# US 2017/0363981 A1 · Electrophotography toner

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0363981 A1
- Document ID: US20170363981A1
- Status: Published application
- Kind: A1
- Application number: 15/532,372
- Filed: 2015-11-25
- Published: 2017-12-21
- Earliest claimed: 2014-12-16
- Assignees: Kao Corporation
- Applicants: Kao Corporation
- Inventors: Shogo WATANABE; Kohei KATAYAMA; Yasuhiro HIDAKA; Hiroki KAKIUCHI
- Web page: https://patentgrep.com/patent/US20170363981A1

## CPC

- G03G 9/08755: {Polyesters}
- G03G 9/08706: {Polymers of alkenyl-aromatic compounds}
- G03G 9/08708: {Copolymers of styrene}
- G03G 9/08711: {with esters of acrylic or methacrylic acid}
- G03G 9/08795: {characterised by their chemical properties, e.g. acidity, molecular weight, sensitivity to reactants}
- G03G 9/08797: {characterised by their physical properties, e.g. viscosity, solubility, melting temperature, softening temperature, glass transition temperature}
- G03G: ELECTROGRAPHY; ELECTROPHOTOGRAPHY; MAGNETOGRAPHY

## Abstract

A toner for electrophotography containing a resin binder containing a crystalline resin and an amorphous resin, and a releasing agent, wherein the crystalline resin contains a crystalline composite resin C containing a polycondensation resin component and a styrenic resin component, wherein the polycondensation resin component is obtained by polycondensing a specified alcohol component and a specified carboxylic acid component, and wherein the amorphous resin contains an amorphous composite resin AC containing a polycondensation resin component and a styrenic resin component, wherein the polycondensation resin component is obtained by polycondensing an alcohol component and a specified carboxylic acid component, and an amorphous polyester AP obtained by polycondensing an alcohol component and a specified carboxylic acid component, wherein a softening point of the amorphous polyester AP is higher than a softening point of the amorphous composite resin AC, wherein a difference in softening points between the amorphous polyester AP and the amorphous composite resin AC is 10° C. or more and 50° C. or less. The toner for electrophotography of the present invention is suitably used in development of latent images or the like which is formed in, for example, electrostatic development method, electrostatic recording method, electrostatic printing method or the like.

## Claims

### Claim 1

A toner for electrophotography comprising a resin binder comprising a crystalline resin and an amorphous resin, and a releasing agent,
wherein the crystalline resin comprises a crystalline composite resin C comprising a polycondensation resin component and a styrenic resin component, wherein the polycondensation resin component is obtained by polycondensing an alcohol component comprising an aliphatic diol having 9 or more carbon atoms and 14 or less carbon atoms, and a carboxylic acid component comprising an aliphatic dicarboxylic acid compound having 9 or more carbon atoms and 14 or less carbon atoms, and
wherein the amorphous resin comprises
an amorphous composite resin AC comprising a polycondensation resin component and a styrenic resin component, wherein the polycondensation resin component is obtained by polycondensing an alcohol component and a carboxylic acid component comprising an aromatic dicarboxylic acid compound, and
an amorphous polyester AP obtained by polycondensing an alcohol component and a carboxylic acid component comprising an aromatic dicarboxylic acid compound,
wherein a softening point of the amorphous polyester AP is higher than a softening point of the amorphous composite resin AC, wherein a difference in softening points between the amorphous polyester AP and the amorphous composite resin AC is 10° C. or more and 50° C. or less.

### Claim 2 (depends on 1)

The toner for electrophotography according to claim 1, wherein a difference in softening points between the amorphous polyester AP and the amorphous composite resin AC is 15° C. or more.

### Claim 3 (depends on 1)

The toner for electrophotography according to claim 1, wherein a mass ratio of the amorphous polyester AP to the amorphous composite resin AC (amorphous polyester AP/amorphous composite resin AC) is 0.1 or more and 10 or less.

### Claim 4 (depends on 1)

The toner for electrophotography according to claim 1, wherein a softening point of the amorphous composite resin AC is higher than a softening point of the crystalline composite resin C, wherein a difference in softening points between the amorphous composite resin AC and the crystalline composite resin C is 50° C. or less.

### Claim 5 (depends on 1)

The toner for electrophotography according to claim 1, wherein a mass ratio of the crystalline composite resin C to a total amount of the amorphous composite resin AC and the amorphous polyester AP (crystalline composite resin C/a total amount of amorphous composite resin AC and amorphous polyester AP) is 2/98 or more and 30/70 or less.

### Claim 6 (depends on 1)

The toner for electrophotography according to claim 1, wherein a loss modulus of the crystalline composite resin C at 140° C. is 5 or more and 400 or less.

