# US 2017/0365561 A1 · Method for preventing bottom layer wrinkling in a semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0365561 A1
- Document ID: US20170365561A1
- Status: Published application
- Kind: A1
- Application number: 15/187,027
- Filed: 2016-06-20
- Published: 2017-12-21
- Earliest claimed: 2016-06-20
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Co., Ltd.
- Inventors: Jung-Hau SHIU; Chung-Chi KO; Tze-Liang LEE; Yu-Yun PENG
- Web page: https://patentgrep.com/patent/US20170365561A1

## CPC

- H10P 50/73: {using masks for insulating materials}
- G03F 7/094: {Multilayer resist systems, e.g. planarising layers}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10W 20/085: {involving intermediate temporary filling with material}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method for manufacturing a semiconductor device includes forming a first insulating film over a semiconductor substrate and forming a second insulating film on the first insulating film. The first insulating film is a tensile film having a first tensile stress and the second insulating film is either a tensile film having a second tensile stress that is less than the first tensile stress or a compressive film. The first insulating film and second insulating film are formed of a same material. A metal hard mask layer is formed on the second insulating film.

## Claims

### Claim at position 1

1-7. (canceled)

### Claim 8

A method for manufacturing a semiconductor device, comprising:
forming a first insulating film over a semiconductor substrate;
forming a second insulating film on the first insulating film,
wherein the first insulating film is formed at a first plasma power condition, the second insulating film is formed at a second plasma power condition, the second plasma power condition being a higher power than the first plasma power condition, and the first insulating film and second insulating film are formed of a same material; and
forming a metal hard mask layer on the second insulating film,
wherein the first insulating film and second insulating film are formed at a temperature of about 100° C. to about 200° C.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the first insulating film and second insulating film are oxide films.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the first insulating film and second insulating film comprise silicon oxide.

### Claim 11 (depends on 8)

The method according to claim 8, further comprising forming a third insulating film on the metal hard mask layer.

### Claim 12 (depends on 8)

The method according to claim 8, further comprising patterning the first insulating film, second insulating film, and metal hard mask layer.

### Claim 13 (depends on 12)

The method according to claim 12, wherein the first insulating film, second insulating film, and metal hard mask layer are patterned by etching.

### Claim 14

(canceled)

### Claim 15 (depends on 8)

The method according to claim 8, wherein the first plasma power condition ranges from about 50 W to about 500 W, and the second plasma power condition ranges from about 550 W to about 800 W.

### Claim 16

A method for manufacturing a semiconductor device, comprising:
forming a first insulating film over a semiconductor substrate;
forming a second insulating film on the first insulating film,
wherein the first insulating film is a tensile film having a first tensile stress, the second insulating film is either a tensile film having a second tensile stress that is less than the first tensile stress or a compressive film, and the first insulating film and second insulating film are formed of a same material;
forming a metal hard mask layer on the second insulating film; and
forming a third insulating film on the metal hard mask layer,
wherein the first, second, and third insulating films are formed at a temperature of about 100° C. to about 200° C.,
the first insulating film is formed at a first plasma power condition, the second insulating film is formed at a second plasma power condition, the second plasma power condition being a higher power than the first plasma power condition, and the first insulating film and second insulating film are formed of a same material; and
removing the metal hard mask layer.

### Claim 17 (depends on 16)

The method according to claim 16, wherein the first plasma power condition ranges from about 50 W to about 500 W, and the second plasma power condition ranges from about 550 W to about 800 W.

### Claim 18 (depends on 16)

The semiconductor device according to claim 16, wherein the first, second, and third insulating films comprise an oxide.

### Claim 19 (depends on 16)

The semiconductor device according to claim 16, wherein the first insulating film has a tensile stress ranging from about 75 MPa to about 25 MPa, and the second insulating film has a tensile stress ranging from about 20 MPa to about −50 MPa.

### Claim 20 (depends on 16)

The semiconductor device according to claim 16, wherein the first and third insulating films have a thickness ranging from about 10 nm to about 50 nm, and the second insulating film has a thickness ranging from about 100 nm to about 500 nm.

### Claim 21

A method for manufacturing a semiconductor device, comprising:
forming a first insulating film over a semiconductor substrate at a first plasma power condition, wherein the first plasma power condition ranges from about 50 W to about 500 W;
forming a second insulating film directly on the first insulating film at a second plasma condition, wherein the second plasma power condition ranges from about 550 W to about 1000 W;
forming a metal hard mask layer on the second insulating film;
forming a third insulating film on the metal hard mask layer;
forming a layer of organic material on the third insulating layer;
forming a silicon containing layer directly on the layer of organic material; and
forming a photoresist directly on the silicon containing layer.

### Claim 22 (depends on 21)

The method according to claim 21, wherein the first insulating film and second insulating film are formed of a same material.

### Claim 23

(canceled)

### Claim 24 (depends on 21)

The method according to claim 21, wherein the first, second, and third insulating films are formed at a temperature of about 100° C. to about 200° C.

### Claim 25 (depends on 21)

The semiconductor device according to claim 21, wherein the first, second, and third insulating films comprise silicon oxide.

### Claim 26

(canceled)

### Claim 27 (depends on 21)

The semiconductor device according to claim 21, wherein the first and third insulating films have a thickness ranging from about 10 nm to about 50 nm, and the second insulating film has a thickness ranging from about 100 nm to about 500 nm.

### Claim 28 (depends on 8)

The method according to claim 8, wherein the metal hard mask comprises titanium nitride.

### Claim 29 (depends on 16)

The method according to claim 16, wherein the metal hard mask comprises titanium nitride.

### Claim 30 (depends on 21)

The semiconductor device according to claim 21, wherein the metal hard mask comprises titanium nitride.