# US 2018/0022024 A1 · Resin powder for solid freeform fabrication, device for solid freeform fabrication object, and method of manufacturing solid freeform fabrication object

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0022024 A1
- Document ID: US20180022024A1
- Status: Published application
- Kind: A1
- Application number: 15/656,248
- Filed: 2017-07-21
- Published: 2018-01-25
- Earliest claimed: 2016-07-22
- Assignees: Ricoh Company, Ltd.
- Inventors: Akira SAITO; Yasuyuki YAMASHITA; Kiichi KAMODA; Shigenori YAGUCHI; Nozomu TAMOTO; Hitoshi IWATSUKI; Shinzo HIGUCHI; Sohichiroh llDA; Yasuo SUZUKI
- Web page: https://patentgrep.com/patent/US20180022024A1

## CPC

- B29C 64/153: using layers of powder being selectively joined, e.g. by selective laser sintering or melting
- B29B 9/12: characterised by structure or composition
- B29B 9/16: Auxiliary treatment of granules
- B33Y 70/00: Materials specially adapted for additive manufacturing
- B33Y 70/10: Composites of different types of material, e.g. mixtures of ceramics and polymers or mixtures of metals and biomaterials
- C08F 110/06: Propene
- C08G 8/02: of ketones
- C08G 63/183: Terephthalic acids
- C08G 67/00: Macromolecular compounds obtained by reactions forming in the main chain of the macromolecule a linkage containing oxygen or oxygen and carbon, not provided for in groups C08G2/00 - C08G65/00
- C08G 69/26: derived from polyamines and polycarboxylic acids
- C08J 3/12: Powdering or granulating
- C08K 3/016: Flame-proofing or flame-retarding additives
- C08K 5/0066: {Flame-proofing or flame-retarding additives}
- B29B 2009/125: {Micropellets, microgranules, microparticles}
- B29K 2101/12: Thermoplastic materials
- B29K 2105/251: {Particles, powder or granules (expandable particles B29K2105/046)}
- B29K 2995/0041: Crystalline
- B33Y 10/00: Processes of additive manufacturing
- C08J 2361/00: Characterised by the use of condensation polymers of aldehydes or ketones; Derivatives of such polymers
- C08J 2361/16: of ketones with phenols
- C08J 2367/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds; (C08J2367/06 takes precedence)
- C08J 2367/04: Polyesters derived from hydroxy carboxylic acids, e.g. lactones (C08J2367/06 takes precedence)
- C08J 2377/02: Polyamides derived from omega-amino carboxylic acids or from lactams thereof (C08J2377/10 takes precedence)
- C08J 2377/08: from polyamines and polymerised unsaturated fatty acids
- C08J 2377/10: Polyamides derived from aromatically bound amino and carboxyl groups of amino carboxylic acids or of polyamines and polycarboxylic acids
- Y02P 10/25: Process efficiency
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29B: PREPARATION OR PRETREATMENT OF THE MATERIAL TO BE SHAPED; MAKING GRANULES OR PREFORMS; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIAL CONTAINING PLASTICS
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A resin powder for solid freeform fabrication has a 50 percent cumulative volume particle diameter of from 5 to 100 μm and a ratio (Mv/Mn) of a volume average particle diameter (Mv) to the number average particle diameter (Mn) of 2.50 or less and satisfies at least one of the following conditions (1) to (3): (1): Tmf1>Tmf2 and (Tmf1−Tmf2)≧3 degrees C., both Tmf1 and Tmf2 are measured in differential scanning calorimetry measuring according to ISO 3146, (2): Cd1>Cd2 and (Cd1−Cd2)≧3 percent, both Cd1 and Cd2 are measured in differential scanning calorimetry measuring according to ISO 3146, and (3): C×1>C×2 and (C1−C2)≧3 percent.

