# US 2017/0373324 A1 · Anode for solid oxide fuel cell and production method therefor, and method for producing electrolyte layer-electrode assembly for fuel cell

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0373324 A1
- Document ID: US20170373324A1
- Status: Published application
- Kind: A1
- Application number: 15/526,831
- Filed: 2015-07-21
- Published: 2017-12-28
- Earliest claimed: 2014-11-21
- Assignees: Sumitomo Electric Industries, Ltd.
- Applicants: Sumitomo Electric Industries, Ltd.
- Inventors: Yohei NODA; Masatoshi MAJIMA; Hiromasa TAWARAYAMA; Naho MIZUHARA; Chihiro HIRAIWA; Takahiro HIGASHINO
- Web page: https://patentgrep.com/patent/US20170373324A1

## CPC

- H01M 4/8875: {Methods for shaping the electrode into free-standing bodies, like sheets, films or grids, e.g. moulding, hot-pressing, casting without support, extrusion without support}
- H01M 4/86: Inert electrodes with catalytic activity, e.g. for fuel cells
- H01M 4/88: Processes of manufacture
- H01M 4/8885: {Sintering or firing}
- H01M 4/9033: {Complex oxides, optionally doped, of the type M1MeO3, M1 being an alkaline earth metal or a rare earth, Me being a metal, e.g. perovskites}
- H01M 8/02: Details (electrodes H01M4/86 - H01M4/98)
- H01M 8/12: operating at high temperature, e.g. with stabilised ZrO2 electrolyte
- H01M 8/1213: characterised by the electrode/electrolyte combination or the supporting material
- H01M 8/124: characterised by the process of manufacturing or by the material of the electrolyte
- H01M 2004/8684: {Negative electrodes}
- H01M 2008/1293: {Fuel cells with solid oxide electrolytes}
- Y02E 60/50: Fuel cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for producing an anode capable of increasing output of a solid oxide fuel cell is provided. The method for producing an anode for a solid oxide fuel cell includes a first step of shaping a mixture that contains a perovskite oxide having proton conductivity and a nickel compound and a second step of firing a shaped product, which has been obtained in the first step, in an atmosphere containing 50% by volume or more of oxygen at 1100° C. to 1350° C. so as to generate an anode.

## Claims

### Claim 1

A method for producing an anode for a solid oxide fuel cell, the method comprising:
a first step of shaping a mixture that contains a perovskite oxide having proton conductivity and a nickel compound; and
a second step of firing a shaped product, which has been obtained in the first step, in an atmosphere containing 50% by volume or more of oxygen at 1100° C. to 1350° C. so as to generate an anode.

### Claim 2 (depends on 1)

The method for producing an anode for a solid oxide fuel cell according to claim 1, wherein the perovskite oxide has an AXO3 crystal structure where A sites contain Ba and X sites contain Ce and Y.

### Claim 3 (depends on 1)

The method for producing an anode for a solid oxide fuel cell according to claim 1, wherein, in the mixture, a volume ratio of the nickel compound to the perovskite oxide is 50/50 to 75/25.

### Claim 4 (depends on 1)

The method for producing an anode for a solid oxide fuel cell according to claim 1, wherein, in the second step, the shaped product is fired in an atmosphere containing 80% by volume or more of oxygen at 1200° C. to 1350° C.

### Claim 5 (depends on 1)

The method for producing an anode for a solid oxide fuel cell according to claim 1, wherein the mixture further contains a binder, and
the method further comprises, after the first step and before the second step, a step of removing the binder by heating the shaped product at a temperature of 450° C. or higher and lower than 800° C.

### Claim 6 (depends on 1)

The method for producing an anode for a solid oxide fuel cell according to claim 1, further comprising, after the first step and before the second step, a step of calcining the shaped product at a temperature of 800° C. or higher and lower than 1100° C.

### Claim 7 (depends on 1)

An anode for a solid oxide fuel cell, obtained through the method according to claim 1.

### Claim 8

A method for producing an electrolyte layer-electrode assembly for a fuel cell, the electrolyte layer-electrode assembly including a solid electrolyte layer and an anode that supports the solid electrolyte layer, the method comprising:
a step A of shaping a mixture of a perovskite oxide having proton conductivity and nickel oxide;
a step B of forming a coating film on one of main surfaces of a shaped product, which has been obtained in the step A, by using a paste that contains a perovskite oxide having proton conductivity; and
a step C of firing the shaped product with the coating film thereon in an atmosphere containing 50% by volume or more of oxygen at 1100° C. to 1350° C. so as to generate the anode from the shaped product and the solid electrolyte layer from the coating film and integrate the anode and the solid electrolyte layer.