# US 2018/0002217 A1 · Method of making optical fiber preform with pressed soot

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0002217 A1
- Document ID: US20180002217A1
- Status: Published application
- Kind: A1
- Application number: 15/631,808
- Filed: 2017-06-23
- Published: 2018-01-04
- Earliest claimed: 2016-06-30
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Daniel Robert Boughton; James Gerard Fagan; Larry Gleason Hubbard, JR.; Ji Wang
- Web page: https://patentgrep.com/patent/US20180002217A1

## CPC

- C03B 37/014: made entirely or partially by chemical means {, e.g. vapour phase deposition of bulk porous glass either by outside vapour deposition [OVD], or by outside vapour phase oxidation [OVPO] or by vapour axial deposition [VAD] (C03C17/02 takes precedence)}
- C03B 37/01217: {for making preforms of polarisation-maintaining optical fibres (polarisation-maintaining optical fibres per se G02B6/105)}
- C03B 37/01222: {for making preforms of multiple core optical fibres (preforms of multifibres C03B37/01214)}
- C03B 37/01282: {by pressing or sintering, e.g. hot-pressing}
- C03B 37/0142: {Reactant deposition burners}
- C03B 2201/06: Doped silica-based glasses
- C03B 2201/10: doped with boron (C03B2201/14 takes precedence)
- C03B 2203/14: Non-solid, i.e. hollow products, e.g. hollow clad or with core-clad interface
- C03B 2203/30: Polarisation maintaining [PM], i.e. birefringent products, e.g. with elliptical core, by use of stress rods, "PANDA" type fibres
- C03B 2203/31: by use of stress-imparting rods, e.g. by insertion
- C03B 2203/34: Plural core other than bundles, e.g. double core
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES

## Abstract

According to some embodiments method for making an optical fiber preform comprises the steps of: (i) placing a plurality of rods with an outer surface having a coefficient of friction 0.02≦COF≦0.3 into an inner cavity of an apparatus; (ii) placing particulate glass material in the inner cavity between the rods and an inner wall of the mold cavity; and (iii) applying pressure against the particulate glass material to press the particulate glass material against the plurality of rods.

## Claims

### Claim 1

A method for forming an optical fiber preform comprising the steps of:
(I) placing a plurality of rods into a mold cavity of an apparatus, wherein at least one of the plurality of rods is (i) a graphite rod; or (ii) a metal or ceramic rod having a coating, the coating comprising at least one of: graphite, graphene, amorphous silicon (a-silicon), an amorphous carbon (a-c); xylan flouropolymer, composites of xylan with other polymers, diamond-like carbon (DLC), boron nitride, molydisulfide (molybdenum disulfide), tungsten disulfide, electroless nickel infused with Teflon, nickel infused with SiC;
(II) placing particulate glass material in the mold cavity between the rods and an inner wall of the mold cavity; and
(III) applying pressure against the particulate glass material to press the particulate glass material against the plurality of rods.

### Claim 2 (depends on 1)

The method of claim 1, wherein at least one of the plurality of rods has an outer surface with a coefficient of friction COF≦0.3.

### Claim 3 (depends on 2)

The method of claim 2, wherein at least one of the plurality of rods has an outer surface with a coefficient of friction COF≦0.15.

### Claim 4 (depends on 2)

The method of claim 2, wherein at least one of the plurality of rods has an outer surface with a coefficient of friction COF≦0.1.

### Claim 5 (depends on 1)

The method for making an optical fiber preform according to claim 1, wherein the pressure is applied at least radially inwards against the particulate glass material to pressurize the particulate glass material against the plurality of rods.

### Claim 6 (depends on 2)

The method of claim 2, wherein at least two of the plurality of rods are graphite rods, and wherein at least one of the plurality of rods is a core cane situated therebetween.

### Claim 7 (depends on 1)

The method of claim 1, wherein prior to the step of applying pressure against the particulate glass material, the particulate glass material has an average density of from 0.1 to 0.5 grams per cubic centimeter and wherein subsequent to the step of applying pressure against the particulate glass material, the pressed particulate glass material has a density of from 0.6 to 1.2 grams per cubic centimeter.

### Claim 8 (depends on 1)

The method of claim 1, wherein the step of applying pressure against the particulate glass material comprises the step of applying radial pressure, and wherein prior to the step of applying pressure against the particulate glass material, the particulate glass material has an average density of from 0.1 to 0.5 grams per cubic centimeter and wherein subsequent to the step of applying a radial pressure against the particulate glass material, the pressed particulate glass material has a density of from 0.6 to 1.2 grams per cubic centimeter.

### Claim 9

A method for making an optical fiber preform comprising the steps of:
placing a plurality of rods into a mold cavity of an apparatus, wherein at least two of the plurality of rods comprise an outer surface with a coefficient of friction COF and 0.02≦COF≦0.3;
placing particulate glass material in the mold cavity between the rods and an inner wall of the mold cavity; and
applying pressure against the particulate glass material to press the particulate glass material against the plurality of rods.

