# US 2017/0372886 A1 · Deposition of SiN

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0372886 A1
- Document ID: US20170372886A1
- Status: Published application
- Kind: A1
- Application number: 15/426,593
- Filed: 2017-02-07
- Published: 2017-12-28
- Earliest claimed: 2014-09-17
- Assignees: ASM IP Holding B.V.
- Applicants: ASM IP Holding B.V.
- Inventors: Shang Chen; Viljami Pore; Ryoko Yamada; Antti Juhani Niskanen
- Web page: https://patentgrep.com/patent/US20170372886A1

## CPC

- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- C23C 16/045: {Coating cavities or hollow spaces, e.g. interior of tubes; Infiltration of porous substrates}
- C23C 16/345: {Silicon nitride}
- C23C 16/45536: {Use of plasma, radiation or electromagnetic fields}
- C23C 16/45553: {characterized by the use of precursors specially adapted for ALD}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

Methods and precursors for forming silicon nitride films are provided. In some embodiments, silicon nitride can be deposited by atomic layer deposition (ALD), such as plasma enhanced ALD. In some embodiments, deposited silicon nitride can be treated with a plasma treatment. The plasma treatment can be a nitrogen plasma treatment. In some embodiments the silicon precursors for depositing the silicon nitride comprise an iodine ligand. The silicon nitride films may have a relatively uniform etch rate for both vertical and the horizontal portions when deposited onto three-dimensional structures such as FinFETS or other types of multiple gate FETs. In some embodiments, various silicon nitride films of the present disclosure have an etch rate of less than half the thermal oxide removal rate with diluted HF (0.5%). In some embodiments, a method for depositing silicon nitride films comprises a multi-step plasma treatment.

## Claims

### Claim 1

A method of forming a SiN thin film on a substrate in a reaction space comprising:
contacting the substrate with a silicon precursor comprising iodine to provide a first silicon species adsorbed on a surface of the substrate;
contacting the substrate comprising the first silicon species adsorbed on the surface with a first plasma comprising activated hydrogen species thereby forming SiN on the substrate; and
conducting a nitrogen plasma treatment, wherein the nitrogen plasma treatment comprises contacting the substrate comprising SiN with a second plasma formed from a nitrogen containing gas substantially free of hydrogen-containing species to form the SiN thin film.