# US 2018/0021981 A1 · Method for recovering silicon particles and abrasive grains from wasted abrasive slurry

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0021981 A1
- Document ID: US20180021981A1
- Status: Published application
- Kind: A1
- Application number: 15/653,388
- Filed: 2017-07-18
- Published: 2018-01-25
- Earliest claimed: 2016-07-20
- Assignees: GET Green Energy Corp., Ltd.; Long-Jin Li
- Applicants: Get Green Energy Corp., Ltd.
- Inventors: Po-Nien Lai; Shin-Lee Liu; Huang-Chih Lu
- Web page: https://patentgrep.com/patent/US20180021981A1

## CPC

- B28D 5/007: {Use, recovery or regeneration of abrasive mediums (for grinding and polishing in general B24B57/00)}
- B23Q 11/1069: {Filtration systems specially adapted for cutting liquids (filtration in general B01D24/00 - B01D41/00)}
- C01B 33/02: Silicon (forming single crystals or homogeneous polycrystalline material with defined structure C30B)
- C10N 2040/22: with essential removal of material {, e.g. cutting, grinding or drilling}
- B28D: WORKING STONE OR STONE-LIKE MATERIALS
- B23Q: DETAILS, COMPONENTS, OR ACCESSORIES FOR MACHINE TOOLS, e.g. ARRANGEMENTS FOR COPYING OR CONTROLLING (tools of the kind used in lathes or boring machines B23B27/00); MACHINE TOOLS IN GENERAL CHARACTERISED BY THE CONSTRUCTION OF PARTICULAR DETAILS OR COMPONENTS; COMBINATIONS OR ASSOCIATIONS OF METAL-WORKING MACHINES, NOT DIRECTED TO A PARTICULAR RESULT
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C10N: INDEXING SCHEME ASSOCIATED WITH SUBCLASS C10M RELATING TO LUBRICATING COMPOSITIONS

## Abstract

Disclosed herein is a method for recovering silicon particles and abrasive grains from a wasted abrasive slurry. The method includes providing a wasted abrasive slurry that contains silicon particles, abrasive grains and a water-soluble glycol, and mixing the wasted abrasive slurry with a metal chloride solution, so as to obtain a micelle layer and a slurry layer, the micelle layer including the water-soluble glycol, and the slurry layer including the silicon particles and the abrasive grains.

## Claims

### Claim 1

A method for recovering silicon particles and abrasive grains from a wasted abrasive slurry, comprising:
providing a wasted abrasive slurry that contains silicon particles, abrasive grains and a water-soluble glycol; and
mixing the wasted abrasive slurry that contains silicon particles, abrasive grains and a water-soluble glycol with a metal chloride solution, so as to obtain a micelle layer and a slurry layer, the micelle layer including the water-soluble glycol, and the slurry layer including the silicon particles and the abrasive grains.

### Claim 2 (depends on 1)

The method of claim 1, further comprising subjecting the slurry layer to a separation treatment, so as to obtain an aqueous supernatant and a precipitate that includes the silicon particles and the abrasive grains.

### Claim 3 (depends on 2)

The method of claim 2, further comprising adding an acid solution into the precipitate so as to separate the silicon particles and the abrasive grains.

### Claim 4 (depends on 3)

The method of claim 3, wherein the acid solution is an organic acid solution.

### Claim 5 (depends on 1)

The method of claim 1, wherein the abrasive grains are selected from the group consisting of silicon carbide grains, aluminium oxide grains, zirconium oxide grains, yttrium oxide grains, brown corundum grains, white corundum grains, and combinations thereof.

### Claim 6 (depends on 1)

The method of claim 1, wherein the water-soluble glycol is selected from the group consisting of diol, polyol and the combination thereof.

### Claim 7 (depends on 6)

The method of claim 6, wherein the water-soluble glycol is selected from the group consisting of polyethylene glycol, diethylene glycol, ethylene glycol, and combinations thereof.

### Claim 8 (depends on 1)

The method of claim 1, wherein the metal chloride solution is selected from the group consisting of alkali metal chloride solution, alkaline earth metal chloride solution and the combination thereof.

### Claim 9 (depends on 1)

The method of claim 1, wherein the weight ratio of the metal chloride solution to the water-soluble glycol is 1:0.5 to 1:3.

### Claim 10 (depends on 1)

The method of claim 1, wherein mixing the wasted abrasive slurry with the metal chloride solution is performed at a temperature ranging from 25° C. to 70° C.