# US 2017/0362697 A1 · Transparent and highly stable screen protector

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0362697 A1
- Document ID: US20170362697A1
- Status: Published application
- Kind: A1
- Application number: 15/544,032
- Filed: 2015-07-06
- Published: 2017-12-21
- Earliest claimed: 2015-01-28
- Assignees: Siltectra GmbH
- Applicants: SILTECTRA GmbH
- Inventors: Jan Richter; Wolfram Drescher
- Web page: https://patentgrep.com/patent/US20170362697A1

## CPC

- C23C 16/01: on temporary substrates, e.g. substrates subsequently removed by etching
- B23K 26/0624: {using ultrashort pulses, i.e. pulses of 1 ns or less}
- B23K 26/08: Devices involving relative movement between laser beam and workpiece
- B23K 26/359: by providing a line or line pattern, e.g. a dotted break initiation line
- B23K 26/53: for modifying or reforming the material inside the workpiece, e.g. for producing break initiation cracks
- B32B 33/00: Layered products characterised by particular properties or particular surface features, e.g. particular surface coatings; Layered products designed for particular purposes not covered by another single class
- B32B 37/025: {Transfer laminating}
- C23C 14/0005: {Separation of the coating from the substrate}
- C23C 14/081: {of aluminium, magnesium or beryllium}
- C23C 14/5813: {using lasers}
- C23C 16/403: {of aluminium, magnesium or beryllium}
- C23C 16/56: After-treatment
- G06V 40/1329: {Protecting the fingerprint sensor against damage caused by the finger}
- A42B 3/22: Visors
- B23K 2101/36: Electric or electronic devices
- B23K 2103/00: Materials to be soldered, welded or cut
- B23K 2103/172: {wherein at least one of the layers is non-metallic}
- B23K 2103/52: {Ceramics}
- B32B 38/10: Removing layers, or parts of layers, mechanically or chemically
- B32B 2037/246: {Vapour deposition}
- B32B 2307/584: Scratch resistance
- B32B 2457/20: Displays, e.g. liquid crystal displays, plasma displays
- G02C 7/02: Lenses; Lens systems {; Methods of designing lenses}
- G02C 2202/16: Laminated or compound lenses
- G06F 3/041: Digitisers, e.g. for touch screens or touch pads, characterised by the transducing means
- G06F 2203/04107: Shielding in digitiser, i.e. guard or shielding arrangements, mostly for capacitive touchscreens, e.g. driven shields, driven grounds
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- G06V: IMAGE OR VIDEO RECOGNITION OR UNDERSTANDING
- A42B: HATS; HEAD COVERINGS (headbands A41D20/00; head-scarves A41D23/00)
- G02C: SPECTACLES; SUNGLASSES OR GOGGLES INSOFAR AS THEY HAVE THE SAME FEATURES AS SPECTACLES; CONTACT LENSES (trial frames for testing the eyes A61B3/04; goggles or eyeshields not having the same features as spectacles A61F9/00)
- G06F: ELECTRIC DIGITAL DATA PROCESSING (computer systems based on specific computational models G06N)

## Abstract

The invention relates to a method for producing at least one solid layer and comprises at least the steps of: providing a carrier substrate (4) having a sacrificial layer (8) arranged thereon or arranging a sacrificial layer (8) on the provided carrier substrate (4), producing a useful layer (6) by way of chemical or physical gas phase deposition on the sacrificial layer (8) to form a multi-layer arrangement (2), removing the useful layer (6) as a result of a material weakening produced between the useful layer (6) and the carrier substrate (4), said material weakening being brought about by modifications (12) to the sacrificial layer (8) which were produced means of laser beams (10).

## Claims

### Claim 1

A method for producing at least one solid layer, comprising at least the steps of:
Providing a carrier substrate (4) having a sacrificial layer (8) disposed thereon or arranging a sacrificial layer (8) on the provided carrier substrate (4),
Generating a wear layer (6) on the sacrificial layer (8) by chemical or physical vapour deposition to form a multilayer arrangement (2),
Separating the wear layer (6) as a consequence of a material weakening created between the wear layer (6) and the carrier substrate (4)
wherein the material weakening is caused by modifications (12) generated in the sacrificial layer (8) by LASER beams (10).

