# US 2017/0363958 A1 · Low dk/df solder resistant composition use for printed circuit board

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0363958 A1
- Document ID: US20170363958A1
- Status: Published application
- Kind: A1
- Application number: 15/185,841
- Filed: 2016-06-17
- Published: 2017-12-21
- Earliest claimed: 2016-06-17
- Assignees: Nan Ya Plastics Corporation
- Applicants: Nan Ya Plastics Corporation
- Inventors: Cheng-Chung LEE; Yeong-Tong HWANG; Shih-Hung HSU; Shao-En HWANG
- Web page: https://patentgrep.com/patent/US20170363958A1

## CPC

- G03F 7/031: Organic compounds not covered by group G03F7/029
- G03F 7/027: Non-macromolecular photopolymerisable compounds having carbon-to-carbon double bonds, e.g. ethylenic compounds (G03F7/075 takes precedence)
- G03F 7/038: Macromolecular compounds which are rendered insoluble or differentially wettable (G03F7/075 takes precedence; macromolecular azides G03F7/012; macromolecular diazonium compounds G03F7/021)
- G03F 7/0385: {using epoxidised novolak resin}
- G03F 7/0388: {with ethylenic or acetylenic bands in the side chains of the photopolymer}
- H05K 3/3452: Solder masks
- G03F 7/0047: {characterised by additives for obtaining a metallic or ceramic pattern, e.g. by firing}
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS

## Abstract

A low dielectric constant (Dk) and dissipation factor (Df) of solder resistant mask composition having excellent photo and thermocurability, and high developability resolution with an alkaline aqueous solution, wherein the dielectric constant is below 3.20 (1 GHz), and the dissipation factor is less than 0.015 (1 GHz); and wherein the composition comprises (A) a photopolymerizable prepolymer; (B) a photopolymerizable vinyl monomer; (C) an epoxy compound; (D) a photopolymerization initiator; (E) an inorganic filler; (F) a catalyst; and (G) an organic solvent.

## Claims

### Claim 1

A low Dielectric constant (Dk)/Dielectric dissipation factor (Df) solder resistant composition comprising following components:
A. a photopolymerizable prepolymer (represented by formula 1) the total amount of resin is 50 to 70 weight % (total amount of resin is defined as the sum of component (A) to component (D)), and prepared by reacting (a1) dicyclo pentadiene-phenol novolac multifunctional epoxy, or (a2) polyphenyl ether modified multifunctional epoxy resin or any combination of two (a1), (a2) with (b) mono carboxlic acid containing a vinyl group, then reacting with (c) a saturated or unsaturated poly anhydride acid;
B. a photopolymerizable vinyl monomer the total amount of resin is 5 to 20 weight % as thinner;
C. an epoxy compound the total amount of resin is 10 to 30 weight % comprising (C1) dicyclo pentadiene-phenol novolac multifunctional epoxy resin or polyphenyl ether modified epoxy resin or any combination of the forgoing two kinds of resins; (C2) tetra methyl biphenol epoxy resin;
D. a photopolymerization initiator the total amount of resin is 5 to 20 weight %;
E. an inorganic filler 10˜30 weight %;
F. a catalyst 0˜2.0 weight %;
G. an organic solvent 10˜30 weight %;

