# US 2018/0021761 A1 · Suspended-Bed Hydrogenation Catalyst and Regeneration Method Therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0021761 A1
- Document ID: US20180021761A1
- Status: Published application
- Kind: A1
- Application number: 15/656,671
- Filed: 2017-07-21
- Published: 2018-01-25
- Earliest claimed: 2016-07-22
- Assignees: Beijing Huashi United Energy Technology and Development Co., Ltd.
- Applicants: Beijing Huashi United Energy Technology and Development Co., Ltd.
- Inventors: Lin Li; Ke Lin; Chuntao Li
- Web page: https://patentgrep.com/patent/US20180021761A1

## CPC

- B01J 29/166: {Y-type faujasite}
- B01J 29/146: {Y-type faujasite}
- B01J 29/46: Iron group metals or copper
- B01J 29/48: containing arsenic, antimony, bismuth, vanadium, niobium tantalum, polonium, chromium, molybdenum, tungsten, manganese, technetium or rhenium
- B01J 29/80: Mixtures of different zeolites
- B01J 29/90: Regeneration or reactivation
- B01J 35/40: characterised by dimensions, e.g. grain size (in a colloidal state B01J35/23; crystallite size B01J35/77)
- B01J 35/695: {polymodal}
- B01J 37/0036: {Grinding}
- B01J 37/009: {Preparation by separation, e.g. by filtration, decantation, screening}
- B01J 37/06: Washing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/084: {Decomposition of carbon-containing compounds into carbon}
- B01J 37/088: {Decomposition of a metal salt}
- B01J 38/02: Heat treatment
- B01J 38/06: using steam
- B01J 38/72: including segregation of diverse particles
- C10G 49/04: containing nickel, cobalt, chromium, molybdenum, or tungsten metals, or compounds thereof
- C10G 49/08: containing crystalline alumino-silicates, e.g. molecular sieves
- B01J 2229/186: not in framework positions
- B01J 2229/20: to introduce other elements in the catalyst composition comprising the molecular sieve, but not specially in or on the molecular sieve itself
- B01J 2229/36: Steaming
- B01J 2229/37: Acid treatment
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C10G: CRACKING HYDROCARBON OILS; PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVE HYDROGENATION, OLIGOMERISATION, POLYMERISATION (cracking to hydrogen or synthesis gas C01B; cracking or pyrolysis of hydrocarbon gases to individual hydrocarbons or mixtures thereof of definite or specified constitution C07C; cracking to cokes C10B); RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, OR GASES; REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS; REFORMING OF NAPHTHA; MINERAL WAXES

## Abstract

A suspended-bed hydrogenation catalyst and a regeneration method are disclosed. A composite support comprises a semi-coke pore-expanding material, a molecular sieve and a spent catalytic cracking catalyst. The hydrogenation catalyst for heavy oil is obtained through mixing the semi-coke pore-expanding material, the molecular sieve and the spent catalytic cracking catalyst, followed by molding, calcining and activating, and then loading an active metal oxide to the composite support. According to the composite support, a macropore, mesopore and micropore uniformly-distributed structure is formed, so that full contact between all ingredients in the heavy oil and active ingredients in a hydrogenation process is facilitated, and the conversion ratio of the heavy oil is increased. The hydrogenation catalyst integrates adsorption, cracking and hydrogenation properties. According to a regeneration method, the loading performance of an active-metal-loaded support in a spent hydrogenation catalyst cannot be destroyed.

## Claims

### Claim 1

A catalyst composite support, comprising
a semi-coke pore-expanding material,
a molecular sieve and
a spent catalytic cracking catalyst,
wherein the mass ratio of the semi-coke pore-expanding material to the molecular sieve to the spent catalytic cracking catalyst is (1 to 5): (2 to 4): (0.5 to 5);
the semi-coke pore-expanding material has a specific surface area of 150 m2/g to 300 m2/g and an average pore size of 70 nm to 80 nm;
the molecular sieve has a specific surface area of 200 m2/g to 300 m2/g and an average pore size of 5 nm to 10 nm; and
the spent catalytic cracking catalyst has a specific surface area of 50 m2/g to 300 m2/g and an average pore size of 3 nm to 7 nm.

### Claim 2 (depends on 1)

The composite support according to claim 1, wherein the semi-coke pore-expanding material has an average particle size of 60 to 100 microns and an average pore volume of 2 cm3/g to 3 cm3/g.

### Claim 3 (depends on 1)

The composite support according to claim 1, wherein the molecular sieve has an average particle size of 1 mm to 4 mm.

