# US 2018/0021851 A1 · Method for manufacturing clock hardware by means of blocky metallic glass

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0021851 A1
- Document ID: US20180021851A1
- Status: Published application
- Kind: A1
- Application number: 15/215,818
- Filed: 2016-07-21
- Published: 2018-01-25
- Earliest claimed: 2016-07-21
- Assignees: BMG Metallurgy limited
- Applicants: BMG Metallurgy limited
- Inventors: Chi Fai WONG
- Web page: https://patentgrep.com/patent/US20180021851A1

## CPC

- B22D 27/04: Influencing the temperature of the metal, e.g. by heating or cooling the mould
- B22D 17/14: Machines with evacuated die cavity
- C22C 1/11: Making amorphous alloys
- C22C 45/10: with molybdenum, tungsten, niobium, tantalum, titanium, or zirconium {or Hf} as the major constituent
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

The present invention relates to the technical field of clock machining, in particular to a method for manufacturing clock hardware by means of blocky metallic glass. According to the present invention, the rapid cooling technique is adopted, complicated hardware can also be formed at a time, errors are extremely small, the precision is high, smooth surfaces can also be formed on the edges of the gear teeth of a manufactured gear, and the clock movement assembly accuracy is improved; the manufacturing technique is simple, the production time is short, the production efficiency is high, the required effect can be achieved without polishing the surface of the manufactured hardware, the product quality is improved, labor is greatly saved, time is saved, and environmental friendliness is achieved.

## Claims

### Claim 1

A method for manufacturing clock hardware by means of blocky metallic glass, characterized by comprising the following steps of:
A. heating raw metal constituting the blocky metallic glass to the temperature of 1400-1500° C. so that the raw metal can be liquefied to form molten metal;
B. vacuumizing a mold cavity of a mold;
C. injecting the molten metal into the mold cavity;
D. pressurizing the mold cavity so that the mold cavity can be filled with the molten metal and rapidly cooling the molten metal in the mold cavity at the same time so that the molten metal can be solidified to form a blocky metallic glass structure.

### Claim 2 (depends on 1)

The method for manufacturing the clock hardware by means of the blocky metallic glass according to claim 1, characterized in that the blocky metallic glass is Zr-based blocky metallic glass.

### Claim 3 (depends on 1)

The method for manufacturing the clock hardware by means of the blocky metallic glass according to claim 1, characterized in that the raw metal of the blocky metallic glass is at least prepared from Zr, Fe, Ni, Cu, Ti, Mn, Si, Pd and Co through mixing.

### Claim 4 (depends on 3)

The method for manufacturing the clock hardware by means of the blocky metallic glass according to claim 3, characterized in that the raw metal of the blocky metallic glass comprises, by weight, 35-50 parts of Zr, 5-8 parts of Fe, 4-9 parts of Ni, 11-16 parts of Cu, 6-8 parts of Ti, 5-9 parts of Mn, 10-15 parts of Si, 1-2 parts of Pd and 1-2 parts of Co.

### Claim 5 (depends on 1)

The method for manufacturing the clock hardware by means of the blocky metallic glass according to claim 1, characterized in that argon is introduced for protection in the process of step A.

### Claim 6 (depends on 1)

The method for manufacturing the clock hardware by means of the blocky metallic glass according to claim 1, characterized in that the mold cavity is pressurized through inflation in step C.

### Claim 7 (depends on 1)

The method for manufacturing the clock hardware by means of the blocky metallic glass according to claims 1, characterized in that a cooling pipeline system is arranged in the mold in advance in step D, and the molten metal in the mold cavity is rapidly cooled through the cooling pipeline system.

### Claim 8 (depends on 2)

The method for manufacturing the clock hardware by means of the blocky metallic glass according to claims 2, characterized in that a cooling pipeline system is arranged in the mold in advance in step D, and the molten metal in the mold cavity is rapidly cooled through the cooling pipeline system.

### Claim 9 (depends on 3)

The method for manufacturing the clock hardware by means of the blocky metallic glass according to claims 3, characterized in that a cooling pipeline system is arranged in the mold in advance in step D, and the molten metal in the mold cavity is rapidly cooled through the cooling pipeline system.

### Claim 10 (depends on 4)

The method for manufacturing the clock hardware by means of the blocky metallic glass according to claims 4, characterized in that a cooling pipeline system is arranged in the mold in advance in step D, and the molten metal in the mold cavity is rapidly cooled through the cooling pipeline system.

### Claim 11 (depends on 5)

The method for manufacturing the clock hardware by means of the blocky metallic glass according to claims 5, characterized in that a cooling pipeline system is arranged in the mold in advance in step D, and the molten metal in the mold cavity is rapidly cooled through the cooling pipeline system.

### Claim 12 (depends on 6)

The method for manufacturing the clock hardware by means of the blocky metallic glass according to claims 6, characterized in that a cooling pipeline system is arranged in the mold in advance in step D, and the molten metal in the mold cavity is rapidly cooled through the cooling pipeline system.