### Claim 2 (depends on 1)

The low Dk/Df solder resistant composition as claimed in claim 1, wherein the component A photopolymerizable prepolymer the total amount of resin is 50 to 70 weight % (total amount of resin is defined as the sum of component (A)+component (B)+component (C) and component (D)), and synthesized and prepared by reacting (a) low-Dk multifunctional epoxy resin with (b) mono carboxlic acid comprising at least one vinyl group, and reacting with (c) saturated or unsaturated poly anhydride acid, wherein the best effect can be acquired when the reaction condition is within following range: the low-Dk/Df multifunctional epoxy resin prevails in terms of quantity for reaction between the (a) low-Dk multifunctional epoxy resin and (b) mono carboxlic acid comprising at least one vinyl group, and epoxy group of each equivalent weight shall be 0.5-1.2 mole preferably, and 0.9-1.1 mole most preferably; during the reaction, the organic solvent shall be applied to dilution, such as petroleum-based aromatic solvent, propylene carbonate, butoxyethanol, butoxyethyl acetate, methylbenzene, dimethylbenzene, butyl carbitol acetate, cyclohexanone, propylene glycol monomethyl ether, dipropylene glycol diethyl ether, methyl carbitol acetate, etc.; and the catalyst is added, such as triphenylphosphine, triethylamine, methyltriethylammonium chloride, etc., wherein the triphenylphosphine shall be the best choice; the catalyst shall be 0.1-10 weight % of the total amount of the mixture for reaction preferably; the thermal polymerization inhibitor shall be added, such as p-dihydroxybenzene and hydroquinone dimethyl ether in order to prevent polymerization during reaction; the polymerization inhibitor shall be 0.01-1 weight % of the mixture for reaction after feeding preferably, and the reaction temperature shall be at 80-120° C. preferably, and the reaction shall be lasted for 6-24 h; and the step of reacting with (c) saturated or unsaturated anhydride shall be lasted, and the hydroxyl generated during reaction between the carboxyl and the epoxy group prevails in terms of quantity of poly anhydride used, the 0.1-1.0 mole of poly anhydride shall be applied to the hydroxyl of equivalent weight, and 0.3-0.7 mole most preferably; the reaction shall be implemented at 80-120° C. preferably, and the reaction shall be lasted for 4-16 h.

### Claim 3 (depends on 1)

The composition as claimed in claim 1, wherein the dosage of the component (B) photopolymerizable vinyl monomer the total amount of resin is 5 to 20 weight % and the component (B) is selected from acrylate comprising tripolycyanamide, hydroxyalkyl acrylate, such as mono acrylic acid or diacrylic acid compound of 2-hydroxyethyl acrylate, 2-hydroxybutyl acrylate, dihydric alcohol (such as glycol, polyglycol, propanediol), alkyl amine acrylic acid compound, such as acrylic acid-nitrogen, nitrogen-dimethylaminoethyl, polyhydrol (such as glycol, trimethylpropane, pentaerythritol, dipentaerythritol) and ethylene oxide, multifunctional acrylate of propylene oxide (which can be adducted itself), and acrylate of allyl glycidyl ether (glycidyl diepoxy ether, trimethylolpropane diepoxypropyl ether, and melaminecyanurate triepoxy isoamyl propionate), and most preferably acrylate or pentaerythritol of tripolycyanamide, multifunctional acrylate of dipentaerythritol.

### Claim 4 (depends on 1)

The composition as claimed in claim 1, wherein the dosage of the component (C) epoxy resin compound the total amount of resin is 10 to 30 weight % and the epoxy resin compound is selected from (C1) dicyclo pentadiene-phenol novolac multifunctional epoxy resin (produced by Nan Ya Plastics Corporation, with trademark NPPN-272H, equivalent of epoxy EEW of 272 g/eq and softening point at 78˜85° C.) or polyphenyl ether modified epoxy resin (produced by Nan Ya Plastics Corporation, with trademark NPPN-433PT60, equivalent of epoxy EEW of 340 g/eq and average molecular weight of Mn1300) or arbitrary combinations of the above-mentioned two epoxy resins; (C2) tetra methyl biphenol epoxy resin, wherein the acid equivalent of the above-mentioned polymerizable oligomer shall prevail in terms of dosage of the epoxy resin compound used, and 1.0-5.0 mole of epoxy group shall be applied to the carboxylic group equivalently, preferably 1.0-2.5 mole.

