# US 2017/0365466 A1 · Film forming method and aluminum nitride film forming method for semiconductor apparatus

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0365466 A1
- Document ID: US20170365466A1
- Status: Published application
- Kind: A1
- Application number: 15/691,211
- Filed: 2017-08-30
- Published: 2017-12-21
- Earliest claimed: 2016-06-12
- Assignees: Beijing Naura Microelectronics Equipment Co., Ltd.
- Applicants: Beijing Naura Microelectronics Equipment Co., Ltd
- Inventors: Jun WANG; Boyu DONG; Bingliang GUO; Yujie GENG; Huaichao MA
- Web page: https://patentgrep.com/patent/US20170365466A1

## CPC

- H10P 14/22: using physical deposition, e.g. vacuum deposition or sputtering
- C23C 14/0036: {Reactive sputtering}
- C23C 14/0617: {AIII BV compounds, where A is Al, Ga, In or Tl and B is N, P, As, Sb or Bi}
- C23C 14/0641: {Nitrides (C23C14/0617 takes precedence)}
- C23C 14/34: Sputtering
- C23C 14/3485: {using pulsed power to the target}
- C23C 14/564: {Means for minimising impurities in the coating chamber such as dust, moisture, residual gases}
- C30B 23/025: {characterised by the substrate}
- C30B 29/403: {AIII-nitrides}
- H10P 14/2921: {being crystalline insulating materials}
- H10P 14/3216: {Nitrides}
- H10P 14/3416: {Nitrides}
- H10P 95/00: Generic processes or apparatus for manufacture or treatments not covered by the other groups of this subclass
- H10H 20/01335: {the light-emitting regions comprising nitride materials}
- H10H 20/812: within the light-emitting regions, e.g. having quantum confinement structures
- H10H 20/815: having stress relaxation structures, e.g. buffer layers
- H10H 20/825: containing nitrogen, e.g. GaN
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS

## Abstract

The present disclosure provides a film forming method and an aluminum nitride film forming method for a semiconductor device. The film forming method for a semiconductor device includes performing multiple sputtering routes sequentially. Each sputtering routes includes: loading a substrate into a chamber; moving a shielding plate between a target and the substrate; introducing an inert gas into the chamber to perform a surface modification process on the target; performing a pre-sputtering to pre-treat a surface of the target; moving the shielding plate away from the substrate, and performing a main sputtering on the substrate to form a film on the substrate; and moving the substrate out of the chamber.

## Claims

### Claim 1

A film forming method for a semiconductor device, comprising:
performing multiple sputtering routes to form films on multi-batch substrates, wherein each sputtering routes comprises:
loading a substrate into a chamber;
moving a shielding plate between a target and the substrate;
introducing an inert gas into the chamber to perform a surface modification process on the target;
performing a pre-sputtering to pre-treat a surface of the target;
moving the shielding plate away from the substrate, and performing a main sputtering to form a film on the substrate; and
moving the substrate out of the chamber;
wherein: the surface modification process of the sputtering routes performed on an N-th batch of substrate and the surface modification process of the sputtering routes performed on a (N+1)-th batch of substrate have at least one different process parameter, where N is a positive integer.

### Claim 2 (depends on 1)

The method according to claim 1, wherein: the inert gas introduced during the surface modification process comprises argon.

### Claim 3 (depends on 1)

The method according to claim 1, wherein: the surface modification process of the sputtering routes performed on the N-th batch of substrate has a first process time, and the surface modification process of the sputtering routes performed on the (N+1)-th batch of substrate has a second process time different from the first process time.

### Claim 4 (depends on 3)

The method according to claim 3, wherein: the second process time is 2 to 8 times of the first process time.

### Claim 5 (depends on 3)

The method according to claim 3, wherein: the first process time is 1˜3 seconds, and the second process time is 6˜8 seconds.

### Claim 6 (depends on 3)

The method according to claim 3, wherein: the surface modification process of the sputtering routes performed on the N-th batch of substrate and the surface modification process of the sputtering routes performed on the (N+1)-th batch of substrate have a same sputtering power.

### Claim 7 (depends on 1)

The method according to claim 1, wherein: the surface modification process of the sputtering routes performed on the N-th batch of substrate and the surface modification process of the sputtering routes performed on the (N+1)-th batch of substrate have different sputtering power.

