# US 2017/0370791 A1 · Method of fabricating acoustic wave device and acoustic wave device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0370791 A1
- Document ID: US20170370791A1
- Status: Published application
- Kind: A1
- Application number: 15/615,012
- Filed: 2017-06-06
- Published: 2017-12-28
- Earliest claimed: 2016-06-28
- Assignees: Taiyo Yuden Co., Ltd.
- Applicants: Taiyo Yuden Co., Ltd.
- Inventors: Kentaro NAKAMURA; Fumiya MATSUKURA; Naoki TAKAHASHI; Takashi MATSUDA; Tsutomu MIYASHITA
- Web page: https://patentgrep.com/patent/US20170370791A1

## CPC

- H03H 3/08: for the manufacture of resonators or networks using surface acoustic waves
- G01L 1/165: {with acoustic surface waves}
- G01L 9/0025: {with acoustic surface waves}
- H03H 3/0072: {of microelectro-mechanical resonators or networks (micromembranes or microbeams B81B2203/01; manufacture of microstructural devices in general B81C)}
- H03H 3/02: for the manufacture of piezoelectric or electrostrictive resonators or networks (H03H3/08 takes precedence)
- H03H 9/02543: {Characteristics of substrate, e.g. cutting angles}
- H03H 9/02834: {of temperature influence (cut angles H03H9/02543)}
- H03H 9/02842: {of reflections (H03H9/6406 takes precedence)}
- H03H 9/145: for networks using surface acoustic waves
- H10N 30/06: Forming electrodes or interconnections, e.g. leads or terminals
- H03H 2003/023: {the resonators or networks being of the membrane type}
- H03H 2003/025: {the resonators or networks comprising an acoustic mirror}
- H03H 2003/027: {the resonators or networks being of the microelectro-mechanical [MEMS] type}
- H10B 12/033: {the capacitor extending over the transistor}
- Y10T 29/42: Piezoelectric device making
- Y10T 29/49005: Acoustic transducer
- H03H: IMPEDANCE NETWORKS, e.g. RESONANT CIRCUITS; RESONATORS (waveguides, resonators, lines or other devices of the waveguide type H01P)
- G01L: MEASURING FORCE, STRESS, TORQUE, WORK, MECHANICAL POWER, MECHANICAL EFFICIENCY, OR FLUID PRESSURE (weighing G01G)
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H10B: ELECTRONIC MEMORY DEVICES
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

An acoustic wave device fabrication method includes: forming on a piezoelectric substrate a comb-shaped electrode and a wiring layer coupled to the comb-shaped electrode; forming on the piezoelectric substrate a first dielectric film having a film thickness greater than those of the comb-shaped electrode and the wiring layer, covering the comb-shaped electrode and the wiring layer, and being made of silicon oxide doped with an element or undoped silicon oxide; forming on the first dielectric film a second dielectric film having an aperture above the wiring layer; removing the first dielectric film exposed by the aperture of the second dielectric film by wet etching using an etching liquid causing an etching rate of the second dielectric film to be less than that of the first dielectric film so that the first dielectric film is left so as to cover an end face of the wiring layer and the comb-shaped electrode.

## Claims

### Claim 1

A method of fabricating an acoustic wave device, the method comprising:
forming on a piezoelectric substrate a comb-shaped electrode and a wiring layer coupled to the comb-shaped electrode;
forming on the piezoelectric substrate a first dielectric film having a film thickness greater than those of the comb-shaped electrode and the wiring layer and covering the comb-shaped electrode and the wiring layer, the first dielectric film being made of silicon oxide doped with an element or undoped silicon oxide;
forming on the first dielectric film a second dielectric film having a first aperture above the wiring layer;
removing the first dielectric film exposed by the first aperture of the second dielectric film by wet etching using an etching liquid that causes an etching rate of the second dielectric film to be less than an etching rate of the first dielectric film so that the first dielectric film is left so as to cover an end face of the wiring layer and the comb-shaped electrode.

