# US 2017/0372874 A9 · Bulk sintered solid solution ceramic which exhibits fracture toughness and halogen plasma resistance

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0372874 A9
- Document ID: US20170372874A9
- Status: Published application
- Kind: A9
- Application number: 14/756,839
- Filed: 2015-10-20
- Published: 2017-12-28
- Earliest claimed: 2007-04-27
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Jennifer Y. Sun; Ren-Guan Duan; Jie Yuan; Li Xu; Kenneth S. Collins
- Web page: https://patentgrep.com/patent/US20170372874A9

## CPC

- H01J 37/32495: {Means for protecting the vessel against plasma}
- C04B 35/486: Fine ceramics
- C04B 35/505: based on yttrium oxide
- H01J 37/3244: {Gas supply means}
- H01J 37/32697: {Electrostatic control}
- H01J 37/32715: {Workpiece holder}
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

A bulk, sintered solid solution-comprising ceramic article useful in semiconductor processing, which is resistant to erosion by halogen-containing plasmas and provides advantageous mechanical properties. The solid solution-comprising ceramic article is formed from a combination of yttrium oxide and zirconium oxide. The bulk, sintered solid solution-comprising article is formed from zirconium oxide at a molar concentration ranging from about 96 mole % to about 94 mole %, and yttrium oxide at a molar concentration ranging from about 4 mole % to about 6 mole %.

## Claims

### Claim at position 1

-13. (canceled)

### Claim 14

A semiconductor processing apparatus, said apparatus having at least one surface exposed to a halogen-comprising plasma during a process, wherein said apparatus comprises a bulk, sintered solid solution ceramic which is resistant to erosion by halogen-containing plasmas, wherein said ceramic is formed from zirconium oxide at a molar concentration ranging from about 96 mole % to about 94 mole %, and yttrium oxide at a molar concentration ranging from about 4 mole % to about 6 mole %.

### Claim 15

(canceled)

### Claim 16

(canceled)

### Claim 17 (depends on 14)

A semiconductor processing apparatus in accordance with claim 14, wherein said apparatus is selected from the group consisting of a lid, a lid liner, a nozzle, a gas distribution plate, a shower head, an electrostatic chuck component, a shadow frame, a substrate holding frame, a processing kit, and a chamber liner.

### Claim 18 (depends on 14)

A semiconductor processing apparatus in accordance with claim 14, wherein a mean grain size of said ceramic ranges from about 0.5 μm to about 1.0 μm.

### Claim 19 (depends on 14)

A semiconductor processing apparatus in accordance with claim 14, wherein a flexural strength of said ceramic ranges from about 1100 MPa to about 1300 MPa.

### Claim 20 (depends on 14)

A semiconductor processing apparatus in accordance with claim 14, wherein a fracture toughness of said ceramic ranges from about 10 MPa·m1/2 to about 12 MPa·m1/2.

### Claim 21

A method of reducing the plasma erosion of a semiconductor processing apparatus contacted by a halogen-containing plasma, comprising: selecting said semiconductor processing apparatus to be a bulk, sintered solid solution ceramic-comprising article, wherein said ceramic is formed from zirconium oxide at a molar concentration ranging from about 96 mole % to about 94 mole %, and yttrium oxide at a molar concentration ranging from about 4 mole % to about 6 mole %.

### Claim 22 (depends on 21)

A method in accordance with claim 21, wherein said plasma erosion rate for a surface of said semiconductor processing apparatus, upon exposure to a halogen-comprising plasma, is less than about 0.4 μm/hr.

### Claim 23 (depends on 22)

A method in accordance with claim 22, wherein said plasma erosion rate for a surface of said semiconductor processing apparatus, upon exposure to a halogen-comprising plasma, ranges from about 0.1 μm/hr to about 0.4 μm/hr.

### Claim 24 (depends on 21)

A method in accordance with claim 21, wherein at least one surface of said semiconductor processing apparatus, which surface is said bulk, sintered solic solution ceramic, is exposed to said halogen-comprising plasma during said semiconductor processing.

### Claim 25

(canceled)

### Claim 26

(canceled)