### Claim 8 (depends on 7)

The method according to claim 7, wherein: the surface modification process of the sputtering routes performed on the N-th batch of substrate and the surface modification process of the sputtering routes performed on the (N+1)-th batch of substrate have a same process time.

### Claim 9 (depends on 1)

The method according to claim 1, wherein: the surface modification process of the sputtering routes performed on the N-th batch of substrate and the surface modification process of the sputtering routes performed on the (N+1)-th batch of substrate have different process times and sputtering power.

### Claim 10 (depends on 1)

The method according to claim 1, wherein: the gas introduced during the pre-sputtering and the gas introduced during the main sputtering are the same.

### Claim 11 (depends on 1)

The method according to claim 1, further comprising continuously applying a sputtering power to the target during the pre-sputtering and the main sputtering.

### Claim 12 (depends on 1)

The method according to claim 1, further comprising:
repeating the sputtering routes continuously for multiple times, wherein the multiple sputtering routes performed continuously constitute one batch of sputtering routes; and
performing a pasting process at least one of after said one batch of sputtering routes and before said one batch of sputtering routes, wherein a power applied to the target is between 2500 watts and 4000 watts during the pasting process.

### Claim 13

An aluminum nitride film forming method for a semiconductor device, comprising:
performing multiple sputtering routes to form aluminum nitride films on multi-batch substrates, wherein each sputtering routes comprises:
loading a substrate into a chamber;
moving a shielding plate between a target containing aluminum and the substrate;
introducing an inert gas into the chamber to perform a surface modification process on the target containing aluminum;
performing a pre-sputtering to pre-treat a surface of the target containing aluminum such that the surface of the target containing aluminum is changed into a transition state from an Al-rich state;
moving the shielding plate away from the substrate, introducing an inert gas and a gas containing nitrogen into the chamber, and performing a main sputtering to form an aluminum nitride film on the substrate using the target containing aluminum; and
moving the substrate out of the chamber;
wherein the surface modification process of the sputtering routes performed on an N-th batch of substrate and the surface modification process of the sputtering routes performed on a (N+1)-th batch of substrate have at least one different process parameter, where N is a positive integer.

### Claim 14

(canceled)

### Claim 15 (depends on 13)

The method according to claim 13, wherein: the surface modification process of the sputtering routes performed on the N-th batch of substrate has a first process time, and the surface modification process of the sputtering routes performed on the (N+1)-th batch of substrate has a second process time different from the first process time.

### Claim 16

(canceled)

### Claim 17

(canceled)

### Claim 18

(canceled)

### Claim 19 (depends on 13)

The method according to claim 13, wherein: the surface modification process of the sputtering routes performed on the N-th batch of substrate and the surface modification process of the sputtering routes performed on the (N+1)-th batch of substrate have different sputtering power.

### Claim 20

(canceled)

### Claim 21 (depends on 13)

The method according to claim 13, wherein: the surface modification process of the sputtering routes performed on the N-th batch of substrate and the surface modification process of the sputtering routes performed on the (N+1)-th batch of substrate have different process times and sputtering power.

### Claim 22 (depends on 13)

The method according to claim 13, wherein: the main sputtering further comprises introducing a gas containing oxygen into the chamber so that the aluminum nitride film includes oxygen dopant.

### Claim 23

(canceled)

### Claim 24 (depends on 13)

The method according to claim 13, further comprising continuously applying a sputtering power to the target containing aluminum during the pre-sputtering and the main sputtering.

### Claim 25 (depends on 13)

The method according to claim 13, wherein: a sputtering power applied to the target containing aluminum during the pre-sputtering is equal to a sputtering power applied to the target containing aluminum during the main sputtering.

### Claim 26 (depends on 13)

The method according to claim 13, further comprising:
repeating the sputtering routes continuously for multiple times, wherein the multiple sputtering routes performed continuously constitute one batch of sputtering routes; and
performing a pasting process at least one of after said one batch of sputtering routes and before said one batch of sputtering routes, wherein a power applied to the target containing aluminum is between 2500 watts and 4000 watts during the pasting process.