# US 2017/0362420 A1 · Heat-Activated Fabrics Made from Blends Containing Propylene-Based Polymers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0362420 A1
- Document ID: US20170362420A1
- Status: Published application
- Kind: A1
- Application number: 15/527,125
- Filed: 2015-07-20
- Published: 2017-12-21
- Earliest claimed: 2014-12-19
- Assignees: ExxonMobil Chemical Patents Inc.
- Applicants: Exxonmobil Chemical Patents Inc.
- Inventors: James N. Coffey; Galen C. Richeson; Jennifer J. Austin; Jurgen J.M. Schroeyers
- Web page: https://patentgrep.com/patent/US20170362420A1

## CPC

- C08L 23/12: Polypropene
- C08L 23/14: Copolymers of propene (C08L23/16 takes precedence)
- C08L 23/16: Ethylene-propylene or ethylene-propylene-diene copolymers
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

The invention relates to an heat-activated fabric comprising a polymer blend of 70 to 100 wt % of a polymer blend component and 0 to 30 wt % of a propylene polymer, wherein the polymer blend component comprises a first propylene-based polymer, wherein the first propylene-based polymer is a homopolymer of propylene or a copolymer of propylene and ethylene or a C4 to C10 alpha-olefin and a second propylene-based polymer, wherein the second propylene-based polymer is a homopolymer of propylene or a copolymer of propylene and ethylene or a C4 to C10 alpha-olefin, wherein the second propylene-based polymer is different than the first propylene-based polymer and wherein the polymer blend component has a MFR of greater than or equal to 20 g/10 min to less than 10,000 g/10 min; and wherein the propylene polymer has a MFR of greater than or equal to 20 g/10 min to less than 5,000 g/10 min.

## Claims

### Claim 1

A heat-activated fabric comprising a polymer blend of from about 70 to about 100 wt % of a polymer blend component and from about 0 to about 30 wt % of a propylene polymer,
wherein the polymer blend component comprises a first propylene-based polymer, wherein the first propylene-based polymer is a homopolymer of propylene or a copolymer of propylene and ethylene or a C4 to C10 alpha-olefin and a second propylene-based polymer, wherein the second propylene-based polymer is a homopolymer of propylene or a copolymer of propylene and ethylene or a C4 to C10 alpha-olefin, wherein the second propylene-based polymer is different than the first propylene-based polymer and wherein the polymer blend component has a MFR, measured according to ASTM D-1238 at 230° C. and 2.16 kg, of greater than or equal to about 20 g/10 min to less than about 10,000 g/10 min; and wherein the propylene polymer has a MFR, measured according to ASTM D-1238 at 230° C. and 2.16 kg, of greater than or equal to about 20 g/10 min to less than about 5,000 g/10 min.

### Claim 2

A heat-activated fabric comprising a polymer blend of from about 70 to about 100 wt % of a polymer blend component and from about 0 to about 30 wt % of a propylene polymer, wherein the polymer blend component comprises a first propylene-based polymer, wherein the first propylene-based polymer is a homopolymer of propylene or a copolymer of propylene and ethylene or a C4 to C10 alpha-olefin and a second propylene-based polymer, wherein the second propylene-based polymer is a homopolymer of propylene or a copolymer of propylene and ethylene or a C4 to C10 alpha-olefin, wherein the second propylene-based polymer is different than the first propylene-based polymer, wherein the polymer blend component has a melt viscosity, measured according to ASTM D-3236 at 190° C., of about 1,000 to about 10,000 cP; and
wherein the propylene polymer has a melt viscosity, measured according to ASTM D-3236 at 190° C., of about 2,000 to about 20,000 cP.

### Claim 3 (depends on 1)

The heat-activated fabric of claim 1, wherein the polymer blend component has a MFR, measured according to ASTM D-1238 at 230° C. and 2.16 kg, of greater than or equal to about 400 g/10 min to less than about 10.000 g/10 min.

### Claim 4 (depends on 1)

The heat-activated fabric of claim 1, wherein the polymer blend component has a MFR, measured according to ASTM D-1238 at 230° C. and 2.16 kg, of greater than or equal to about 20 g/10 min to less than about 400 g/10 min.