### Claim 2

Method for coating at least a transparent body (14), particularly a display glass (20) or a display protector layer,
comprising at least the steps of:
Arranging or producing the at least partly transparent body (14), particularly made of plastic, glass or a ceramic material, on a wear layer (6) produced according to claim,
or
Providing a carrier substrate (4) with a sacrificial layer (8) disposed thereon or arranging a sacrificial layer (8) on the carrier substrate (4) provided,
Generating a wear layer (6) by chemical or physical vapour deposition on the sacrificial layer (8) to form a multilayer arrangement (2),
Arranging or generating the at least partially transparent body (14) on the wear layer (6),
Separating the wear layer (6) as a consequence of a material weakening created between the wear layer (6) and the carrier substrate (4)
wherein the material weakening is caused by modifications (12) generated in the sacrificial layer (8) by LASER beams (10).

### Claim 3 (depends on 2)

Method according to claim 2,
characterised in that
the at least partly transparent body (14) is made from a polymer material, wherein the transparent body (14) has a lower modulus of elasticity than the wear layer (6), particularly a modulus of elasticity that is lower by a factor of at least 10 or a factor of 100.

### Claim 4 (depends on 2, 3)

Method according to claim 2 or 3,
characterised in that
the wear layer (6) and the transparent body (14) have an external shape with at least one curved portion (22),
wherein the modifications (12) for conducting a crack in the sacrificial layer (8) and/or the wear layer (6) are created corresponding to the external shape of the wear layer (6), or wherein the sacrificial layer (8) is produced with a surface that is curved in such a manner, or the surface of the sacrificial layer (8) is processed after production of the sacrificial layer (8) in such manner that it forms a curved surface shape, and the wear layer (6) is created with a corresponding shape due to its creation on the curved surface of the sacrificial layer (8)
or
the wear layer (6) substantially as a solid layer with a two-dimensional flat plane and the transparent body (14) has an external shape which includes at least one curved portion, wherein the wear layer (6) is applied to the transparent body (14) in such manner, particularly by bonding, that the wear layer (6) conforms to the outer shape of the transparent body (14).

### Claim 5

Method according to any one of the preceding claims, characterised in that
the wear layer (6) consists of a ceramic material, particularly silicon carbide (SiC) or aluminium oxide (Al2O3) and is created in an amorphous or polycrystalline state particularly by sputtering, wherein the wear layer (6) the ceramic material is cured by means of thermal treatment at temperatures higher than 500° C. preferably higher than 700° C. and particularly preferably higher than 1000° C. after or during production of the wear layer (6),
wherein the ceramic material preferably comprises corundum, which is produced in a gamma phase or alpha phase.

### Claim 6

Method according to any one of the preceding claims, characterised in that
the wear layer (6) is thinner than 100 μm and preferably thinner than 50 μm and particularly preferably 20 μm thick or thinner than 20 μm.

### Claim 7

Method according to any one of the preceding claims, characterised in that
the modifications (12) are local cracks in the crystal lattice and/or are material parts transferred into another phase and/or the modifications (12) are created by means of LASER radiation (10) introduced over an outer surface of the multilayer arrangement (2) from at least one picosecond or femtosecond LASER.

### Claim 8

Method according to any one of the preceding claims, characterised in that
the wear layer (6) is separated by means of a crack guided between the wear layer (6) and the carrier substrate (4)
wherein the crack is guided by modifications (12) generated in the sacrificial layer (8) by LASER beams (10) and/or
wherein stresses for initiating and/or propagating the crack are generated via a thermal shock to a stress-inducing layer (16) arranged additionally on the multilayer arrangement (2)
the stress-inducing layer (16) contains or consists of a polymer, particularly polydimethylsiloxane (PDMS), wherein the thermal shock is applied in such manner that the polymer undergoes a glass transition, wherein the temperature of the stress-inducing layer (16) is adjusted particularly by means of liquid nitrogen to a temperature at which the polymer undergoes at least partial and preferably complete glass transition, in which the temperature of polymer is preferably cooled to a temperature below room temperature or below 0° C. or below −50° C. or below −100° C. or below −110° C., particularly to a temperature below the glass transition temperature of the stress-inducing layer (16), or the temperature is adjusted a temperature above room temperature, particularly to a temperature between 40° C. and 180° C.

