nanocrystals with a concentration of 50-100 ppm and with a particle size of 50-80 nm. The zeolite suspension has a pH value of 11-13. A graphene oxide suspension containing graphene oxide with a concentration of 50-200 ppm is mixed with the zeolite suspension to form a composite solution. The composite solution is transferred into a 15° C. water bath when a color of the composite solution turns from brownish-yellow into deep brown. A surfactant is added into the composite solution in the 15° C. water bath. The composite solution is then sonicated for 5-30 minutes and removed out of the 15° C. water bath, with the color of the composite solution turning from deep brown into black. The composite solution is further processed to form a graphene composite film having not more than 5 layers.

## Claims

### Claim 1

A method for manufacturing a graphene composite film, comprising:
(a) preparing a zeolite suspension containing zeolite nanocrystals with a concentration of 50-100 ppm, wherein a particle size of the zeolite nanocrystals is 50-80 nm, and wherein the zeolite suspension has a pH value of 11-13;
(b) preparing a graphene oxide suspension containing graphene oxide with a concentration of 50-200 ppm;
(c) mixing the graphene oxide suspension with the zeolite suspension according to a volume ratio of 1:1 to 9:1 to form a composite solution and transferring the composite solution into a 15° C. water bath when a color of the composite solution turns from brownish-yellow into deep brown;
(d) adding a surfactant into the composite solution in the 15° C. water bath;
(e) sonicating the composite solution after step (d) for 5-30 minutes and removing the composite solution out of the 15° C. water bath, with the color of the composite solution turning from deep brown into black;
(f) atomizing the composite solution after step (e) to form atomized droplets;
(g) treating the atomized droplets with a plasma to charge the atomized droplets; and
(h) depositing the charged atomized droplets on a substrate having a temperature of 150-350° C., forming a graphene composite film having not more than 5 layers.

### Claim 2 (depends on 1)

The method for manufacturing a graphene composite film as claimed in claim 1, wherein the composite solution in step (c) is sonicated at 50-90° C. to turn the color of the composite solution from brownish-yellow into deep brown.

### Claim 3 (depends on 2)

The method for manufacturing a graphene composite film as claimed in claim 2, wherein the composite solution in step (e) is sonicated at 50-90° C. for 12-24 hours to turn the color of the composite solution from deep brown into black.

### Claim 4 (depends on 1)

The method for manufacturing a graphene composite film as claimed in claim 1, wherein the surfactant is 1-methy-2-pyrrolidone, isopropanol (NMP), propylene glycol methyl ether (PGME), ethyl acetate or methyl ethyl ketone (MEK).

### Claim 5 (depends on 1)

The method for manufacturing a graphene composite film as claimed in claim 1, wherein the zeolite suspension further comprises a metal salt.

### Claim 6 (depends on 5)

The method for manufacturing a graphene composite film as claimed in claim 5, wherein the metal salt is a salt of gold, platinum, silver, copper or nickel.

### Claim 7 (depends on 1)

The method for manufacturing a graphene composite film as claimed in claim 1, wherein in step (d), the composite solution is sonicated for 1-3 hours before adding the surfactant.

### Claim 8 (depends on 1)

The method for manufacturing a graphene composite film as claimed in claim 1, wherein step (g) comprises using a gas to carry the atomized droplets through the plasma to change the atomized droplets.

### Claim 9 (depends on 8)