### Claim 4 (depends on 1)

The composite support according to claim 1, wherein the spent catalytic cracking catalyst has an average particle size of no greater than 150 microns.

### Claim 5 (depends on 1)

The composite support according to claim 1, wherein on the basis of the mass of the spent catalytic cracking catalyst, the spent catalytic cracking catalyst comprises the following ingredients in parts by mass:
Y-type molecular sieve 15-55 parts;
aluminum oxide 15-55 parts; and
at least one of nickel, vanadium and ferrum 0.5-1 part.

### Claim 6 (depends on 1)

A preparation method for the catalyst composite support according to claim 1, characterized by comprising the following steps:
(S1) mixing the semi-coke pore-expanding material, the molecular sieve and the spent catalytic cracking catalyst, followed by molding to obtain a molded material;
(S2) calcining the molded material in an oxygen-free condition to obtain a calcined material; and
(S3) activating the calcined material with a gas to obtain the catalyst composite support.

### Claim 7 (depends on 6)

The preparation method according to claim 6, wherein the step (S1) further comprises the step of
separately grinding the semi-coke pore-expanding material, the molecular sieve and the spent catalytic cracking catalyst prior to mixing, or
grinding the molded material obtained by mixing the semi-coke pore-expanding material, the molecular sieve and the spent catalytic cracking catalyst.

### Claim 8 (depends on 6)

The preparation method according to claim 6, wherein the calcining is carried out at a temperature of 650 DEG C. to 750 DEG C. for a period of 1.5 to 2.5 hours.

### Claim 9 (depends on 6)

The preparation method according to claim 6, wherein in the step (S3), the gas is an oxidizing gas; and
the activating is carried out at a temperature of 900 DEG C. to 950 DEG C. for a period of 1.5 to 2 hours.

### Claim 10 (depends on 1)

A hydrogenation catalyst, comprising
the catalyst composite support according to claim 1, and
an active metal oxide loaded onto the catalyst composite support.

### Claim 11 (depends on 10)

The hydrogenation catalyst according to claim 10, wherein the active metal oxide is selected from VIII metal oxide, VIB metal oxide, or a mixture thereof;
the mass ratio of the composite support to active metals in the active metal oxide is 100:(0.5 to 10); and
the mass ratio of the VIII metal oxide to the VIB metal oxide is (1 to 20):(0.5 to 10).

### Claim 12

A method for regenerating a spent hydrogenation catalyst, comprising the following steps:
(S1) carrying out dry distillation treatment on the spent hydrogenation catalyst to obtain a dehydrated and deoiled catalyst A and a dry distillation gas;
(S2) activating the catalyst A to obtain a catalyst B; and
(S3) grinding the catalyst B to obtain a regenerated hydrogenation catalyst.

### Claim 13 (depends on 12)

The method according to claim 12, wherein the dry distillation treatment is carried out at a temperature of 400 DEG C. to 800 DEG C. for a period of 2 to 2.5 hours.

### Claim 14 (depends on 13)

The method according to claim 13, wherein the dry distillation treatment is carried out at a temperature of 600 DEG C. to 800 DEG C. for a period of 2 to 2.5 hours.

### Claim 15 (depends on 12)

The method according to claim 12, wherein the activating is carried out at a temperature of 850 DEG C. to 950 DEG C. for a period of 0.5 to 2 hours.

### Claim 16 (depends on 12)

The method according to claim 12, wherein water vapor is used as an activator in the activating.

### Claim 17 (depends on 12)

The method according to claim 12, wherein in the step (S3), the catalyst B is ground into powder with a grain size of 20 to 200 microns.

### Claim 18 (depends on 12)

The method according to claim 12, wherein the spent hydrogenation catalyst is obtained through carrying out solid-liquid separation on a liquid mixture of a spent catalyst and a heavy oil product discharged from the bottom of a vacuum distillation tower after suspended-bed hydrogenation of a heavy oil feedstock.

### Claim 19 (depends on 12)

The method according to claim 12, wherein the method further comprises the steps of:
carrying out dust removal on the dry distillation gas to obtain a dust and a dedusted dry distillation gas,
mixing the dust with the catalyst A,
cooling the dedusted dry distillation gas to obtain a high-boiling-point oil-water mixture and a combustible low-boiling-point gas, and
subjecting the high-boiling-point oil-water mixture to oil-water separation, thereby obtaining crude product oil and oil-containing wastewater.

### Claim 20 (depends on 10, 12)

The method according to claim 12, wherein the spent hydrogenation catalyst is a spent catalyst generated after the hydrogenation catalyst according to claim 10 is subjected to a hydrogenation process.