# US 2017/0321347 A1 · Isoelectronic surfactant induced sublattice disordering in optoelectronic devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0321347 A1
- Document ID: US20170321347A1
- Status: Published application
- Kind: A1
- Application number: 15/654,576
- Filed: 2017-07-19
- Published: 2017-11-09
- Earliest claimed: 2002-10-02
- Assignees: The Boeing Company
- Applicants: The Boeing Company
- Inventors: Christopher M. FETZER; James H. ERMER; Richard R. KING; Peter C. COLTER
- Web page: https://patentgrep.com/patent/US20170321347A1

## CPC

- C30B 25/186: {being specially pre-treated by, e.g. chemical or physical means}
- C30B 29/40: AIIIBV compounds {wherein A is B, Al, Ga, In or Tl and B is N, P, As, Sb or Bi}
- H10F 10/142: comprising multiple PN homojunctions, e.g. tandem cells
- H10F 71/127: {The active layers comprising only Group III-V materials, e.g. GaAs or InP}
- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10P 14/3211: {Silicon, silicon germanium or germanium}
- H10P 14/3216: {Nitrides}
- H10P 14/3221: {Arsenides}
- H10P 14/3248: {consisting of two layers}
- H10P 14/3402: {characterised by the chemical composition}
- H10P 14/3418: {Phosphides}
- H10P 14/36: {characterised by treatments done before the formation of the materials}
- Y02E 10/544: Solar cells from Group III-V materials
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method of disordering a layer of an optoelectronic device including; growing a plurality of lower layers; introducing an isoelectronic surfactant; growing a layer; allowing the surfactant to desorb; and growing subsequent layers all performed at a low pressure of 25 torr.

## Claims

### Claim 1

A method of making a III-V optoelectronic device, comprising:
growing a lower structure;
introducing an isoelectronic surfactant in a molar ratio of isoelectronic surfactant to group-III precursor that is between about 1×10−5 to 0.2; and
growing a subsequent structure at a reduced pressure of 10 to 100 torr in the presence of the isoelectronic surfactant;
wherein a band gap associated with the subsequent structure is increased by a disordering induced by the isoelectronic surfactant to substantially match a photogenerated current between the subsequent structure and one or more other layers;
wherein the subsequent structure is characterized by an ordering parameter η that is at most about 0.3; and
wherein any remaining CuPtB-type ordering of the subsequent structure produces at most 0.100 eV of band gap reduction from a disordered alloy maximum.

### Claim 2 (depends on 1)

The method of claim 1, wherein the lower structure comprises a bottom subcell and a middle subcell.

### Claim 3 (depends on 1)

The method of claim 1, wherein a first side of the subsequent structure comprises an n-type side.

### Claim 4 (depends on 1)

The method of claim 1, wherein the subsequent structure comprises a top layer selected from the group consisting of GaInP, GaInAs, GaAsSb, GaPAs, GaInPAs, AlInP, AlGaInP, AlGaAs, AlGaInAs, AlGaAsSb, AlGaPAs, AlInAs, InPAs, AlInPAs, SiGe, CdZnSe, CdZnTe, ZnSSe, ZnSeTe, CuGaInSe, CuGaInSSe, and AgGaInSe.

### Claim 5 (depends on 1)

The method of claim 1, wherein the isoelectronic surfactant comprises Sb.

### Claim 6 (depends on 5)

The method of claim 5, wherein the subsequent structure comprises GaInP.

### Claim 7 (depends on 6)

The method of claim 6, wherein the GaInP comprises GaxIn1-xP and is mismatched to a substrate material.

### Claim 8 (depends on 6)

The method of claim 6, wherein introducing the isoelectronic surfactant comprises introducing according to the molar ratio as TESb/(TMGa+TMIn) wherein TESb is triethylantimony, TMGa is trimethylgallium, and TMIn is trimethylindium.

### Claim 9 (depends on 1)

The method of claim 1, wherein the device comprises a solar cell.

### Claim 10

A method of making a III-V optoelectronic device, comprising:
growing a lower structure;
growing a first side and a second side of a tunnel junction;
introducing an isoelectronic surfactant in a molar ratio of isoelectronic surfactant to group III precursor that is between about 1×10−5 to 0.2;
increasing a band gap associated with a top structure by growing the top structure in the presence of the isoelectronic surfactant at a pressure of 10 to 100 torr; and
growing a subsequent structure:
wherein the band gap associated with the top structure is increased by a disordering induced by the isoelectronic surfactant to substantially match a photogenerated current between the top structure and one or more other layers;
wherein the top structure is characterized by an ordering parameter 11 that is at most about 0.3; and
wherein any remaining CuPtB-type ordering of the subsequent structure produces at most 0.100 eV of band gap reduction from a disordered alloy maximum.

### Claim 11 (depends on 10)

The method of claim 10, wherein the lower structure comprises a bottom subcell and a middle subcell.

### Claim 12 (depends on 10)

The method of claim 10, wherein the first side of the tunnel junction comprises an n-type side.

### Claim 13 (depends on 10)

The method of claim 10, wherein the top structure comprises a composition selected from the group consisting of GaInP, GaInAs, GaAsSb, GaPAs, GaInPAs, AlInP, AlGaInP, AlGaAs, AlGaInAs, AlGaAsSb, AlGaPAs, AlInAs, InPAs, AlInPAs, SiGe, CdZnSe, CdZnTe, ZnSSe, ZnSeTe, CuGaInSe, CuGaInSSe, and AgGaInSe.

### Claim 14 (depends on 10)

The method of claim 10, wherein the isoelectronic surfactant comprises Sb.

### Claim 15 (depends on 14)

The method of claim 14, wherein the top structure comprises GaxIn1-xP and is mismatched to a substrate material.

### Claim 16 (depends on 15)

The method of claim 15, wherein introducing the isoelectronic surfactant comprises introducing according to the molar ratio as TESb/(TMGa+TMin) wherein TESb is triethylantimony, TMGa is trimethylgallium, and TMIn is trimethylindium.

### Claim 17 (depends on 16)

The method of claim 16, wherein the molar ratio is between about 1×10−5 to 0.1.

### Claim 18

A method of making a solar cell having a GainP top layer, comprising:
growing a lower structure;
introducing an isoelectronic surfactant selected from the group consisting of Sb, As, Bi, Tl, the isoelectronic surfactant being present in a molar ratio of isoelectronic surfactant to group III precursor that is at least 1×10−5; and
growing a subsequent structure at a reduced pressure of 10 to 100 torr in the presence of the isoelectronic surfactant that comprises a top layer,
wherein the top layer comprises GaInP:
wherein a band gap associated with the top layer is increased by a disordering induced by the isoelectronic surfactant to substantially match a photogenerated current between the top layer and one or more other layers;
wherein the top layer is characterized by an ordering parameter 11 that is at most about 0.3; and
wherein any remaining CuPtB-type ordering of the subsequent structure produces at most 0.100 eV of band gap reduction from a disordered alloy maximum.

### Claim 19 (depends on 18)

The method of claim 18, wherein the top layer is further characterized by a formula selected from the group consisting of:
GayIn1-yP1-xSbx, GayIn1-yP1-xBix, GayIn1-yP1-xAsx, and (GayIn1-y)1-xTlxP.

### Claim 20 (depends on 18)

The method of claim 18, wherein the isoelectronic surfactant is Sb and is introduced in the molar ratio that is defined as TESb/(TMGa+TMIn)=about 1×10−5 to 0.1, wherein TESb is triethylantimony, TMGa is trimethylgallium, and TMIn is trimethylindium.