### Claim 7 (depends on 1)

The toner for electrophotography according to claim 1, wherein the crystalline composite resin C is a resin obtained by polymerizing
(i) raw material monomers for the polycondensation resin component comprising an alcohol component comprising an aliphatic diol having 9 or more carbon atoms and 14 or less carbon atoms, and a carboxylic acid component comprising an aliphatic dicarboxylic acid compound having 9 or more carbon atoms and 14 or less carbon atoms;
(ii) raw material monomers for the styrenic resin component; and
(iii) a dually reactive monomer capable of reacting with the raw material monomers for the polycondensation resin component and the raw material monomers for the styrenic resin component.

### Claim 8 (depends on 1)

The toner for electrophotography according to claim 1, wherein the amorphous composite resin AC is a resin obtained by polymerizing
(i′) raw material monomers for the polycondensation resin component comprising an alcohol component comprising an alkylene oxide adduct of bisphenol A represented by the formula (I):
wherein R1O and OR1 are an oxyalkylene group, wherein R1 is an ethylene group and/or a propylene group; and each of x1 and y1 is a positive number which is an average number of moles of an alkylene oxide added, wherein a value of the sum of x1 and y1 is 1 or more and 16 or less; and
a carboxylic acid component comprising an aromatic dicarboxylic acid compound;
(ii′) raw material monomers for the styrenic resin component; and
(iii′) a dually reactive monomer capable of reacting with the raw material monomers for the polycondensation resin component and the raw material monomers for the styrenic resin component.

### Claim 9 (depends on 1)

The toner for electrophotography according to claim 1, wherein a softening point of the amorphous polyester AP is 120° C. or higher and 170° C. or lower.

### Claim 10 (depends on 1)

The toner for electrophotography according to claim 1, wherein the alcohol component for the amorphous polyester AP comprises an alkylene oxide adduct of bisphenol A represented by the formula (II):
wherein R2O and OR2 are an oxyalkylene group, wherein R2 is an ethylene group and/or a propylene group; and each of x2 and y2 is a positive number which is an average number of moles of an alkylene oxide added, wherein a value of the sum of x2 and y2 is 1 or more and 16 or less.

### Claim 11 (depends on 1)

The toner for electrophotography according to claim 1, wherein a melting point of the releasing agent is 60° C. or higher and 120° C. or lower.

### Claim 12 (depends on 1)

The toner for electrophotography according to claim 1, wherein the content of the releasing agent is 0.5 parts by mass or more and 10 parts by mass or less, based on 100 parts by mass of the resin binder.

### Claim 13 (depends on 1)

The toner for electrophotography according to claim 1, wherein the releasing agent is one or more members selected from the group consisting of polypropylene wax, polyethylene wax, polypropylene-polyethylene copolymer wax, microcrystalline wax, paraffin waxes, Fischer-Tropsch wax, sazole wax, ester waxes, fatty acid amides, fatty acids, higher alcohols, and metal salts of fatty acids.

### Claim 14 (depends on 1)

The toner for electrophotography according to claim 1, wherein the softening point of the crystalline composite resin C is 70° C. or higher and 105° C. or lower.

### Claim 15 (depends on 1)

The toner for electrophotography according to claim 1, wherein the content of the aromatic dicarboxylic acid compound contained in the carboxylic acid component for the amorphous composite resin AC is 50% by mol or more of the carboxylic acid component of the amorphous composite resin AC.

### Claim 16 (depends on 1)

The toner for electrophotography according to claim 1, wherein the styrenic resin component of amorphous composite resin AC is a polymerization product of raw material monomers comprising an alkyl (meth)acrylate.

### Claim 17 (depends on 1)

The toner for electrophotography according to claim 1, wherein the softening point of the amorphous composite resin AC is higher than the softening point of the crystalline composite resin C, and wherein the difference in softening points between the amorphous composite resin AC and the crystalline composite resin C is 10° C. or more and 40° C. or less.

### Claim 18 (depends on 1)

The toner for electrophotography according to claim 1, wherein the content of the aromatic dicarboxylic acid compound in the carboxylic acid component for the amorphous polyester AP is 10% by mol or more and 90% by mol or less of the carboxylic acid component for the amorphous polyester AP.

### Claim 19 (depends on 1)

The toner for electrophotography according to claim 1, wherein the softening point of the amorphous polyester AP is higher than the softening point of the amorphous composite resin AC, and wherein the difference in softening points between the amorphous polyester AP and the amorphous composite resin AC is 20° C. or more and 40° C. or less.

### Claim 20 (depends on 1)

The toner for electrophotography according to claim 1, wherein the releasing agent comprises an ester wax and an aliphatic hydrocarbon wax.