# US 2018/0022140 A1 · Pressure-sensitive adhesives for bonding flexible printing plates

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0022140 A1
- Document ID: US20180022140A1
- Status: Published application
- Kind: A1
- Application number: 15/652,989
- Filed: 2017-07-18
- Published: 2018-01-25
- Earliest claimed: 2016-07-19
- Assignees: Tesa SE
- Applicants: tesa SE
- Inventors: KAI ELLRINGMANN; KRISTIN KERBER; BENJAMIN PÜTZ
- Web page: https://patentgrep.com/patent/US20180022140A1

## CPC

- B41N 6/00: Mounting boards; {Sleeves} Make-ready devices, e.g. underlays, overlays; Attaching by chemical means, e.g. vulcanising
- B41N 6/02: Chemical means for fastening printing formes on mounting boards
- C08L 31/04: Homopolymers or copolymers of vinyl acetate
- C09J 5/00: Adhesive processes in general; Adhesive processes not provided for elsewhere, e.g. relating to primers
- C09J 133/08: Homopolymers or copolymers of acrylic acid esters
- C09J 2431/00: Presence of polyvinyl acetate
- C09J 2433/00: Presence of (meth)acrylic polymer
- B41N: PRINTING PLATES OR FOILS (photosensitive material G03); MATERIALS FOR SURFACES USED IN PRINTING MACHINES FOR PRINTING, INKING, DAMPING, OR THE LIKE; PREPARING SUCH SURFACES FOR USE AND CONSERVING THEM
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)

## Abstract

Pressure-sensitive adhesives and methods, for bonding flexible printing plates, comprising at least one adhesive component comprising at least one polymer component based on a monomer mixture comprising at least one of the following monomers: at least one acrylic ester; at least one methacrylic ester; acrylic acid; and methacrylic acid. The pressure-sensitive adhesives further comprise 1 to 30 wt %, based on the overall blend of the at least one adhesive component without solvent, of a polyvinyl acetate.