### Claim 5 (depends on 1)

The composition as claimed in claim 1, wherein the dosage of the component (D) photopolymerization initiator of the solder resistant composition with low dielectric constant and dissipation factor in the invention, the total amount of resin is 5 to 20 weight % and the photopolymerization initiator is selected from any of known photoinitiators, such as benzoin methyl ether, benzoin, isopropyl ether, 2,2-dimethyl-2-phenylacetophenone, 1,1-dichloroacetophenone, 1-hydroxy cyclohexyl phenyl ketone, 2-methyl-1-[4-(methylthio) phenyl]-2-morpholinylacet-1-one, N,N-dimethyl amino acetophenone, 2,4-dimethyl 9-oxdibenzothian, 2,4-diethyl 9-oxdibenzothian, 2-chloro-9-oxdibenzothian, 2,4-diisopropyl 9-oxdibenzothian, benzophenone dimethyl acetal, diphenylketone, methyl diphenylketone, 4,4′-dichlorobenzophenone, 4,4′-diethylamino phenyl ketone, Michler's ketone, 4-phenylmethylacyldiphenyl phosphorus oxide etc., which can be used separately or after mixing; moreover, the best combination shall be 2-methyl-1-[4-(methylthio) phenyl]-2-morpholinylacet-1-one (Irgacure 907) and 2,4-diisopropyl 9-oxdibenzothian (Kayacure ITX manufactured by the chemical company in Japan).

### Claim 6 (depends on 1)

The composition as claimed in claim 1, wherein the dosage of the component (E) inorganic filler is 10-30 weight % (total amount of resin is defined as the sum of component (A)+component (B)+component (C) and component (D)), and the inorganic fillers, such as talcum powder, magnesium carbonate, calcium carbonate, alumina, powder of silicon dioxide, etc., are used after mixing.

### Claim 7 (depends on 1)

The composition as claimed in claim 1, wherein the dosage of the component (F) accelerant is 0.1-2.0 weight % (total amount of resin is defined as the sum of component (A)+component (B)+component (C) and component (D)), and the hardening accelerant can be selected from imidazoles, quaternary ammonium compounds, and quaternary phosphates, and commonly dimethyl imidazole, diphenylimidazole, bis(hydroxymethyl) diphenylimidazole, etc.

### Claim 8 (depends on 1)

The composition as claimed in claim 1, wherein the dosage of the component (G) organic solvent is solid content 10-30 weight % preferably and and the organic solvent is selected from propylene carbonate, butoxyethanol, butoxyethyl acetate, methylbenzene, dimethylbenzene, butyl carbitol acetate, cyclohexanone, propylene glycol monomethyl ether, dipropylene glycol diethyl ether, methyl carbitol acetate, etc., and the propylene carbonate and the butoxyethyl acetate are preferable in the embodiment.

### Claim 9 (depends on 1)

The low Dk/Df solder resistant composition as claimed in claim 1, wherein the component A photopolymerizable prepolymer (represented by formula 1) prepared by reacting (a1) dicyclo pentadiene-phenol novolac multifunctional epoxy, or (a2) polyphenyl ether modified multifunctional epoxy resin or any combination of two (a1), (a2) with (b) mono carboxlic acid comprising a vinyl group, then reacting with (c) a saturated or unsaturated poly anhydride acid; The (a1) dicyclo pentadiene-phenol novolac multifunctional epoxy, and (a2) polyphenyl ether modified multifunctional epoxy resin, represented by the following formula a1 and a2.

### Claim 10 (depends on 1)

The low Dk/Df solder resistant composition as claimed in claim 1, wherein the component A photopolymerizable prepolymer (represented by formula 1) prepared by reacting (a1) dicyclo pentadiene-phenol novolac multifunctional epoxy, or (a2) polyphenyl ether modified multifunctional epoxy resin or any combination of two (a1), (a2) with (b) mono carboxlic acid comprising a vinyl group, then reacting with (c) a saturated or unsaturated poly anhydride acid; Wherein the (b) mono carboxlic acid comprising at least one vinyl group is selected from acrylic acid, methylacrylic acid, crotonic acid, cinnamic acid, and acrylic acid shall be preferable in the embodiment; Wherein (c) saturated or unsaturated poly anhydride acid is selected from succinic anhydride, hexahydrophthalic anhydride, cis-4-methyl-1,2,3,6-tetrahydrophthalic anhydride, 2,3,6-tetrahydro-3-phthalic anhydride, maleic anhydride, 2,3,6-tetrahydro-3-phthalic anhydride.