# US 2018/0022603 A1 · Mems devices having tethering structures

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0022603 A1
- Document ID: US20180022603A1
- Status: Published application
- Kind: A1
- Application number: 15/215,753
- Filed: 2016-07-21
- Published: 2018-01-25
- Earliest claimed: 2016-07-21
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Co., Ltd.
- Inventors: Chia-Hua Chu
- Web page: https://patentgrep.com/patent/US20180022603A1

## CPC

- B81C 1/00825: {Protect against mechanical threats, e.g. against shocks, or residues (B81C1/00261 take precedence)}
- B81C 1/00873: {characterised by special arrangements of the devices, allowing an easier separation}
- B81C 99/008: {separating the processed structure from a mother substrate}
- B81B 2201/0257: Microphones or microspeakers
- B81C 2201/0194: the layer being structured
- B81C 2203/054: using structural alignment aids, e.g. spacers, interposers, male/female parts, rods or balls
- B81C: PROCESSES OR APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OR TREATMENT OF MICROSTRUCTURAL DEVICES OR SYSTEMS (making microcapsules or microballoons B01J13/02; processes or apparatus specially adapted for the manufacture or treatment of piezoelectric, electrostrictive or magnetostrictive elements per se H10N30/01)
- B81B: MICROSTRUCTURAL DEVICES OR SYSTEMS, e.g. MICROMECHANICAL DEVICES (piezoelectric, electrostrictive or magnetostrictive elements per se H10N30/00, H10N35/00)

## Abstract

The present disclosure relates to a method for fabricating a micro-electromechanical system (MEMS) device. In the method, a carrier wafer is received. A MEMS wafer, which includes a plurality of die, is bonded to the carrier wafer. A cavity is formed to separate an upper surface of the carrier wafer from a lower surface of a die of the MEMS wafer. A separation trench is formed to laterally surround the die, wherein formation of the cavity and the separation trench leaves a tethering structure suspending the die over the upper surface of the carrier wafer. The die and carrier wafer are translated with respect to one another to break the tethering structure and separate the die from the carrier wafer.

## Claims

### Claim 1

A method for fabricating a micro-electromechanical system (MEMS) device, the method comprising:
receiving a carrier wafer;
bonding a MEMS wafer, which includes a plurality of die, to the carrier wafer;
forming a cavity separating an upper surface of the carrier wafer from a lower surface of a die of the MEMS wafer;
forming a separation trench that laterally surrounds the die, wherein formation of the cavity and the separation trench leaves a tethering structure suspending the die over the upper surface of the carrier wafer; and
translating the die and carrier wafer with respect to one another to break the tethering structure and separate the die from the carrier wafer.

### Claim 2 (depends on 1)

The method of claim 1, wherein separating the die from the carrier wafer leaves the carrier wafer intact.

### Claim 3 (depends on 1)

The method of claim 1, wherein formation of the separation trench leaves an anchor support structure extending upwardly from the upper surface of the carrier wafer, the anchor support structure laterally surrounding the separation trench, and wherein the tethering structure includes a plurality of projections that each extend over the separation trench to suspend the die over the upper surface of the carrier wafer.

### Claim 4 (depends on 1)

The method of claim 1, wherein the MEMS wafer, when bonded to the carrier wafer, is initially separated from the carrier wafer by an intermediate oxide layer; and
wherein the cavity is formed by removing at least some portions of intermediate oxide layer.

### Claim 5 (depends on 4)

The method of claim 4, wherein the carrier wafer has a first face and a second face opposite the first face, the intermediate oxide being in contact with the first face, the method further comprising:
affixing tape to the second face of the carrier wafer; and
after the tape has been affixed to the second face of the carrier wafer, translating the die and carrier wafer with respect to one another to break the tethering structure.

### Claim 6 (depends on 1)

The method of claim 1, further comprising:
after the MEMS wafer has been bonded to the carrier wafer, reducing a thickness of the MEMS wafer to a desired MEMS substrate thickness.