### Claim 2

A method of fabricating an acoustic wave device, the method comprising:
forming on a piezoelectric substrate a comb-shaped electrode and a wiring layer coupled to the comb-shaped electrode;
forming on the piezoelectric substrate a first dielectric film having a film thickness greater than those of the comb-shaped electrode and the wiring layer and covering the comb-shaped electrode and the wiring layer, the first dielectric film being made of silicon oxide doped with an element or undoped silicon oxide;
forming on the first dielectric film a second dielectric film having a first aperture above the wiring layer, the second dielectric film containing at least one of tantalum oxide, niobium oxide, tungsten oxide, titanium oxide, tellurium oxide, aluminum oxide, silicon nitride, aluminum nitride, and silicon carbide; and
removing the first dielectric film exposed by the first aperture of the second dielectric film by wet etching using a hydrofluoric acid-based etching liquid so that the first dielectric film is left so as to cover an end face of the wiring layer and the comb-shaped electrode.

### Claim 3 (depends on 1)

The method according to claim 1, wherein
the forming of the second dielectric film includes forming the second dielectric film having the first aperture and a second aperture above a region in which neither the comb-shaped electrode or the wiring layer is formed, and
the removing of the first dielectric film includes removing the first dielectric film exposed by the first aperture and the second aperture of the second dielectric film so that the first dielectric film is left so as to cover an end face of the wiring layer and extend along the end face of the wiring layer.

### Claim 4 (depends on 3)

The method according to claim 3, wherein
the removing of the first dielectric film includes removing the first dielectric film so that the first dielectric film is left as a protrusion portion in the region in which neither the comb-shaped electrode or the wiring layer is formed.

### Claim 5 (depends on 1)

The method according to claim 1, wherein
the forming of the second dielectric film includes forming the second dielectric film having a thick film portion of which a thickness around a third aperture to be formed by removing the first dielectric film is greater than a thickness in a remaining portion.

### Claim 6 (depends on 5)

The method according to claim 5, wherein
the forming of the second dielectric film includes forming the second dielectric film having the thick film portion with a side wall to which a residue adheres by dry etching the second dielectric film.

### Claim 7

An acoustic wave device comprising:
a piezoelectric substrate;
a comb-shaped electrode located on the piezoelectric substrate;
a wiring layer located on the piezoelectric substrate and coupled to the comb-shaped electrode;
a first dielectric film located on the piezoelectric substrate and made of silicon oxide doped with an element or undoped silicon oxide, the first dielectric film covering the comb-shaped electrode and an end face of the wiring layer, having an aperture that exposes the wiring layer, and having a film thickness greater than those of the comb-shaped electrode and the wiring layer; and
a second dielectric film located on the first dielectric film, the second dielectric film having an etching rate in wet etching using a hydrofluoric acid-based etching liquid less than that of the first dielectric film.

### Claim 8

An acoustic wave device comprising:
a piezoelectric substrate;
a comb-shaped electrode located on the piezoelectric substrate;
a wiring layer located on the piezoelectric substrate and coupled to the comb-shaped electrode;
a first dielectric film located on the piezoelectric substrate and made of silicon oxide doped with an element or undoped silicon oxide, the first dielectric film covering the comb-shaped electrode and an end face of the wiring layer, having an aperture that exposes the wiring layer, and having a film thickness greater than those of the comb-shaped electrode and the wiring layer; and
a second dielectric film located on the first dielectric film, the second dielectric film containing at least one of tantalum oxide, niobium oxide, tungsten oxide, titanium oxide, tellurium oxide, aluminum oxide, silicon nitride, aluminum nitride, and silicon carbide.

### Claim 9 (depends on 2)

The method according to claim 2, wherein
the forming of the second dielectric film includes forming the second dielectric film having the first aperture and a second aperture above a region in which neither the comb-shaped electrode or the wiring layer is formed, and
the removing of the first dielectric film includes removing the first dielectric film exposed by the first aperture and the second aperture of the second dielectric film so that the first dielectric film is left so as to cover an end face of the wiring layer and extend along the end face of the wiring layer.

### Claim 10 (depends on 9)

The method according to claim 9, wherein
the removing of the first dielectric film includes removing the first dielectric film so that the first dielectric film is left as a protrusion portion in the region in which neither the comb-shaped electrode or the wiring layer is formed.

### Claim 11 (depends on 2)

The method according to claim 2, wherein
the forming of the second dielectric film includes forming the second dielectric film having a thick film portion of which a thickness around a third aperture to be formed by removing the first dielectric film is greater than a thickness in a remaining portion.

### Claim 12 (depends on 11)

The method according to claim 11, wherein
the forming of the second dielectric film includes forming the second dielectric film having the thick film portion with a side wall to which a residue adheres by dry etching the second dielectric film.