# US 2017/0372953 A1 · Cvd based oxide-metal multi structure for 3d nand memory devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0372953 A1
- Document ID: US20170372953A1
- Status: Published application
- Kind: A1
- Application number: 15/633,366
- Filed: 2017-06-26
- Published: 2017-12-28
- Earliest claimed: 2016-06-28
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Susmit Singha ROY; Kelvin CHAN; Hien Minh LE; Sanjay KAMATH; Abhijit Basu MALLICK; Srinivas GANDIKOTA; Karthik JANAKIRAMAN
- Web page: https://patentgrep.com/patent/US20170372953A1

## CPC

- H10P 14/40: of conductive or resistive materials
- C23C 16/0272: {Deposition of sub-layers, e.g. to promote the adhesion of the main coating}
- C23C 16/06: characterised by the deposition of metallic material
- C23C 16/402: {Silicon dioxide}
- C23C 16/505: using radio frequency discharges
- C23C 28/322: {only coatings of metal elements only}
- C23C 28/34: {including at least one inorganic non-metallic material layer, e.g. metal carbide, nitride, boride, silicide layer and their mixtures, enamels, phosphates and sulphates}
- C23C 28/345: {with at least one oxide layer}
- C23C 28/42: {characterized by the composition of the alternating layers}
- H10P 14/3211: {Silicon, silicon germanium or germanium}
- H10P 14/3216: {Nitrides}
- H10P 14/3241: {being conductive materials}
- H10P 14/412: {Deposition of metallic or metal-silicide materials}
- H10P 14/418: {the conductive layers comprising transition metals}
- H10P 14/43: Chemical deposition, e.g. chemical vapour deposition [CVD]
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6506: {Formation of intermediate materials}
- H10P 14/6514: {by exposure to a plasma}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10W 20/045: {for deposition from the gaseous phase, e.g. for chemical vapour deposition [CVD]}
- H10B 43/27: the channels comprising vertical portions, e.g. U-shaped channels
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

Implementations described herein generally relate to a method for forming a metal layer and to a method for forming an oxide layer on the metal layer. In one implementation, the metal layer is formed on a seed layer, and the seed layer helps the metal in the metal layer nucleate with small grain size without affecting the conductivity of the metal layer. The metal layer may be formed using plasma enhanced chemical vapor deposition (PECVD) and nitrogen gas may be flowed into the processing chamber along with the precursor gases. In another implementation, a barrier layer is formed on the metal layer in order to prevent the metal layer from being oxidized during subsequent oxide layer deposition process. In another implementation, the metal layer is treated prior to the deposition of the oxide layer in order to prevent the metal layer from being oxidized.

## Claims

### Claim 1

A method, comprising:
placing a substrate into a processing chamber; and
forming a metal-containing layer on the substrate, wherein the forming a metal-containing layer on the substrate comprises:
increasing a temperature of the substrate to a processing temperature;
flowing a metal-containing precursor and nitrogen gas into the processing chamber, wherein a ratio of a flow rate of the metal-containing precursor to a flow rate of the nitrogen gas ranges from 10:1 to 1:3; and
forming a plasma inside of the processing chamber by igniting the metal-containing precursor and nitrogen gas with a high frequency radio frequency power and a low frequency radio frequency power.

### Claim 2 (depends on 1)

The method of claim 1, further comprising forming a seed layer on the substrate, wherein the metal-containing layer is formed on the seed layer.

### Claim 3 (depends on 2)

The method of claim 2, wherein the seed layer comprises titanium nitride, molybdenum nitride, tungsten nitride, amorphous boron, or amorphous silicon.

### Claim 4 (depends on 1)

The method of claim 1, wherein the metal-containing layer comprises cobalt, molybdenum, tungsten, tantalum, titanium, ruthenium, rhodium, copper, iron, manganese, vanadium, niobium, hafnium, zirconium, yttrium, aluminum, tin, chromium, or lanthanum.

### Claim 5 (depends on 1)

The method of claim 1, wherein the metal-containing layer comprises metal nitrides, metal silicides, or metal silicon nitrides.

### Claim 6 (depends on 1)

The method of claim 1, wherein the processing temperature ranges from about 350 degrees Celsius to about 450 degrees Celsius.

### Claim 7 (depends on 6)

The method of claim 6, wherein the ratio of a flow rate of the metal-containing precursor to a flow rate of the nitrogen gas ranges from 10:1 to 1:2.

### Claim 8 (depends on 6)

The method of claim 6, wherein the low frequency radio frequency power ranges from about 0.071 W/cm2 to about 0.283 W/cm2.

### Claim 9 (depends on 1)

The method of claim 1, wherein the processing temperature ranges from about 500 degrees Celsius to about 600 degrees Celsius.

### Claim 10 (depends on 9)

The method of claim 9, wherein the ratio of a flow rate of the metal-containing precursor to a flow rate of the nitrogen gas ranges from 5:1 to 1:3.

### Claim 11 (depends on 9)

The method of claim 9, wherein the low frequency radio frequency power ranges from about 0.071 W/cm2 to about 0.566 W/cm2.

### Claim 12

A method, comprising:
placing a substrate into a processing chamber;
forming a metal layer on the substrate;
treating a surface of the metal layer with a nitrogen-containing plasma; and
forming an oxide layer on the treated surface of the metal layer.

### Claim 13 (depends on 12)

The method of claim 12, wherein the nitrogen-containing plasma is formed by flowing a nitrogen-containing gas into the processing chamber and igniting the nitrogen-containing gas.

### Claim 14

A method, comprising:
placing a substrate into a processing chamber;
forming a metal layer on the substrate; and
forming an oxide layer on the metal layer, wherein the forming an oxide layer comprises:
flowing an oxygen-free precursor into the processing chamber, wherein the oxygen-free precursor is excited by a plasma to form oxygen-free species;
flowing an oxygen-containing gas into the processing chamber, wherein the oxygen-containing gas is excited by the plasma to form oxygen species; and
bonding the oxygen-free species to the oxygen species.

### Claim 15 (depends on 14)

The method of claim 14, further comprising flowing one or more non-reactive gases into the processing chamber prior to flowing an oxygen-free precursor into the processing chamber.

### Claim 16 (depends on 15)

The method of claim 15, wherein the one or more non-reactive gases comprises argon and hydrogen gas.

### Claim 17 (depends on 14)

The method of claim 14, wherein the oxygen-free precursor is a silicon-containing precursor.

### Claim 18 (depends on 17)

The method of claim 17, wherein the oxygen-free precursor is silane.

### Claim 19 (depends on 14)

The method of claim 14, wherein the oxygen-containing gas is oxygen gas.

### Claim 20 (depends on 14)

The method of claim 14, wherein the metal layer is tungsten and the oxide layer is silicon oxide.