## Claims

### Claim 1

A method comprising:
bonding of one or more printing plates to at least one selected from one or more printing cylinders and one or more printing sleeves with a pressure-sensitive adhesive comprising at least one adhesive component comprising at least one polymer component based on a monomer mixture comprising at least one of the following monomers:
at least one acrylic ester;
at least one methacrylic ester;
acrylic acid; and
methacrylic acid,
wherein the pressure-sensitive adhesive further comprises
1 to 30 wt %, based on the overall blend of the at least one adhesive component without solvent, of a polyvinyl acetate.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the polyvinyl acetate has a molar mass Mn of 10,000 to 100,000 g/mol.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the monomer mixture comprises at least the following monomers:
a) 20 to 99.5 wt % of at least one first acrylic ester and/or methacrylic ester whose homopolymer has a static glass transition temperature of <0° C.;
b) 0 to 40 wt % of at least one second acrylic ester and/or methacrylic ester whose homopolymer has a static glass transition temperature of >0° C.;
c) 0.5 to 20 wt % of acrylic acid and/or methacrylic acid; and
d) 0 to 25 wt % of further copolymerizable monomers, the quantity figures being based in each case on the monomer mixture.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the monomer mixture comprises at least the following monomers:
i.a) 50-99.5 wt % of at least one acrylic ester and/or methacrylic ester having the following formula:
CH2═C(R1)(COOR2), where
R1═H and R2 is a linear alkyl radical having 2 to 10 carbon atoms or is a branched, non-cyclic alkyl radical having at least 4 carbon atoms, and/or
R1═CH3 and R2 is a linear alkyl radical having 8 to 10 carbon atoms or is a branched, non-cyclic alkyl radical having at least 10 carbon atoms;
i.b) 0 to 40 wt % of at least one acrylic ester and/or methacrylic ester having the following formula:
CH2═C(R3)(COOR4), where
R3═H or CH3 and R4 is a linear alkyl radical having at least 12 carbon atoms, preferably a stearyl radical;
i.c) 0.5-20 wt % of acrylic acid and/or methacrylic acid; and
i.d) 0-25 wt % of at least one N-alkyl-substituted acrylamide, where the quantity figures are based in each case on the monomer mixture.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the monomer mixture comprises at least the following monomers:
ii.a) 49.5-89.5 wt % of at least one acrylic ester and/or methacrylic ester and/or their free acids, having the following formula:
CH2═C(R5)(COOR6), where
R5═H or CH3 and R6 is an alkyl radical having 1 to 10 carbon atoms or H and the homopolymer has a static glass transition temperature of <−30° C.;
ii.b) 10 to 40 wt % of at least one acrylic ester and/or methacrylic ester having the following formula:
CH2═C(R7)(COOR6), where
R7═H or CH3 and R8 is a cyclic alkyl radical having at least 8 carbon atoms or is a linear alkyl radical having at least 12 carbon atoms and the homopolymer has a static glass transition temperature Tg of at least 30° C.; and
ii.c) 0.5 to 10 wt % of at least one acrylic ester and/or methacrylic ester and/or their free acids, having the following formula:
CH2═C(R9)(COOR10), where
R9═H or CH3 and R10═H or an aliphatic radical having a functional group X, where X comprises COOH, OH, —NH(R11), SH, SO3H, and the homopolymer has a static glass transition temperature Tg of at least 30° C., where R11═H or a linear or branched alkyl radical having up to 10 carbon atoms,
wherein the quantity figures are based in each case on the monomer mixture.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the monomer mixture comprises at least the following monomers:
iii.a) 25 to 82 wt % of linear acrylic esters having 2 to 10 carbon atoms in the alkyl radical;
iii.b) 10 to 40 wt % of branched, non-cyclic acrylic esters having a static glass transition temperature Tg of not more than 0° C., preferably not more than −10° C., more particularly not more than −20° C.;
iii.c) 8 to 15 wt % of acrylic acid, based on the total amount of monomers to be polymerized; and
iii.d) optionally up to 10 wt % of further copolymerizable monomers, based on the total amount of monomers to be polymerized,
wherein the ratio of the linear acrylic esters to the branched acrylic esters is in the range from 1:6 to 10:1 mass fractions.

### Claim 7 (depends on 3)

The method according to claim 3, wherein the polymer component or polymer components based on monomer mixtures comprising the monomers a) to d) or i.a) to i.d) or ii.a) to ii.c) or iii.a) to iii.d) make(s) up at least 90 wt % of the adhesive component or components.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the pressure-sensitive adhesive is in crosslinked form.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the pressure-sensitive adhesive is provided in the form of an adhesive tape.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the pressure-sensitive adhesive further comprises 5 to 25 wt %, based on the overall blend of the at least one adhesive component without solvent, of the polyvinyl acetate.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the pressure-sensitive adhesive further comprises 7 to 20 wt %, based on the overall blend of the at least one adhesive component without solvent, of the polyvinyl acetate.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the pressure-sensitive adhesive further comprises 10 to 15 wt %, based on the overall blend of the at least one adhesive component without solvent, of the polyvinyl acetate.

### Claim 13 (depends on 2)

The method according to claim 2, wherein the polyvinyl acetate has a molar mass Mn of 15,000 to 25,000 g/mol.

### Claim 14 (depends on 3)

The method according to claim 3, wherein the at least one first acrylic ester and/or methacrylic ester whose homopolymer has a static glass transition temperature of <−20° C. and the at least one second acrylic ester and/or methacrylic ester whose homopolymer has a static glass transition temperature of >20° C.

### Claim 15 (depends on 7)

The method according to claim 7, wherein the polymer component or polymer components based on monomer mixtures comprising the monomers a) to d) or i.a) to i.d) or ii.a) to ii.c) or iii.a) to iii.d) make(s) up at least 99.9 wt % of the adhesive component or components.