# US 2017/0365724 A1 · Transparent Conductive Oxide In Silicon Heterojunction Solar Cells

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0365724 A1
- Document ID: US20170365724A1
- Status: Published application
- Kind: A1
- Application number: 15/625,426
- Filed: 2017-06-16
- Published: 2017-12-21
- Earliest claimed: 2016-06-16
- Assignees: Arizona Board of Regents on behalf of Arizona State University
- Inventors: Stanislau Herasimenka
- Web page: https://patentgrep.com/patent/US20170365724A1

## CPC

- H10F 77/315: {the coatings being antireflective or having enhancing optical properties}
- H10F 10/166: the Group IV-IV heterojunctions being heterojunctions of crystalline and amorphous materials, e.g. silicon heterojunction [SHJ] photovoltaic cells
- H10F 71/10: the devices comprising amorphous semiconductor material
- H10F 71/103: {including only Group IV materials}
- H10F 71/128: {Annealing}
- H10F 77/215: {Geometries of grid contacts}
- Y02E 10/50: Photovoltaic [PV] energy
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Devices and methods for reducing optical losses in transparent conductive oxides (TCOs) used in silicon heterojunction (SHJ) solar cells while enhancing series resistance are disclosed herein. In particular, the methods include reducing the thickness of TCO layers by about 200% to 300% and depositing hydrogenated dielectric layers on top to form double layers of antireflection coating. It has been discovered that the conductivity of a thin TCO layer can be increased through a hydrogen treatment supplied from the capping dielectric during the post deposition annealing. The optimized cells with ITO/SiOx:H stacks achieved more than 41 mA/cm2 generation current on 120-micron-thick wafers while having approximately 100 Ohm/square sheet resistance. Further, solar cells and methods may include integration of ITO/SiOx:H stacks with Cu plating and use ITO/SiNx/SiOx triple layer antireflection coatings. The experimental data details the improved optics and resistance in cell stacks with varying materials and thicknesses.

## Claims

### Claim 1

A solar cell, comprising:
a silicon base layer;
an emitter layer disposed on a first side of the silicon base layer, wherein the emitter layer comprises amorphous silicon;
a first antireflective coating layer disposed on the emitter layer, wherein the first antireflective coating layer comprises a transparent conducting oxide; and
a second antireflective coating layer disposed on the first antireflective coating layer, wherein the second antireflective coating layer comprises a hydrogenated silicon oxide.

### Claim 2 (depends on 1)

The solar cell of claim 1, wherein the first antireflective coating layer is hydrogenated by the second antireflective coating layer after annealing such that conductivity of the first antireflective coating layer is increased.

### Claim 3 (depends on 2)

The solar cell of claim 2, wherein conductivity of the first antireflective coating layer is increased by about 20% to about 40%.

### Claim 4 (depends on 1)

The solar cell of claim 1, wherein the second antireflective coating layer has an atomic percentage of hydrogen between about 10% and about 40%.

### Claim 5 (depends on 4)

The solar cell of claim 4, wherein the atomic percentage of hydrogen is about 25%.

### Claim 6 (depends on 1)

The solar cell of claim 1, further comprising:
a conducting grid disposed on the second antireflective coating layer.

### Claim 7 (depends on 6)

The solar cell of claim 6, wherein the conducting grid comprises at least one of silver, copper, and nickel.

### Claim 8 (depends on 1)

The solar cell of claim 1, wherein the silicon base layer includes a crystalline-Si substrate.

### Claim 9 (depends on 1)

The solar cell of claim 1, wherein the silicon base layer includes an epitaxially formed crystalline-Si thin film.

### Claim 10

A method for fabricating a solar cell, comprising:
(a) preparing a silicon (Si) base layer;
(b) depositing an emitter layer on a first surface of the Si base layer, wherein the emitter layer comprises an amorphous silicon;
(c) depositing a first antireflective coating layer on the emitter layer, wherein the first antireflective coating layer comprises a transparent conducting oxide; and
(d) depositing a second antireflective coating layer on the first antireflective coating layer, wherein the second antireflective coating layer comprises a hydrogenated silicon oxide.

### Claim 11 (depends on 10)

The method of claim 10, further comprising:
(e) annealing the solar cell such that the first antireflective coating layer is hydrogenated by the second antireflective coating layer thereby increasing conductivity of the first antireflective coating layer.

### Claim 12 (depends on 11)

The method of claim 11, wherein conductivity of the first antireflective coating layer is increased by about 20% to about 40%.

### Claim 13 (depends on 10)

The method of claim 10, wherein the second antireflective coating layer has an atomic percentage of hydrogen between about 10% and about 40%.

### Claim 14 (depends on 13)

The method of claim 13, wherein the atomic percentage of hydrogen is about 25%.

### Claim 15 (depends on 10)

The method of claim 10, further comprising:
depositing a conducting grid on the second antireflective coating layer.

### Claim 16 (depends on 15)

The method of claim 15, wherein the conducting grid comprises at least one of silver, copper, and nickel.

### Claim 17 (depends on 10)

The method of claim 10, wherein the silicon base layer includes a crystalline-silicon substrate.

### Claim 18 (depends on 10)

The method of claim 10, wherein the silicon base layer includes an epitaxially formed crystalline-silicon thin film.