## Claims

### Claim 1

Resin powder for solid freeform fabrication wherein the resin powder has a 50 percent cumulative volume particle diameter of from 5 to 100 μm and a ratio (Mv/Mn) of a volume average particle diameter (Mv) to a number average particle diameter (Mn) of 2.50 or less and satisfies at least one of the following conditions (1) to (3):
(1): Tmf1>Tmf2 and (Tmf1−Tmf2)≧3 degrees C., where Tmf1 represents a melting starting temperature of an endothermic peak as the resin powder is heated to a temperature 30 degrees C. higher than a melting point of the resin powder at a temperature rising speed of 10 degrees C. per minute for a first time and Tmf2 represents a melting starting temperature of an endothermic peak as the resin powder is heated for the first time, cooled down to −30 degrees C. or lower at a temperature falling speed of 10 degrees C. per minute, and heated to the temperature 30 degrees C. higher than the melting point at a temperature rising speed of 10 degrees C. per minute for a second time, and both Tmf1 and Tmf2 are measured in differential scanning calorimetry measuring according to ISO 3146, wherein the melting starting temperature of the endothermic peak represents a temperature at a point −15 mW lower from a straight line parallel to X axis drawn from a site where quantity of heat becomes constant after endotherm at the melting point finishes to a lower temperature side,
(2): Cd1>Cd2 and (Cd1−Cd2)≧3 percent, where Cd1 represents a crystallinity obtained from an energy amount of the endothermic peak when the resin powder is heated to a temperature 30 degrees C. higher than the melting point of the resin powder at a temperature rising speed of 10 degrees C. per minute for a first time and Cd2 represents a crystallinity obtained from an energy amount of the endothermic peak as the resin powder is heated for the first time, cooled down to −30 degrees C. or lower at a temperature falling speed of 10 degrees C. per minute, and heated to the temperature 30 degrees C. higher than the melting point at a temperature rising speed of 10 degrees C. per minute for a second time, and both Cd1 and Cd2 are measured in differential scanning calorimetry measuring according to ISO 3146, and
(3): C×1>C×2 and (C×1−C×2)≧3 percent, where C×1 represents a crystallinity of the resin powder obtained by X-ray diffraction measuring and C×2 represents a crystallinity obtained by X-ray diffraction measuring as the resin powder is heated to the temperature 30 degrees C. higher than the melting point thereof at a temperature rising speed of 10 degrees C. per minute, cooled down to −30 degrees C. or lower at a temperature falling speed of 10 degrees C. per minute, and thereafter heated to the temperature 30 degrees C. higher than the melting point at a temperature rising speed of 10 degrees C. per minute in nitrogen atmosphere.

### Claim 2 (depends on 1)

The resin powder according to claim 1, wherein the 50 percent cumulative volume particle diameter is from 20 to 70 μm.

### Claim 3 (depends on 1)

The resin powder according to claim 1, wherein the resin powder has a melting point of 100 degrees C. or higher as measured according to ISO 3146.

### Claim 4 (depends on 1)

The resin powder according to claim 1, wherein the ratio (Mv/Mn) is 1.50 or less.

### Claim 5 (depends on 1)

The resin powder according to claim 1, further comprising at least one member selected from the group consisting of polyolefin, polyamide, polyester, polyarylketone, polyphenylene sulfide, a liquid crystal polymer, polyacetal, polyimide, and a fluorochemical resin.

### Claim 6 (depends on 5)

The resin powder according to claim 5, wherein polyamide includes at least one member selected from the group including aromatic polyamides consisting of polyamide 410, polyamide 4T, polyamide 6, polyamide 66, polyamide MXD6, polyamide 610, polyamide 6T, polyamide 11, polyamide 12, polyamide 9T, polyamide 10T, and aramid.

### Claim 7 (depends on 5)

The resin powder according to claim 5, wherein polyester includes at least one member selected from the group consisting of polyethylene terephthalate, polybutylene terephthalate, and polylactate.

### Claim 8 (depends on 5)

The resin powder according to claim 5, wherein polyaryl ketone includes at least one member selected from the group consisting of polyether ether ketone, polyether ketone, and polyether ketone ketone.

### Claim 9 (depends on 1)

The resin powder according to claim 1, wherein the resin powder has an average circularity of 0.83 or greater in a range in which the resin powder has a particle diameter of from 0.5 to 200 μm.

### Claim 10 (depends on 1)

The resin powder according to claim 1, further comprising a toughening agent.

### Claim 11 (depends on 1)

The resin powder according to claim 1, further comprising a flame retardant.

### Claim 12 (depends on 1)

A device for manufacturing a solid freeform fabrication object, comprising:
a layer forming device configured to form a layer including the resin powder of claim 1; and
a powder attaching device configured to attach the resin powder to each other in a selected area of the layer.

### Claim 13 (depends on 1)

A method of manufacturing a solid freeform fabrication object, comprising:
forming a layer including the resin powder of claim 1;
irradiating the layer with electromagnetic wave to melt the layer; and
cooling down the layer to cure the layer;
wherein the forming, the irradiating, and the cooling down and are repeated.