### Claim 9

Method according to any one of the preceding claims, characterised in that
the LASER beams (10) are emitted by at least one LASER device (11), wherein the LASER device (11) for providing the LASER beams (10) to be introduced into the wear layer (6) and/or the sacrificial layer (8) is configured in such manner that the LASER beams (10) emitted thereby create the modifications (12) at predetermined locations within the wear layer (6) and/or the sacrificial layer (8), wherein the LASER device (11) is adjusted such that the LASER beams (10) emitted thereby for generating the modifications (12) penetrate the wear layer (6) and/or the sacrificial layer (8) to a defined depth of less than 200 μm, preferably less than 100 μm and more preferably less than 50 μm and particularly preferably less than 20 μm, wherein the LASER device (11) has a pulse duration of less than 10 ps preferably less than 1 ps and particularly preferably less than 500 fs.

### Claim 10

Method according to any one of the preceding claims, characterised in that
the LASER device (11) comprises a femtosecond LASER (fs LASER) and the energy of the LASER beams (10) of the fs-LASER is chosen such that the propagation of the damage of any modification (12) in the wear layer (6) and/or the sacrificial layer (8) is less than 3 times the Rayleigh length, preferably less than the Rayleigh length and particularly preferably less than one-third of the Rayleigh length
and/or
the wavelength of the LASER beams (10) of the fs-LASER is chosen such the absorption by the wear layer (6) and/or the sacrificial layer (8) is less than 10 cm−1 and preferably less than 1 cm−1 and more preferably less than 0.1 cm−1
and/or the individual modifications (12) are each generated as a consequence of a o multi-photon excitation effected by the fs-LASER.

### Claim 11

Method according to any one of the preceding claims, characterised in that
the carrier substrate (4) is crystalline and the sacrificial layer (8) serves as a transfer layer, wherein the transfer layer (8) is arranged between the carrier substrate (4) and the wear layer (6) and is joined to the carrier substrate (4) and the wear layer (6),
wherein the sacrificial layer (8) is designed such that it transfers a crystal lattice information of the carrier substrate (4) to the wear layer (6),
wherein the wear layer (6) is produced or treated in such manner that at least part thereof has a crystal lattice,
wherein the formation of the crystal lattice is based at least in part on the crystal lattice information provided by the transfer layer (8).

### Claim 12 (depends on 11)

Method according to claim 11,
characterised in that
the wear layer (6) converted from an amorphous state to an at least partially, particularly mostly crystalline state as a consequence of a temperature change, wherein the wear layer (6) receives the crystal lattice information provided by the transfer layer (8) when changing states, wherein the temperature change is preferably effected by exposure to an electron beam.

### Claim 13 (depends on 10, 11)

Method according to claim 10 or claim 11, characterised in that
the sacrificial layer (8) is produced on the carrier substrate (4) in a crystalline state or arranged on the carrier substrate (4) in an amorphous state, and is converted at least partly and preferably mostly or completely to a crystalline state by a thermal shock, or
the carrier substrate (4) and the wear layer (6) consist of the same material, particularly sapphire or silicon carbide, and the sacrificial layer (8) consists of a different material from the material of the carrier substrate (4) and the wear layer (6), particularly silicon.

### Claim 14 (depends on 10, 11, 12)

Method according to any one of claims 10 to 12 characterised in that
the wear layer (6) is thinner than 100 μm and preferably thinner than 50 μm and particularly preferably 20 μm thick or thinner than 20 μm
and the sacrificial layer (8) is thinner than 10 μm and preferably thinner than 5 μm and particularly preferably 1 μm thick or thinner than 1 μm.

### Claim 15

Multilayer transparent device, particularly a display element or fingerprint sensor element or glasses lens or visor, particularly a helmet visor,
comprising at least an at least partially transparent body (14) and an at least partially transparent wear layer (6) connected to the transparent body (14),
wherein the transparent body (14) preferably contains a polymer material or a ceramic material or a viscous material such as glass, and said wear layer (6) consists of a ceramic material, wherein the wear layer (6) is harder than the transparent body (14) and
wherein the production of the multilayer transparent device comprises at least the following steps:
Generating the wear layer (6) by chemical or physical vapour deposition and
Arranging the transparent body (14) on the wear layer (6), particularly by generation or bonding.

### Claim 16 (depends on 14)

Electronic device (18),
at least comprising an image signal processing device and a display device for outputting an image signal processed by the image signal processing device, characterised in that
at least the display device and/or an optically conductive further part, such as a camera cover or a fingerprint sensor or a separate area of a touch screen, is at least partially or completely overlaid by a multilayer transparent display protector according to claim 14.