# US 2018/0021895 A1 · Field girth welding technology for high manganese steel slurry pipelines

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0021895 A1
- Document ID: US20180021895A1
- Status: Published application
- Kind: A1
- Application number: 15/584,794
- Filed: 2017-05-02
- Published: 2018-01-25
- Earliest claimed: 2016-05-02
- Assignees: ExxonMobil Research and Engineering Company; Posco
- Applicants: Exxonmobil Research and Engineering Company; Posco
- Inventors: Andrew J. Wasson; Timothy D. Anderson; Douglas P. Fairchild; Xin Yue; HyunWoo Jin; Ning Ma; IIWook Han; Sangchul Lee; Bongkeun Lee; Jongsub Lee
- Web page: https://patentgrep.com/patent/US20180021895A1

## CPC

- B23K 35/3073: {with Mn as next major constituent}
- B23K 9/025: for rectilinear seams
- B23K 9/09: Arrangements or circuits for arc welding with pulsed current or voltage
- B23K 9/16: making use of shielding gas
- B23K 9/173: and of a consumable electrode
- B23K 9/23: taking account of the properties of the materials to be welded
- B23K 35/0261: {Rods, electrodes or wires}
- B23K 35/383: {mainly containing noble gases or nitrogen}
- C22C 38/02: containing silicon
- C22C 38/22: with molybdenum or tungsten
- C22C 38/38: with more than 1.5% by weight of manganese
- C22C 38/44: with molybdenum or tungsten
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C22C 38/58: with more than 1.5% by weight of manganese
- B23K 2103/04: Steel {or steel} alloys
- C21D 2211/001: Austenite
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)

## Abstract

The present disclosure relates to a welding composition for joining high manganese steel base metals and methods of applying the same. The composition includes: carbon in a range of about 0.4 wt % to about 0.8 wt %; manganese in a range of about 18 wt % to about 24 wt %; chromium in an amount of ≦about 6 wt %; molybdenum in an amount of ≦about 4 wt %; nickel in an amount of ≦about 5 wt %; silicon in an amount of about 0.4 wt % to about 1.0 wt %; sulfur in an amount of ≦about 200 ppm; phosphorus in an amount of ≦about 200 ppm; and a balance including iron. In an embodiment, the composition has an austenitic phase.

## Claims

### Claim 1

A welding composition for high manganese steel base metals, the composition comprising:
carbon in a range of about 0.4 wt % to about 0.8 wt %;
manganese in a range of about 18 wt % to about 24 wt %;
chromium in an amount of about ≦6 wt %;
molybdenum in an amount of about ≦4 wt %;
nickel in an amount of about ≦5 wt %;
silicon in an amount of about 0.4 wt % to about 1.0 wt %;
sulfur in an amount of about ≦200 ppm;
phosphorus in an amount of about ≦200 ppm; and
the balance comprising iron.

### Claim 2 (depends on 1)

The composition of claim 1, further comprising at least one of:
titanium in an amount of about ≦2 wt %;
niobium in an amount of about ≦5 wt %;
tungsten in an amount of about ≦5 wt %;
aluminum in an amount of about ≦1.0 wt %;
boron in an amount of about ≦0.1 wt %;
nitrogen in an amount of about ≦1.5 wt % or a combination thereof.

### Claim 3 (depends on 1)

The composition of claim 1, wherein the composition has an austenitic microstructure.

### Claim 4 (depends on 3)

The composition of claim 3, wherein the austenitic microstructure transforms into hard α′-martensite and undergoes microtwinning upon straining.

### Claim 5

A system for providing erosion/corrosion resistant high manganese welds, the system comprising:
a consumable wire electrode producing a weldment comprising carbon in a range of about 0.4 wt % to about 0.8 wt %, manganese in a range of about 18 wt % to about 24 wt %, chromium in an amount of about ≦6 wt %, molybdenum in an amount of about ≦4 wt %, nickel in an amount of about ≦5 wt %, silicon in a range of about 0.4 wt % to about 1.0 wt %, sulfur in an amount of about ≦200 ppm, phosphorus in an amount of about ≦200 ppm, and a balance comprising iron; and
a gas metal arc welding power source that perform gas metal are welding, wherein the gas metal arc welding power source produces a welding heat input no more than about 2.5 kJ/mm.

### Claim 6 (depends on 5)

The system of claim 5, wherein the welding heat input is in a range of about 0.6 to about 1.0 kJ/mm.

### Claim 7 (depends on 5)

The system of claim 5, further comprising an apparatus for providing at least one shielding gas.

### Claim 8 (depends on 7)

The system of claim 7, wherein the at least one shielding gas includes CO2 in a range of about 10% to 30%.

### Claim 9 (depends on 7)

The system of claim 7, wherein the at least one shielding gas comprises about 80% Argon and about 20% CO2.

### Claim 10

A method of producing a weld deposit of erosion/corrosion resistant high Mn steel, the method comprising:
providing at least two high Mn steel bases to be welded, and a weldment comprising carbon in a range of about 0.4 wt % to about 0.8 wt %, manganese in a range of about 18 wt % to about 24 wt %, chromium in an amount of about ≦6 wt %, molybdenum in an amount of about ≦4 wt %, nickel in an amount of about ≦5 wt %, silicon in a range of about 0.4 wt % to about 1.0 wt %, sulfur in an amount of about ≦200 ppm, phosphorus in an amount of about ≦200 ppm, and a balance comprising iron; and
melting and cooling the welding filler material to create a weld deposit.

### Claim 11 (depends on 10)

The method of claim 10, wherein melting comprising providing a welding heat input no more than about 2.5 kJ/mm to the welding filler metal.

### Claim 12 (depends on 10)

The method of claim 10, wherein the at least two high Mn steel bases comprise a portion to be welded, the portions having bevels of about 30 degrees to about 37.5 degrees.

### Claim 13 (depends on 10)

The method of claim 10, wherein the weld deposition has a yield strength in the as-welded condition greater than a yield strength of a high manganese steel base.

### Claim 14 (depends on 10)

The method of claim 10, wherein the weld deposit has a yield strength in the as-welded condition greater than about 70 ksi.

### Claim 15 (depends on 10)

The method of claim 10, wherein the weld deposit has an ultimate tensile strength in the as-welded condition greater than about 82.7 ksi.

### Claim 16 (depends on 10)

The method of claim 10, wherein the weld deposit has a tensile elongation in the as-welded condition greater than about 16%.

### Claim 17 (depends on 10)

The method of claim 10, wherein the weld deposit has a solidification cracking temperature range in the as-welded condition of about 40° C. to about 170° C. at 7% strain.

### Claim 18 (depends on 10)

The method of claim 10, wherein the weld deposit and/or a heat affected zone of the bases has a CVN energy at −29° C. in the as-welded condition greater than 27 J.

### Claim 19 (depends on 10)

The method of claim 10, wherein the base steel is an erosion/corrosion resistant high Mn steel.

### Claim 20 (depends on 10)

The method of claim 10, further comprising limiting carbon content in the weld metal to an amount less than an amount of carbon in a heat affected zone of the base metal.