### Claim 10 (depends on 9)

The method of claim 9, wherein 0.05≦COF≦0.3.

### Claim 11 (depends on 9)

The method of claim 9, wherein at least two of the plurality of rods are graphite rods.

### Claim 12 (depends on 9)

The method of claim 9, wherein at least two of the plurality of rods include at least one of: a graphite coating, an amorphous silicon (a-silicon) coating, amorphous carbon (a-c) coating.

### Claim 13 (depends on 9)

The method of claim 9, wherein at least two of said plurality of rods are metal or ceramic rods each having at least one of the following coatings: graphite, graphene, amorphous silicon (a-silicon), Teflon, amorphous carbon (a-c); xylan flouropolymer, composites of xylan with other polymers, diamond-like carbon (DLC), boron nitride, molydisulfide (molybdenum disulfide), tungsten disulfide, electroless nickel infused with Teflon, nickel infused with SiC.

### Claim 14 (depends on 9)

The method for making an optical fiber preform according to claim 9, wherein the pressure is applied at least radially inwards against the particulate glass material to press the particulate glass material against the plurality of rods.

### Claim 15 (depends on 9)

The method for making an optical fiber preform according to claim 9, wherein the plurality of rods comprises: (i) at least one glass rod; and (ii) at least two mold rods; and said pressure is applied axially and/or radially.

### Claim 16 (depends on 9)

The method for making an optical fiber preform according to claim 9, wherein the apparatus comprises an outer wall, the outer wall surrounding the inner wall; the pressure is applied at least radially inwards, and the pressure has a magnitude from 25 psig to 250 psig.

### Claim 17 (depends on 9)

The method of claim 9, wherein at least one of the plurality of rods is a core cane situated along the axial center of the mold cavity.

### Claim 18 (depends on 9)

The method of claim 9, wherein at least one of the plurality of rods comprises a consolidated core cane surrounded by a porous soot clad layer and the core cane is situated along the axial center of said mold cavity.

### Claim 19 (depends on 9)

The method of claim 9, wherein prior to the step of applying a radial pressure against the particulate glass material, the particulate glass material has an average density of from 0.1 to 0.5 grams per cubic centimeter and wherein subsequent to the step of applying a radial pressure against the particulate glass material, the pressed particulate glass material has a density of from 0.6 to 1.2 grams per cubic centimeter.

### Claim 20 (depends on 9)

The method of claim 9 wherein the plurality of rods are arranged co-linearly within the mold cavity.

### Claim 21

A method of making an optical fiber, the method comprising the steps of:
(I) placing a plurality of rods into a mold cavity of an apparatus, wherein at least one of the plurality of rods is (i) a graphite rod; or (ii) a metal or ceramic rod having a coating thereon, the coating comprising at least one of: graphite, graphene, amorphous silicon coating (a-silicon), an amorphous carbon (a-c); xylan flouropolymer, composites of xylan with other polymers, diamond-like carbon (DLC), boron nitride, molydisulfide (molybdenum disulfide), tungsten disulfide, electroless nickel infused with Teflon, nickel infused with SiC;
(II) placing particulate glass material in the mold cavity between the rods and inner wall of the mold cavity;
(III) forming a soot compact by applying pressure against the particulate glass material to press the particulate glass material against the plurality of rods;
(IV) removing the least one of said plurality of rods from the soot compact, thereby to format least one void within the soot compact;
(V) and forming an optical fiber preform assembly by inserting at least one glass rod into the at least one void;
(VI) and forming the optical fiber preform by sintering the optical fiber preform; and
(VII) drawing an optical fiber from the optical fiber preform.

### Claim 22

A method of making an optical fiber, the method comprising the steps of:
(I) placing a plurality of rods into a mold cavity of an apparatus, wherein at least two of the plurality of rods comprise an outer surface with a coefficient of friction COF, and 0.02≦COF≦0.3;
(II) placing particulate glass material in the mold cavity between the rods and an the inner wall of the mold cavity;
(III) forming a soot compact by applying pressure against the particulate glass material to press the particulate glass material against the plurality of rods, and;
(IV) removing at least two of the plurality of rods from the soot compact to form at least two voids within the soot compact;
(V) forming an optical fiber preform assembly by inserting at glass rods into said voids;
(VI) forming the optical fiber preform by sintering the optical fiber preform assembly; and
(VII) drawing an optical fiber from the optical fiber preform.

### Claim 23

A method of making an optical fiber, the method comprising the steps of:
(I) placing a plurality of rods into a mold cavity of an apparatus, wherein at least two of the plurality of rods comprise an outer surface with a coefficient of friction COF, and 0.02≦COF≦0.3;
(II) placing particulate glass material in the mold cavity between the rods and an inner wall of the mold cavity;
(III) forming a soot compact by applying pressure against the particulate glass material to press the particulate glass material against the plurality of rods, and;
(IV) forming an optical preform assembly by removing the at least two of the plurality of rods from the soot compact to form at least two voids within the soot compact;
(V) sintering the optical fiber preform assembly and forming the optical fiber preform; and
(VI) drawing an optical fiber from the optical fiber preform.