# US 2017/0361309 A1 · Catalyst for ethane odh

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0361309 A1
- Document ID: US20170361309A1
- Status: Published application
- Kind: A1
- Application number: 15/617,426
- Filed: 2017-06-08
- Published: 2017-12-21
- Earliest claimed: 2016-06-20
- Assignees: NOVA Chemicals (International) S.A.
- Applicants: NOVA Chemicals (International) S.A.
- Inventors: Vasily Simanzhenkov; Xiaoliang Gao; David Jeffrey Sullivan; Leonid Modestovich Kustov; Aleksey Victorovich Kucherov; Elena Dmitrievna Finashina
- Web page: https://patentgrep.com/patent/US20170361309A1

## CPC

- B01J 27/0576: {Tellurium; Compounds thereof}
- B01J 23/002: {Mixed oxides other than spinels, e.g. perovskite}
- B01J 23/6525: {Molybdenum}
- B01J 37/0207: {Pretreatment of the support}
- B01J 37/0213: {Preparation of the impregnating solution}
- B01J 37/0236: {Drying, e.g. preparing a suspension, adding a soluble salt and drying}
- B01J 37/04: Mixing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/10: in the presence of water, e.g. steam
- C07C 5/48: with oxygen as an acceptor
- B01J 2523/00: Constitutive chemical elements of heterogeneous catalysts
- Y02P 20/52: using catalysts, e.g. selective catalysts
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A catalyst for oxidative dehydrogenation (ODH) of ethane with an empirical formula Mo—V—Te—Nb—Pd—O produced using a process comprising impregnation of the Pd component on the surface of the catalyst following a calcination step using a Pd compound free of halogens. The resulting catalyst can be used in both diluted and undiluted ODH processes and shows higher than expected activity without any loss of selectivity.

## Claims

### Claim 1

A process for preparing an oxidative dehydrogenation catalyst comprising a mixed metal oxide having the empirical formula
MoaVbTecNbdPdeOf
wherein
a, b, c, d, e and f are the relative atomic amounts of the elements Mo, V, Te, Nb, Pd and O, respectively; and
when a=1, b=0.01 to 1.0, c=0.01 to 1.0, d=0.01 to 1.0, 0.001<e≦0.10 and f is dependent on the oxidation state of the other elements;
the process comprising:
i) admixing compounds of elements Mo, V, Te, and Nb, in a solvent comprising water to produce a first mixture;
ii) heating said first mixture in a first pressurized vessel at a temperature of from 100° C. to 200° C., for from 6 hours to 240 hours;
iii) recovering first insoluble material from said first pressurized vessel;
iv) subjecting said first recovered insoluble material to a calcining under an inert atmosphere to produce a calcined product;
v) then, impregnating said calcined product from iv) with an aqueous solution of a Pd compound free of halogens to form second mixture;
vi) subjecting said second mixture to drying at a temperature of from 50° C. to 150° C., for from 1 hour to 48 hours; and
vii) recovering second insoluble material from vi) to obtain a catalyst.

### Claim 2 (depends on 1)

The process of claim 1 wherein the step ii) heating of said first mixture in said first pressurized vessel is done at a temperature of from 160° C. to 185° C.

### Claim 3 (depends on 1)

The process of claim 1 wherein the step vi) drying temperature is from 120° C. to 130° C.

### Claim 4 (depends on 1)

The process of claim 1 wherein b equals from 0.1 to 0.5.

### Claim 5 (depends on 1)

The process of claim 1 wherein b equals from 0.2 to 0.4.

### Claim 6 (depends on 1)

The process of claim 1 wherein c equals from 0.05 to 0.4.

### Claim 7 (depends on 1)

The process of claim 1 wherein c equals from 0.08 to 0.3.

### Claim 8 (depends on 1)

The process of claim 1 wherein d equals from 0.05 to 0.4.

### Claim 9 (depends on 1)

The process of claim 1 wherein d equals from 0.08 to 0.3.

### Claim 10 (depends on 1)

The process of claim 1 wherein d equals from 0.10 to 0.25.

### Claim 11 (depends on 1)

The process of claim 1 wherein e equals from 0.005 to 0.10.

### Claim 12 (depends on 1)

The process of claim 1 wherein e equals from 0.01 to 0.05.

### Claim 13 (depends on 1)

The process of claim 1 wherein e equals from 0.015 to 0.03.

### Claim 14 (depends on 1)

The process of claim 1 wherein the inert atmosphere comprises gaseous nitrogen.

### Claim 15 (depends on 1)

The process of claim 1 wherein the said first recovered insoluble material is calcined at a temperature of from 500° C. to 700° C., (preferably from 550° C. to 650° C., most preferably from 580° C. to 620° C.), for from 1 hours to 8 hours.

### Claim 16 (depends on 1)

The process of claim 1 wherein the said first recovered insoluble material is calcined by ramping temperature from at or about room temperature to at or about 600° C. over a period of 4 to 7 hours, followed by holding at or about 600° C. for from 1 hour to 4 hours.

### Claim 17 (depends on 1)

The process of claim 1 wherein the Pd compound free of halogens is selected from [Pd(NH3)4](NO3)2, Pd(HCO3)2, Pd(CH3COO)2 and an analogous Pd containing salt.

### Claim 18 (depends on 1)

The process of claim 1 wherein impregnation of said calcined product is accomplished by admixing an aqueous solution of a Pd compound free of halogens.

### Claim 19

An oxidative dehydrogenation catalyst comprising a mixed metal oxide having the empirical formula
MoaVbTecNbdPdeOf
wherein
a, b, c, d, e and f are the relative atomic amounts of the elements Mo, V, Te, Nb, Pd and O, respectively; and
when a=1, b=0.01 to 1.0, c=0.01 to 1.0, d=0.01 to 1.0, 0.001<e≦0.10 and f is dependent on the oxidation state of the other elements;
prepared by a process comprising:
i) admixing compounds of elements Mo, V, Te, and Nb, in a solvent comprising water to produce a first mixture;
ii) heating said first mixture in a first pressurized vessel at a temperature of from 100° C. to 200° C., for from 6 hours to 240 hours;
iii) recovering first insoluble material from said first pressurized vessel;
iv) subjecting said first recovered insoluble material to a calcining under an inert atmosphere to produce a calcined product;
v) then, impregnating said calcined product from iv) with an aqueous solution of a Pd compound free of halogens to form second mixture;
vi) subjecting said second mixture to drying at a temperature of from 50° C. to 150° C., for from 1 hour to 48 hours; and
vii) recovering second insoluble material from vi) to obtain a catalyst.

### Claim 20 (depends on 19)

The process of claim 19 wherein impregnation of said calcined product is accomplished by admixing an aqueous solution of a Pd compound free of halogens.