### Claim 7 (depends on 6)

The method of claim 6, wherein the desired MEMS substrate thickness is in a range of 20 μm to 400 μm.

### Claim 8 (depends on 1)

The method of claim 1, wherein the die includes a MEMS microphone having a diaphragm and back plates.

### Claim 9

A method for fabricating a micro-electromechanical system (MEMS) device, the method comprising:
receiving a carrier wafer bonded to an intermediate oxide layer;
bonding a MEMS wafer to the intermediate oxide layer;
etching the MEMS wafer to form a separation trench;
forming a MEMS structure in or over the MEMS wafer, wherein the MEMS structure includes a dielectric structure and a tethering structure spanning the separation trench;
etching the carrier wafer, the intermediate oxide layer, and the MEMS wafer to form a recess;
removing a first portion of material from the dielectric structure overlying the recess; and
plucking the MEMS structure from the carrier wafer by breaking the tethering structure.

### Claim 10 (depends on 9)

The method of claim 9, wherein the tethering structure includes a plurality of projections that are stacked in parallel over one another over the separation trench.

### Claim 11 (depends on 10)

The method of claim 10, wherein the MEMS wafer has a thickness in a range of 20 μm to 400 μm.

### Claim 12 (depends on 9)

The method of claim 9, wherein after the separation trench has been formed, an anchor support structure extends upwards from an upper surface of the carrier wafer and laterally surrounds the separation trench, and wherein the tethering structure includes a plurality of projections that each extend over the separation trench to suspend the MEMS structure over the upper surface of the carrier wafer.

### Claim 13 (depends on 9)

The method of claim 9, wherein removing the first portion of material from the dielectric structure includes etching using vapor-phase hydrofluoric acid.

### Claim 14 (depends on 9)

The method of claim 9, wherein the carrier wafer has a first face and a second face opposite the first face, the intermediate oxide being in contact with the first face, the method further comprising:
affixing tape to the second face of the carrier wafer; and
after the tape has been affixed to the second face of the carrier wafer, translating the MEMS structure with respect to the carrier wafer to break the tethering structure.

### Claim 15 (depends on 9)

The method of claim 9, wherein the MEMS structure is MEMS microphone having a diaphragm and back plates.

### Claim at position 16

16-20. (canceled)

### Claim 21

A method for fabricating a micro-electromechanical system (MEMS) device, the method comprising:
receiving a carrier wafer;
bonding a MEMS wafer, which includes a plurality of die, to the carrier wafer;
forming a cavity separating an upper surface of the carrier wafer from a lower surface of a die of the MEMS wafer;
forming a separation trench that laterally surrounds the die, wherein formation of the cavity and the separation trench leaves a tethering structure suspending the die over the upper surface of the carrier wafer, wherein the tethering structure includes a plurality of projections that each extend over the separation trench to suspend the die over the upper surface of the carrier wafer; and
translating the die and carrier wafer with respect to one another to break the tethering structure and separate the die from the carrier wafer leaving the carrier wafer intact.

### Claim 22 (depends on 21)

The method of claim 21, wherein formation of the separation trench leaves an anchor support structure extending upwardly from the upper surface of the carrier wafer, the anchor support structure laterally surrounding the separation trench.

### Claim 23 (depends on 21)

The method of claim 21, wherein the MEMS wafer, when bonded to the carrier wafer, is initially separated from the carrier wafer by an intermediate oxide layer; and
wherein the cavity is formed by removing at least some portions of intermediate oxide layer.

### Claim 24 (depends on 23)

The method of claim 23, wherein the carrier wafer has a first face and a second face opposite the first face, the intermediate oxide being in contact with the first face, the method further comprising:
affixing tape to the second face of the carrier wafer; and
after the tape has been affixed to the second face of the carrier wafer, translating the die and carrier wafer with respect to one another to break the tethering structure.

### Claim 25 (depends on 21)

The method of claim 21, further comprising:
after the MEMS wafer has been bonded to the carrier wafer, reducing a thickness of the MEMS wafer to a desired MEMS substrate thickness.