# US 2017/0323777 A1 · Selectively lateral growth of silicon oxide thin film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0323777 A1
- Document ID: US20170323777A1
- Status: Published application
- Kind: A1
- Application number: 15/656,045
- Filed: 2017-07-21
- Published: 2017-11-09
- Earliest claimed: 2015-02-09
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Yihong CHEN; Kelvin CHAN; Shaunak MUKHERJEE; Abhijit Basu MALLICK
- Web page: https://patentgrep.com/patent/US20170323777A1

## CPC

- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- C23C 16/45525: {Atomic layer deposition [ALD]}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6506: {Formation of intermediate materials}
- H10P 14/6508: {by exposure to a liquid}
- H10P 14/6512: {by exposure to a gas or vapour}
- H10P 14/6514: {by exposure to a plasma}
- H10P 14/6682: {the compound being a silane, e.g. disilane, methylsilane or chlorosilane}
- H10P 14/6684: {the compound comprising silicon and oxygen}
- H10P 14/6686: {the compound being a molecule comprising at least one silicon-oxygen bond and the compound having hydrogen or an organic group attached to the silicon or oxygen, e.g. a siloxane}
- H10P 14/6687: {the compound comprising silicon and nitrogen}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 14/6922: {the material containing Si, O and at least one of H, N, C, F or other non-metal elements, e.g. SiOC, SiOC:H or SiONC}
- H10P 76/4085: {characterised by the processes involved to create the masks}
- H10P 95/00: Generic processes or apparatus for manufacture or treatments not covered by the other groups of this subclass
- H10W 20/077: {on sidewalls or on top surfaces of conductors (H10W20/076 takes precedence)}
- H10W 20/4421: {the principal metal being copper}
- H10W 20/076: {in via holes or trenches}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Implementations disclosed herein generally relate to methods of forming silicon oxide films. The methods can include performing silylation on the surface of the substrate having terminal hydroxyl groups. The hydroxyl groups on the surface of the substrate are then regenerated using a plasma and H2O soak in order to perform an additional silylation. Further methods include catalyzing the exposed surfaces using a Lewis acid, directionally inactivating the exposed first and second surfaces and deposition of a silicon containing layer on the sidewall surfaces. Multiple plasma treatments may be performed to deposit a layer having a desired thickness.

## Claims

### Claim 1

A method of processing a substrate, comprising:
(a) conformally forming a catalyst layer on an exposed surface of a layer formed over a substrate, wherein the catalyst layer comprises trimethylaluminum (TMA);
(b) exposing the substrate to a plasma formed from a catalyst deactivator gas, wherein the catalyst deactivator gas comprises O2, N2, NH3, H2, H2O, He, Ar, or any combination thereof;
(c) exposing the substrate to a silanol to form a material layer on the substrate; and
(d) repeating (a) to (c) until a desired thickness of the material layer is achieved.

### Claim 2 (depends on 1)

The method of claim 1, wherein the silanol is a compound having the general formula Si(OR)3OH, the R group being a hydrocarbon.

### Claim 3 (depends on 2)

The method of claim 2, wherein the silanol is tris-(tert-butoxy)silanol, tris-(tert-pentoxy)silanol, or derivatives thereof.

### Claim 4 (depends on 1)

The method of claim 1, wherein the material layer is silicon oxide.

### Claim 5 (depends on 1)

The method of claim 1, wherein the catalyst deactivator gas is O2 or H2O.

### Claim 6 (depends on 1)

The method of claim 1, wherein the substrate is biased during the process.

### Claim 7 (depends on 1)

The method of claim 1, wherein the layer is a dielectric layer.

### Claim 8 (depends on 1)

The method of claim 1, wherein the material layer is formed on sidewalls of a patterned feature formed in the layer.

### Claim 9

A method of processing a substrate, comprising:
providing a substrate having a first layer and a second layer disposed over the first layer, the second layer being patterned to expose a portion of a top surface of the first layer, wherein the second layer having a top surface and sidewall surfaces;
forming a catalyst layer on the exposed top surface of the first layer and the top surface and the sidewall surfaces of the second layer, wherein the catalyst layer comprises trimethylaluminum (TMA), tetramethyl titanium, tetramethyl zinc or combinations thereof;
exposing the substrate to a plasma formed from a catalyst deactivator gas, wherein the catalyst deactivator gas comprises O2, N2, NH3, H2, H2O, He, Ar, or any combination thereof, and the substrate is being biased while exposing to the plasma;
exposing the substrate to a silanol to form a material layer on the substrate; and
repeating forming a catalyst layer on the exposed top surface of the first layer and the top surface and the sidewall surfaces of the second layer, exposing the substrate to a plasma formed from a catalyst deactivator gas, and exposing the substrate to a silanol to form a material layer on the substrate until a predetermined thickness of the material layer is achieved.

### Claim 10 (depends on 9)

The method of claim 9, wherein the silanol is a compound having the general formula Si(OR)3OH, the R group being a hydrocarbon.

### Claim 11 (depends on 10)

The method of claim 10, wherein the silanol is tris-(tert-butoxy)silanol, tris-(tert-pentoxy)silanol, or derivatives thereof.

### Claim 12 (depends on 9)

The method of claim 9, wherein the material layer is silicon oxide.

### Claim 13 (depends on 9)

The method of claim 9, wherein the catalyst deactivator gas is O2 or H2O.

### Claim 14 (depends on 9)

The method of claim 9, wherein the material layer is formed on the sidewall surfaces of the second layer.

### Claim 15 (depends on 9)

The method of claim 9, wherein the first layer is a metal-containing layer.

### Claim 16 (depends on 9)

The method of claim 9, wherein the second layer is a dielectric layer.