# US 2017/0372900 A1 · Multi-Layer Mask and Method of Forming Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0372900 A1
- Document ID: US20170372900A1
- Status: Published application
- Kind: A1
- Application number: 15/700,884
- Filed: 2017-09-11
- Published: 2017-12-28
- Earliest claimed: 2016-06-15
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Teng-Chun Tsai; Yung-Cheng Lu; Ying-Tsung Chen; Tien-I Bao
- Web page: https://patentgrep.com/patent/US20170372900A1

## CPC

- H10P 76/4085: {characterised by the processes involved to create the masks}
- H10P 14/6342: {Liquid deposition, e.g. spin-coating, sol-gel techniques or spray coating}
- H10P 14/6902: {composed of carbon, e.g. alpha-C, diamond or hydrogen doped carbon}
- H10P 50/283: {by chemical means}
- H10P 76/204: {of organic photoresist masks}
- H10P 76/2041: {Photolithographic processes}
- H10P 76/405: {characterised by their composition, e.g. multilayer masks}
- H10P 95/06: {Planarisation of inorganic insulating materials}
- H10P 95/062: {involving a dielectric removal step}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method includes forming a first insulating layer over a substrate, the first insulating layer having a non-planar top surface, the first insulating layer having a first etch rate. A second insulating layer is formed over the first insulating layer, the second insulating layer having a non-planar top surface, the second insulating layer having a second etch rate, the second etch rate being greater than the first etch rate. The second insulating layer is polished, the polishing partially removing the second insulating layer. The first insulating layer and the second insulating layer are non-selectively recessed.

## Claims

### Claim 1

A method comprising:
forming a first insulating layer over a substrate, the first insulating layer having a non-planar top surface;
forming a second insulating layer over the first insulating layer, the second insulating layer having a non-planar top surface;
partially removing the second insulating layer, a remaining portion of the second insulating layer having a planar top surface; and
non-selectively etching the first insulating layer and the remaining portion of the second insulating layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first insulating layer has a first etch rate, wherein the second insulating layer has a second etch rate, and wherein the second etch rate is greater than the first etch rate.

### Claim 3 (depends on 2)

The method of claim 2, further comprising, after partially removing the second insulating layer, reducing a difference between the second etch rate and the first etch rate.

### Claim 4 (depends on 1)

The method of claim 1, wherein partially removing the second insulating layer comprises exposing at least a portion of the non-planar top surface of the first insulating layer.

### Claim 5 (depends on 1)

The method of claim 1, further comprising forming a third insulating layer between the first insulating layer and the second insulating layer, the third insulating layer having a non-planar top surface.

### Claim 6 (depends on 5)

The method of claim 5, wherein non-selectively etching the first insulating layer and the remaining portion of the second insulating layer further comprises non-selectively etching the third insulating layer.

### Claim 7 (depends on 1)

The method of claim 1, wherein, after non-selectively etching the first insulating layer and the remaining portion of the second insulating layer, a remaining portion of the first insulating layer has a planar top surface.

### Claim 8

A method comprising:
forming a structure over a base layer;
forming a first carbon-rich layer over the structure, the first carbon-rich layer having a non-planar top surface;
annealing the first carbon-rich layer;
forming an insulating layer over the first carbon-rich layer, the insulating layer having a non-planar top surface;
annealing the insulating layer;
polishing the insulating layer; and
non-selectively recessing the first carbon-rich layer and the insulating layer.

### Claim 9 (depends on 8)

The method of claim 8, wherein the first carbon-rich layer has a first etch rate, wherein the insulating layer has a second etch rate, and wherein the second etch rate is greater than the first etch rate.

### Claim 10 (depends on 9)

The method of claim 9, further comprising, after polishing the insulating layer, annealing the first carbon-rich layer and the insulating layer to reduce a difference between the second etch rate and the first etch rate.

### Claim 11 (depends on 8)

The method of claim 8, wherein forming the insulating layer comprises forming a second carbon-rich layer.

### Claim 12 (depends on 8)

The method of claim 8, wherein non-selectively recessing the first carbon-rich layer and the insulating layer comprises completely removing the insulating layer.

### Claim 13 (depends on 8)

The method of claim 8, further comprising forming an etch stop layer between the first carbon-rich layer and the insulating layer.

### Claim 14 (depends on 13)

The method of claim 13, wherein non-selectively recessing the first carbon-rich layer and the insulating layer comprises completely removing the etch stop layer.

### Claim 15

A method comprising:
coating a substrate with a first spin-on carbon (SOC) material, the first SOC material having a non-planar top surface;
forming an insulating layer over the first SOC material, the insulating layer having a non-planar top surface;
coating the insulating layer with a second SOC material, the second SOC material having a non-planar top surface;
performing a polishing process on the second SOC material, at least a portion of the second SOC material remaining over the insulating layer after performing the polishing process; and
non-selectively thinning the first SOC material, the second SOC material, and the insulating layer to form a thinned first SOC material, the thinned first SOC material having a planar top surface.

### Claim 16 (depends on 15)

The method of claim 15, wherein an etch rate of the second SOC material is greater than an etch rate of the first SOC material.

### Claim 17 (depends on 15)

The method of claim 15, wherein non-selectively thinning the first SOC material, the second SOC material, and the insulating layer comprises completely removing the second SOC material and the insulating layer.

### Claim 18 (depends on 15)

The method of claim 15, further comprising, after performing the polishing process, annealing the first SOC material, the second SOC material and the insulating layer.

### Claim 19 (depends on 15)

The method of claim 15, further comprising:
forming a silicon-containing layer over the thinned first SOC material; and
forming a photoresist layer over the silicon-containing layer.

### Claim 20 (depends on 15)

The method of claim 15, wherein an atomic fraction of carbon in the first SOC material is greater than about 0.5.