# US 2018/0021857 A1 · Method of preparing tungsten metal material and tungsten target with high purity

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0021857 A1
- Document ID: US20180021857A1
- Status: Published application
- Kind: A1
- Application number: 15/365,776
- Filed: 2016-11-30
- Published: 2018-01-25
- Earliest claimed: 2016-07-20
- Assignees: National Chung Shan Institute of Science and Technology
- Applicants: National Chung Shan Institute of Science and Technology
- Inventors: CHIA-SHIH LIN; CHAO-NAN WEI; CUO-YO NIEH; HUI-YUN BOR; KUAN-ZONG FUNG
- Web page: https://patentgrep.com/patent/US20180021857A1

## CPC

- B22F 9/30: with decomposition of metal compounds, e.g. by pyrolysis
- B22F 1/09: {Mixtures of metallic powders}
- B22F 3/1017: {Multiple heating or additional steps (B22F3/101 takes precedence)}
- B22F 9/04: starting from solid material, e.g. by crushing, grinding or milling ({C22C1/1084 takes precedence}; crushing, grinding or milling, in general, see the relevant subclasses, e.g. B02C)
- B22F 2009/043: {by ball milling}
- B22F 2301/20: Refractory metals
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER

## Abstract

A method of preparing a tungsten metal material with high purity, comprising the steps of (A) providing a tungsten metal powder to mix with a metal nitrate to form a mixed powder slurry; (B) ball-grinding the mixed powder slurry to obtain a uniformly mixed powder; (C) sintering the uniformly mixed powder to obtain the tungsten metal material with high purity. Accordingly, the tungsten metal material with purity more than 99.9% can be prepared, so as to prepare the tungsten metal target.

## Claims

### Claim 1

A method of preparing a tungsten metal material with high purity, comprising the steps of:
(A) providing a tungsten metal powder to mix with a metal nitrate to form a mixed powder slurry;
(B) ball-grinding the mixed powder slurry to obtain a uniformly mixed powder;
(C) sintering the uniformly mixed powder to obtain the tungsten metal material with high purity.

### Claim 2 (depends on 1)

The method of preparing a tungsten metal material with high purity as claimed in claim 1, wherein the purity of the tungsten metal material with high purity is more than 99.9%, and the density thereof is more than 99% of the density of pure tungsten.

### Claim 3 (depends on 2)

The method of preparing a tungsten metal material with high purity as claimed in claim 2, wherein the tungsten metal material with high purity is used to prepare a tungsten metal target.

### Claim 4 (depends on 3)

The method of preparing a tungsten metal material with high purity as claimed in claim 3, wherein before the sintering step (C), the uniformly mixed powder is further pressed and shaped to a desired shape.

### Claim 5 (depends on 1)

The method of preparing a tungsten metal material with high purity as claimed in claim 1, wherein the metal nitrate is selected from nickel nitrate, ferric nitrate, and a mixture thereof.

### Claim 6 (depends on 1)

The method of preparing a tungsten metal material with high purity as claimed in claim 1, wherein a solvent is added to the mixed powder slurry in the ball-grinding step (B), and the solvent is oleic acid.

### Claim 7 (depends on 1)

The method of preparing a tungsten metal material with high purity as claimed in claim 1, wherein the sintering treatment include a plurality of stages of heating treatments.

### Claim 8 (depends on 7)

The method of preparing a tungsten metal material with high purity as claimed in claim 7, wherein the temperature in the first stage of heating treatments of the sintering treatment is more than 200° C.

### Claim 9 (depends on 7)

The method of preparing a tungsten metal material with high purity as claimed in claim 7, wherein the temperature in the last stage of heating treatments of the sintering treatment is more than 1400° C.

### Claim 10 (depends on 1)

The method of preparing a tungsten metal material with high purity as claimed in claim 1, wherein after the ball-grinding step (B), a heating/drying process and a filtering process are further performed.