# US 2017/0372944 A1 · Methods for fabricating trench isolation structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0372944 A1
- Document ID: US20170372944A1
- Status: Published application
- Kind: A1
- Application number: 15/193,632
- Filed: 2016-06-27
- Published: 2017-12-28
- Earliest claimed: 2016-06-27
- Assignees: Vanguard International Semiconductor Corporation
- Applicants: Vanguard International Semiconductor Corporation
- Inventors: Shin-Hao LIU; Chih-Cherng LIAO; Ching-Yi HSU; Yun-Chou WEI
- Web page: https://patentgrep.com/patent/US20170372944A1

## CPC

- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10W 10/0145: {of trenches having shapes other than rectangular or V-shape (H10W10/0143 takes precedence)}
- H10P 74/203: {Structural properties, e.g. testing or measuring thicknesses, line widths, warpage, bond strengths or physical defects}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method for fabricating a trench isolation structure is provided. The method includes providing a substrate and forming a patterned mask layer on the substrate. A first etching step is performed on the substrate by using the patterned mask layer to form a trench in the substrate. A dielectric material is formed in the trench and on the patterned mask layer, wherein the dielectric material on the patterned mask layer has a first height. An etch back step is performed to decrease the dielectric material on the patterned mask layer to a second height. A planarization process is performed to remove the dielectric material on the patterned mask layer, where a polishing pad is used, and a first pressure and a second pressure are respectively applied on a central portion and a peripheral portion of the polishing pad, wherein the second pressure is greater than the first pressure.

## Claims

### Claim 1

A method for fabricating a trench isolation structure, comprising:
providing a substrate;
forming a patterned mask layer on the substrate;
performing a first etching step to the substrate by using the patterned mask layer to form a trench in the substrate;
forming a dielectric material in the trench and on the patterned mask layer, wherein the dielectric material on the patterned mask layer has a first height;
performing an etch back step to decrease the dielectric material on the patterned mask layer from the first height to a second height;
performing a second etching step to the dielectric material on the patterned mask layer, wherein after the second etching step, the dielectric material on the patterned mask layer has a third height that is 2%-3.5% of the second height; and
performing a planarization process to remove the dielectric material on the patterned mask layer, wherein a polishing pad is used during the planarization process, a first pressure is applied on a central portion of the polishing pad, a second pressure is applied on a peripheral portion of the polishing pad, and the second pressure is greater than the first pressure.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein the first etching step comprises a top corner rounding process to form a rounding corner between a sidewall of the trench and a top surface of the substrate.

### Claim 3 (depends on 1)

The method as claimed in claim 1, further comprising after forming the trench and before forming the dielectric layer, performing a pullback process to the patterned mask layer such that an opening of the patterned mask layer has a width larger than a width of the trench.

### Claim 4 (depends on 3)

The method as claimed in claim 3, further comprising after performing the pullback process and before forming the dielectric layer, forming an oxide liner layer on a sidewall and a bottom of the trench.

### Claim 5 (depends on 4)

The method as claimed in claim 4, further comprising performing an annealing process to the oxide liner layer.

### Claim 6 (depends on 1)

The method as claimed in claim 1, wherein the step of forming the dielectric material comprises performing a high-density plasma chemical vapor deposition process.

### Claim 7 (depends on 1)

The method as claimed in claim 1, wherein the etch back step comprises a sputter etch back process.

### Claim 8 (depends on 1)

The method as claimed in claim 1, wherein the difference between the second height and the first height is 0.2 μm-0.3 μm.

### Claim 9

(canceled)

### Claim 10 (depends on 1)

The method as claimed in claim 1, wherein the second etching step comprises a dry-etching process, and the dry-etching process has an etch selectivity ratio of the patterned mask layer to the dielectric material being 1:20-1:25.

### Claim 11

(canceled)

### Claim 12 (depends on 1)

The method as claimed in claim 1, wherein the peripheral portion of the polishing pad has a width in a direction from an edge of the polishing pad to a central point of the polishing pad being 35%-50% of the radius of the polishing pad.

### Claim 13 (depends on 1)

The method as claimed in claim 1, wherein the difference between the second pressure and the first pressure is 30 psi-40 psi.

### Claim 14 (depends on 1)

The method as claimed in claim 1, wherein the patterned mask layer comprises a pad oxide layer and a silicon nitride layer disposed on the pad oxide layer.

### Claim 15 (depends on 1)

The method as claimed in claim 1, wherein the trench has an aspect ratio between 0.375 and 0.5.