### Claim 5 (depends on 1)

The heat-activated fabric of claim 1, wherein the propylene polymer is a homopolymer of propylene or a copolymer of propylene units with from about 0.5 to about 4 wt % ethylene or C4 to C10 alpha-olefin comonomer derived units.

### Claim 6 (depends on 1)

The heat-activated fabric of claim 1, wherein the polymer blend component has an Mw of about 10,000 g/mol to about 150,000 g/mol.

### Claim 7 (depends on 1)

The heat-activated fabric of claim 1, wherein the polymer blend component is a dual reactor blend.

### Claim 8 (depends on 1)

The heat-activated fabric of claim 1, wherein the polymer blend component is a solution blend and/or melt blend.

### Claim 9 (depends on 1)

The heat-activated fabric of claim 1, wherein the first propylene-based polymer of the polymer blend component comprises a copolymer of propylene and ethylene, and the second propylene-based polymer of the polymer blend component comprises a copolymer of propylene and ethylene.

### Claim 10 (depends on 1)

The heat-activated fabric of claim 1, wherein the first propylene-based polymer of the polymer blend component and the second propylene-based propylene polymer of the polymer blend component have a difference in heat of fusion of at least 10 J/g.

### Claim 11 (depends on 1)

An article comprising the heat-activated fabric of claim 1.

### Claim 12 (depends on 11)

An article of claim 11, comprising the heat-activated fabric and one or more Substrates, wherein at least one of the one or more substrates comprises paper, cardboard, plastic, nonwoven, metal, wood, other natural fiber based material, or combinations thereof.

### Claim 13

A process to prepare a heat-activated fabric, comprising combining
a. from about 70 to about 100 wt % of a polymer blend component;
wherein the polymer blend component comprises a first propylene-based polymer, wherein the first propylene-based polymer is a homopolymer of propylene or a copolymer of propylene and ethylene or a C4 to C10 alpha-olefin and a second propylene-based polymer, wherein the second propylene-based polymer is a homopolymer of propylene or a copolymer of propylene and ethylene or a C4 to C10 alpha-olefin, wherein the second propylene-based polymer is different than the first propylene-based polymer; and
wherein the polymer blend component has a MFR, measured according to ASTM D-1238 at 230° C. and 2.16 kg, of greater than or equal to about 20 g/10 min to less than about 10,000 g/10 min; and
b. from about 0 to about 30 wt % of a propylene polymer, wherein the propylene polymer has a MFR, measured according to ASTM D-1238 at 230° C. and 2.16 kg, of greater than or equal to about 20 g/10 min to less than about 5,000 g/10 min.

### Claim 14 (depends on 13)

The process of claim 13, wherein the polymer blend component has a melt viscosity, measured according to ASTM D-3236 at 190° C., of about 1,000 to about 10,000 cP, and wherein the propylene polymer has a melt viscosity, measured according to ASTM D-3236 at 190° C., of about 2,000 to about 20,000 cP.

### Claim 15 (depends on 2)

The heat-activated fabric of claim 2, wherein the polymer blend component has a MFR, measured according to ASTM D-1238 at 230° C. and 2.16 kg, of greater than or equal to about 400 g/10 min to less than about 10,000 g/10 min.

### Claim 16 (depends on 2)

The heat-activated fabric of claim 2, wherein the polymer blend component has a MFR, measured according to ASTM D-1238 at 230° C. and 2.16 kg, of greater than or equal to about 20 g/10 min to less than about 400 g/10 min.

### Claim 17 (depends on 2)

The heat-activated fabric of claim 2, wherein the propylene polymer is a homopolymer of propylene or a copolymer of propylene units with from about 0.5 to about 4 wt % ethylene or C4 to C10 alpha-olefin comonomer derived units.

### Claim 18 (depends on 2)

The heat-activated fabric of claim 2, wherein the polymer blend component has an Mw of about 10,000 g/mol to about 150,000 g/mol.

### Claim 19 (depends on 2)

The heat-activated fabric of claim 2, wherein the polymer blend component is a dual reactor blend.

### Claim 20 (depends on 2)

The heat-activated fabric of claim 2, wherein the polymer blend component is a solution blend and/or melt blend.