# US 2017/0323785 A1 · Method to deposit conformal and low wet etch rate encapsulation layer using pecvd

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0323785 A1
- Document ID: US20170323785A1
- Status: Published application
- Kind: A1
- Application number: 15/279,314
- Filed: 2016-09-28
- Published: 2017-11-09
- Earliest claimed: 2016-05-06
- Applicants: Lam Research Corporation
- Inventors: Akhil Singhal; Joseph Hung-chi Wei; Yisha Mao; Bart J. van Schravendijk
- Web page: https://patentgrep.com/patent/US20170323785A1

## CPC

- H10P 14/6336: {in the presence of a plasma [PECVD]}
- C23C 16/325: {Silicon carbide}
- C23C 16/345: {Silicon nitride}
- C23C 16/50: using electric discharges {(generation and control of plasma in discharge tubes for surface treatment H01J37/32, H01J37/34)}
- C23C 16/515: using pulsed discharges
- C23C 16/56: After-treatment
- H01J 37/32009: {Arrangements for generation of plasma specially adapted for examination or treatment of objects, e.g. plasma sources (plasma generation in general H05H1/24)}
- H01J 37/32082: {Radio frequency generated discharge (H01J37/32357, H01J37/32366, H01J37/32394 and H01J37/32403 take precedence)}
- H01J 37/32155: {Frequency modulation}
- H01J 37/32165: {Plural frequencies}
- H01J 37/3244: {Gas supply means}
- H10N 50/01: Manufacture or treatment
- H10N 50/10: Magnetoresistive devices
- H10N 50/80: Constructional details
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/6532: {by exposure to a plasma}
- H10P 14/6538: {by exposure to UV light}
- H10P 14/6682: {the compound being a silane, e.g. disilane, methylsilane or chlorosilane}
- H10P 14/6905: {being a silicon carbide or silicon carbonitride and not containing oxygen, e.g. SiC or SiC:H}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 14/6922: {the material containing Si, O and at least one of H, N, C, F or other non-metal elements, e.g. SiOC, SiOC:H or SiONC}
- H10P 14/6939: {characterised by the metal}
- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- H10W 74/01: Manufacture or treatment
- H10W 74/43: comprising oxides, nitrides or carbides, e.g. ceramics or glasses
- H01J 2237/3321: CVD [Chemical Vapor Deposition]
- H01J 2237/334: Etching
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Methods of depositing conformal, dense silicon-containing films having low hydrogen content are provided herein. Methods involve pulsing a plasma while exposing a substrate to a silicon-containing precursor and reactant to facilitate a primarily radical-based pulsed plasma enhanced chemical vapor deposition process for depositing a conformal silicon-containing film. Methods also involve periodically performing a post-treatment operation whereby, for every about 20 Å to about 50 Å of film deposited using pulsed plasma PECVD, the deposited film is exposed to an inert plasma to densify and reduce hydrogen content in the deposited film.

## Claims

### Claim 1

A method of processing a substrate housed in a process chamber, the method comprising:
introducing a silicon-containing precursor and a reactant to the process chamber at a substrate temperature less than about 400° C.;
igniting and pulsing a first plasma while introducing the silicon-containing precursor and the reactant to generate radical species for forming a silicon-containing film over the substrate; and
after forming the silicon-containing film, performing a post-treatment operation, the post-treatment operation comprising:
stopping flow of the silicon-containing precursor and the flow of the reactant;
introducing a post-treatment gas into the process chamber; and
igniting a second plasma to treat the silicon-containing film,
wherein a duration of each pulse during the pulsing of the first plasma is between about 0.02 ms and about 5 ms, and
wherein the silicon-containing precursor is silane (SiH4).

### Claim 2 (depends on 1)

The method of claim 1, wherein the first plasma is pulsed between 500 and 2000 times.

### Claim 3 (depends on 1)

The method of claim 1, wherein the post-treatment operation is performed after the silicon-containing film is formed to a thickness between about 20 Å and about 50 Å.

### Claim 4 (depends on 1)

The method of claim 1, wherein the second plasma is ignited for a duration between about 10 seconds and about 60 seconds.

### Claim 5 (depends on 1)

The method of claim 1, wherein the silicon-containing film is silicon oxide and the post-treated silicon-containing film has a wet etch rate in a 100:1 hydrofluoric acid solution of about 50 Å/minute.

### Claim 6

A method of processing a substrate housed in a process chamber, the method comprising:
introducing a silicon-containing precursor and a reactant to the process chamber at a substrate temperature less than about 400° C.;
igniting and pulsing a first plasma while introducing the silicon-containing precursor and the reactant to generate radical species for forming a silicon-containing film over the substrate; and
after forming the silicon-containing film, performing a post-treatment operation, the post-treatment operation comprising:
stopping flow of the silicon-containing precursor and the flow of the reactant;
introducing a post-treatment gas into the process chamber; and
igniting a second plasma to treat the silicon-containing film,
wherein a duration of each pulse during the pulsing of the first plasma is between about 0.02 ms and about 5 ms, and
wherein the silicon-containing film is silicon nitride and the post-treated silicon-containing film has a wet etch rate in a 100:1 hydrofluoric acid solution of less than about 20 Å/minute.

### Claim 7 (depends on 1)

The method of claim 1, wherein the silicon-containing film is selected from the group consisting of silicon nitride, silicon carbide, and silicon oxide.

### Claim 8 (depends on 1)

The method of claim 1, wherein the silicon-containing film is deposited at a temperature of between about 250° C. and about 350° C.

### Claim 9 (depends on 1)

The method of claim 1, wherein the post-treatment operation is performed at a temperature of between about 250° C. and about 350° C.

### Claim 10 (depends on 1)

The method of claim 1, wherein the process chamber has a chamber pressure between about 2 Torr and about 10 Torr.

### Claim 11 (depends on 1)

The method of claim 1, wherein the silicon-containing film is deposited over a magnetic device.

### Claim 12 (depends on 1)

The method of claim 1, wherein the first and second plasma are generated in situ.

### Claim 13 (depends on 1)

The method of claim 1, wherein the first and second plasmas are ignited using a dual frequency plasma generator.

### Claim 14

(canceled)

### Claim 15

A method of processing a substrate housed in a process chamber, the method comprising:
introducing a silicon-containing precursor and a reactant to the process chamber at a substrate temperature less than about 400° C.;
igniting and pulsing a first plasma while introducing the silicon-containing precursor and the reactant to generate radical species for forming a silicon-containing film over the substrate; and
after forming the silicon-containing film, performing a post-treatment operation, the post-treatment operation comprising:
stopping flow of the silicon-containing precursor and the flow of the reactant;
introducing a post-treatment gas into the process chamber; and
igniting a second plasma to treat the silicon-containing film,
wherein a duration of each pulse during the pulsing of the first plasma is between about 0.02 ms and about 5 ms,
wherein the first and second plasmas are ignited using a dual frequency plasma generator, and
wherein the silicon-containing film is silicon nitride, and wherein the density of the silicon nitride is at least about 2.6 g/cm3.

### Claim 16 (depends on 1)

The method of claim 1, wherein the first and second plasmas are ignited using a single frequency plasma generator.

### Claim 17

(canceled)

### Claim 18 (depends on 16)

The method of claim 16, wherein the silicon-containing film is silicon nitride, and wherein the density of the silicon nitride is at least about 2.1 g/cm3.

### Claim 19 (depends on 1)

The method of claim 1, wherein the silicon-containing film is deposited as an encapsulation layer over a magnetic device.

### Claim 20 (depends on 1)

The method of claim 1, wherein the post-treatment operation is performed to remove hydrogen from the silicon-containing film.