# US 2017/0345999 A1 · Integrated circuits with magnetic tunnel junctions and methods for producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0345999 A1
- Document ID: US20170345999A1
- Status: Published application
- Kind: A1
- Application number: 15/443,799
- Filed: 2017-02-27
- Published: 2017-11-30
- Earliest claimed: 2016-04-26
- Assignees: Globalfoundries Singapore Pte. Ltd.
- Applicants: Globalfoundries Singapore Pte. Ltd.
- Inventors: Seungmo Noh; Kazutaka Yamane; Kangho Lee
- Web page: https://patentgrep.com/patent/US20170345999A1

## CPC

- H10N 50/85: Materials of the active region
- H01F 10/145: {containing Al, e.g. SENDUST}
- H01F 10/16: containing cobalt ({H01F10/126} , H01F10/13 take precedence)
- H01F 10/3213: {Exchange coupling of magnetic semiconductor multilayers, e.g. MnSe/ZnSe superlattices}
- H01F 41/32: for applying conductive, insulating or magnetic material on a magnetic film {, specially adapted for a thin magnetic film}
- H10N 50/10: Magnetoresistive devices
- H10B 61/22: {of the field-effect transistor [FET] type}
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

Integrated circuits and methods of producing the same are provided. In an exemplary embodiment, an integrated circuit includes a magnetic tunnel junction with a fixed layer, a total free structure, and a barrier layer between the fixed layer and the total free structure. The total free structure includes a first free layer, a second free layer, and a first spacer layer disposed between the first and second free layers. The first spacer layer is non-magnetic. At least one of the first or second free layers include a primary free layer alloy with cobalt, iron, boron, and a free layer additional element. The free layer additional element is present at from about 1 to about 10 atomic percent. The free layer additional element is selected from one or more of molybdenum, aluminum, germanium, tungsten, vanadium, niobium, tantalum, zirconium, manganese, titanium, chromium, silicon, and hafnium.

## Claims

### Claim 1

An integrated circuit comprising:
a magnetic tunnel junction comprising a fixed layer, a total free structure, and a barrier layer positioned between the fixed layer and the total free structure, wherein the total free structure comprises a first free layer, a second free layer, and a first spacer layer, wherein the first spacer layer is non-magnetic, wherein the first spacer layer is disposed between the first free layer and the second free layer, wherein at least one of the first free layer or the second free layer comprise a primary free layer alloy, wherein the primary free layer alloy comprises an alloy of cobalt, iron, boron, and a free layer additional element, wherein the free layer additional element is present at a concentration of from about 1 atomic percent to about 10 atomic percent, based on a total weight of the primary free layer alloy, and wherein the free layer additional element is selected from one or more of molybdenum (Mo), aluminum (Al), germanium (Ge), tungsten (W), vanadium (V), niobium (Nb), tantalum (Ta), zirconium (Zr), manganese (Mn), titanium (Ti), chromium (Cr), silicon (Si), and hafnium (Hf).

### Claim 2 (depends on 1)

The integrated circuit of claim 1 wherein the free layer additional element is selected from one or more of Mo, W, Nb, Ta, Zr, Mn, Ti, Si, and Hf.

### Claim 3 (depends on 1)

The integrated circuit of claim 1 wherein the free layer additional element is Mo.

### Claim 4 (depends on 1)

The integrated circuit of claim 1 wherein the first spacer layer comprises a non-magnetic material selected from one or more of titanium (Ti), vanadium (V), chromium (Cr), zirconium (Zr), niobium (Nb), molybdenum (Mo), hafnium (Hf), tantalum (Ta), tungsten (W), and aluminum (Al).

### Claim 5 (depends on 1)

The integrated circuit of claim 1 wherein the total free structure comprises a third free layer, wherein the third free layer directly contacts one of the first free layer or the second free layer.

### Claim 6 (depends on 5)

The integrated circuit of claim 5 wherein one of the first free layer and the second free layer consists of iron and cobalt.

