# US 2017/0363167 A1 · Sintered friction material for a friction lining

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0363167 A1
- Document ID: US20170363167A1
- Status: Published application
- Kind: A1
- Application number: 15/624,973
- Filed: 2017-06-16
- Published: 2017-12-21
- Earliest claimed: 2016-06-17
- Assignees: Hoerbiger Antriebstechnik Holding GmbH
- Applicants: Hoerbiger Antriebstechnik Holding GmbH
- Inventors: Zoltan CSANADI; Bruno TOURNERET; Peter ECHTLER; Werner FUERGUTH; Andreas OHR; Andreas SCHNABEL
- Web page: https://patentgrep.com/patent/US20170363167A1

## CPC

- F16D 69/027: {Compositions based on metals or inorganic oxides}
- B22F 3/10: Sintering only
- B22F 7/04: with one or more layers not made from powder, e.g. made from solid metal
- B22F 7/08: with one or more parts not made from powder {(B22F7/062 takes precedence)}
- C09K 3/14: Anti-slip materials; Abrasives {(products specifically intended for the fabrication of abrasive tools, blocks or papers, or for operations of the kind of sand-blasting and barrelling B24B31/14, B24C1/00; polishing compositions containing abrasive or grinding agents C09G1/02; friction compositions for brakes or clutches F16D69/02; polishing of semi-conductors H10P52/40)}
- C22C 1/05: Mixtures of metal powder with non-metallic powder (C22C1/08 takes precedence)
- C22C 1/1084: {by mechanical alloying (blending, milling)}
- C22C 29/02: based on carbides or carbonitrides
- C22C 32/0052: {only carbides}
- B22F 2301/10: Copper
- B22F 2301/30: Low melting point metals, i.e. Zn, Pb, Sn, Cd, In, Ga
- B22F 2302/10: Carbide
- B22F 2302/40: Carbon, graphite
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- B23K 35/262: {Sn as the principal constituent}
- B23K 35/302: {Cu as the principal constituent}
- F16D 2200/0026: Non-ferro
- F16D 2200/0043: Ceramic base, e.g. metal oxides or ceramic binder
- F16D 2200/0052: Carbon
- F16D 2200/0082: Production methods therefor
- F16D: COUPLINGS FOR TRANSMITTING ROTATION; CLUTCHES; BRAKES
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

A sintered friction material comprises a metallic matrix and granular constituents embedded in the matrix. The metallic matrix comprises a copper base alloy. The friction material is characterized in that the granular constituents comprise at least one sintered cemented carbide in a proportion of up to 9 weight percent, based on the total weight of the friction material. Furthermore, a friction body, in particular for clutches and brakes, that comprises a friction lining with at least one layer made of the sintered friction material, and a method for the production of a friction lining with the sintered friction material are described.

## Claims

### Claim 1

A sintered friction material comprising a metallic matrix and granular constituents embedded in the matrix, the metallic matrix comprising a copper base alloy, wherein the granular constituents comprise at least a sintered cemented carbide in a proportion of up to 9 weight percent, based on the total weight of the friction material.

### Claim 2 (depends on 1)

The friction material according to claim 1, wherein the sintered cemented carbide is contained in a proportion of 0.2 to 9 weight percent, based on the total weight of the friction material.

### Claim 3 (depends on 1)

The friction material according to claim 1, wherein the sintered cemented carbide has a grain size in a range of 1 to 200 μm.

### Claim 4 (depends on 1)

The friction material according to claim 1, wherein the sintered cemented carbide has a primary grain size in a range of 1 to 15 μm.

### Claim 5 (depends on 1)

The friction material according to claim 1, wherein the sintered cemented carbide comprises a metallic binder selected from the group consisting of iron, cobalt, nickel, chromium, molybdenum, aluminum, and combinations thereof.

### Claim 6 (depends on 5)

The friction material according to claim 5, wherein the binder is an alloy of iron, chromium, and aluminum.

### Claim 7 (depends on 1)

The friction material according to claim 1, wherein the sintered cemented carbide comprises 70 to 95 weight percent of tungsten carbide (WC) and 5 to 30 weight percent of a metallic binder, each based on the total weight of the sintered cemented carbide.

### Claim 8 (depends on 7)

The friction material according to claim 7, wherein the sintered cemented carbide comprises 83.5 to 88% WC, 9 to 11% Fe, 2.5 to 4% Cr, and 0.5 to 1.5% Al, each based on the total weight of the sintered cemented carbide.

### Claim 9 (depends on 1)

A friction body including a friction lining, comprising at least one layer made of the sintered friction material according to claim 1.

### Claim 10 (depends on 1, 9)

The friction body according to claim 9, characterized in that the friction lining comprises at least one basic layer and one outermost friction layer arranged on the basic layer, the friction layer being formed by the sintered friction material made according to claim 1.

### Claim 11 (depends on 1)

A method for the production of a friction lining comprising at least one layer made of a sintered friction material according to claim 1, in which a powder blend is provided, scattered onto a carrier or pressed into a friction foil, and subsequently sintered, the powder blend containing a copper base alloy and granular constituents, wherein the powder blend contains a sintered cemented carbide powder in a proportion of up to 9 weight percent, based on the total weight of the powder blend.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the powder blend has the following composition:
60 to 91.8 weight percent of a copper base alloy;
0 to 25 weight percent of further metals or metal alloys;
5 to 15 weight percent of graphite;
3 to 10 weight percent of granular constituents, except sintered cemented carbides, selected from metal oxides, carbides, nitrides, and borides;
0.2 to 9 weight percent of a sintered cemented carbide powder; and
0 to 15 weight percent of further additives selected from adhesion promotors, solders and fluxes;
all powder constituents together being 100 weight percent.

### Claim 13 (depends on 1)

The sintered friction material according to claim 1 configured for use in a friction lining for a friction body running in oil.