# US 2017/0372903 A1 · Method for doping semiconductors

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0372903 A1
- Document ID: US20170372903A1
- Status: Published application
- Kind: A1
- Application number: 15/540,618
- Filed: 2015-12-01
- Published: 2017-12-28
- Earliest claimed: 2014-12-30
- Assignees: Merck Patent GmbH
- Applicants: Merck Patent GmbH
- Inventors: Oliver DOLL; Ingo KOEHLER; Sebastian BARTH
- Web page: https://patentgrep.com/patent/US20170372903A1

## CPC

- H10P 32/19: {Diffusion sources}
- H10F 71/121: {The active layers comprising only Group IV materials}
- H10F 77/1223: characterised by the dopants
- Y02E 10/547: Monocrystalline silicon PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present invention relates to a process for the production of structured, highly efficient solar cells and of photovoltaic elements which have regions of different doping. The invention likewise relates to the solar cells having increased efficiency produced in this way.

## Claims

### Claim 1

Process for the direct doping of a silicon substrate, characterised in that
a) a doping paste which is suitable as sol-gel for the formation of oxide layers and comprises at least one doping element selected from the group boron, gallium, silicon, germanium, zinc, tin, phosphorus, titanium, zirconium, yttrium, nickel, cobalt, iron, cerium, niobium, arsenic and lead is printed onto the substrate surface, over the entire surface or selectively, and dried,
b) this step is optionally repeated with a doping paste of the same or different composition,
c) doping by diffusion is optionally carried out by temperature treatment at temperatures in the range from 750 to 1100° C.,
d) doping of the substrate is carried out by laser irradiation,
and
e) repair of the damage induced in the substrate by the laser irradiation is optionally carried out by a tubular furnace step or in-line diffusion step at elevated temperature,
and
f) when the doping is complete, the glass layer formed from the applied paste is removed again,
where steps b) to e) can, depending on the desired doping result, be carried out in a different sequence and optionally repeated.

### Claim 2 (depends on 1)

Process according to claim 1, characterised in that a temperature treatment is carried out at temperatures in the range from 750 to 1100° C. for the doping by diffusion after laser irradiation for doping of the substrate, where repair of the damage induced in the substrate by the laser irradiation is carried out at the same time.

### Claim 3 (depends on 1)

Process according to claim 1, characterised in that a doping paste which is suitable for the formation of oxide layers and comprises at least one doping element selected from the group boron, phosphorus, antimony, arsenic and gallium is printed on.

### Claim 4 (depends on 1)

Process according to claim 1, characterised in that the doping paste is printed on by a printing process selected from the group screen printing, flexographic printing, gravure printing, offset printing, microcontact printing, electrohydrodynamic dispensing, roller coating, spray coating, ultrasonic spray coating, pipe jetting, laser transfer printing, pad printing, flat-bed screen printing and rotation screen printing.

### Claim 5 (depends on 1)

Process according to claim 1, characterised in that the doping paste is printed on by screen printing.

### Claim 6 (depends on 1)

Process according to claim 1, characterised in that doping is carried out directly from the printed and dried-on glass after boron diffusion with exclusion of an oxidation process of the “boron skin”.

### Claim 7 (depends on 1)

Process according to claim 1, characterised in that structured, highly efficient solar cells which have regions of different doping are produced by at least one two-stage doping with only one thermal diffusion or high-temperature treatment of the substrate.

### Claim 8 (depends on 1)

Process according to claim 1, characterised in that a glass layer which comprises at least one doping element selected from the group boron, gallium, silicon, germanium, zinc, tin, phosphorus, titanium, zirconium, yttrium, nickel, cobalt, iron, cerium, niobium, arsenic and lead is generated on the substrate surface over the entire surface or selectively in step a) by gas-phase deposition by means of PECVD (plasma-enhanced chemical vapour deposition), APCVD (atmospheric pressure chemical vapour deposition), ALD (atomic layer deposition) or sputtering.

### Claim 9 (depends on 8)

Process according claim 8, characterised in that the glass layer is removed by means of hydrofluoric acid when the doping is complete.

### Claim 10 (depends on 1)

Solar cells, produced by a process according to claim 1.

### Claim 11 (depends on 1)

Photovoltaic elements, produced by a process according to claim 1.