### Claim 7 (depends on 5)

The integrated circuit of claim 5 wherein the first free layer, the second free layer, and the third free layer all have different compositions.

### Claim 8 (depends on 5)

The integrated circuit of claim 5 wherein the third free layer comprises about 100 percent of a tertiary free layer alloy, wherein the tertiary free layer alloy is an alloy of cobalt, iron, boron, and the free layer additional element.

### Claim 9 (depends on 8)

The integrated circuit of claim 8 wherein the tertiary free layer alloy has a different composition than the primary free layer alloy.

### Claim 10 (depends on 1)

The integrated circuit of claim 1 wherein the magnetic tunnel junction further comprises:
a second spacer layer that is non-magnetic, wherein the second spacer layer overlies the second free layer;
a third free layer that is magnetic, wherein the third free layer overlies the second spacer layer.

### Claim 11 (depends on 1)

The integrated circuit of claim 1 wherein one of the first free layer or the second free layer consists of an alloy of cobalt, iron, and boron.

### Claim 12 (depends on 1)

The integrated circuit of claim 1 wherein one of the first free layer or the second free layer comprises an alloy of iron and cobalt at about 100 atomic percent.

### Claim 13

An integrated circuit comprising:
a magnetic tunnel junction comprising a fixed layer, a total free structure, and a barrier layer positioned between the fixed layer and the total free structure, wherein the total free structure comprises a first free layer, a second free layer, and a first spacer layer, wherein the first spacer layer is non-magnetic, wherein the first free layer and the second free layer are magnetic, wherein the first spacer layer is disposed between the first free layer and the second free layer, wherein at least one of the first free layer or the second free layer comprise a primary free layer alloy, wherein the primary free layer alloy comprises an alloy of cobalt, iron, boron, and a free layer additional element, wherein the free layer additional element is non-magnetic, based on a total weight of the primary free layer alloy.

### Claim 14 (depends on 13)

The integrated circuit of claim 13 wherein one of the first free layer or the second free layer consists of cobalt, iron, and boron.

### Claim 15 (depends on 13)

The integrated circuit of claim 13 wherein the total free structure further comprises a third free layer, wherein the third free layer is magnetic.

### Claim 16 (depends on 15)

The integrated circuit of claim 15 wherein the third free layer directly contacts one of the first free layer and the second free layer.

### Claim 17 (depends on 16)

The integrated circuit of claim 16 wherein the third free layer consists of cobalt and iron.

### Claim 18 (depends on 17)

The integrated circuit of claim 17 wherein the first free layer and the second free layer comprise the free layer additional element.

### Claim 19 (depends on 15)

The integrated circuit of claim 15 further comprising:
a second spacer layer overlying the second free layer, wherein the third free layer overlies the second spacer layer.

### Claim 20

A method of producing an integrated circuit comprising:
forming a fixed layer, wherein the fixed layer is magnetic;
forming a barrier layer overlying the fixed layer, wherein the barrier layer comprises a non-magnetic material;
forming a total free structure overlying the barrier layer, wherein the total free structure comprises a first free layer that is magnetic, a first spacer layer overlying the first free layer, wherein the first spacer layer is non-magnetic, a second free layer overlying the first spacer layer wherein the second free layer is magnetic, wherein at least one of the first free layer or the second free layer comprise a primary free layer alloy, wherein the primary free layer alloy comprises an alloy of cobalt, iron, boron, and a free layer additional element, where the free layer additional element is present in the primary free layer alloy at a concentration of from about 1 atomic percent to about 10 atomic percent, based on a total weight of the primary free layer alloy, and wherein the free layer additional element is selected from one or more of molybdenum (Mo), aluminum (Al), germanium (Ge), tungsten (W), vanadium (V), niobium (Nb), tantalum (Ta), zirconium (Zr), manganese (Mn), titanium (Ti), chromium (Cr), silicon (Si), and hafnium (Hf).