# US 2017/0321048 A1 · Polymer compositions and extrusion coated articles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0321048 A1
- Document ID: US20170321048A1
- Status: Published application
- Kind: A1
- Application number: 15/526,957
- Filed: 2015-11-20
- Published: 2017-11-09
- Earliest claimed: 2014-11-24
- Assignees: Borealis AG
- Applicants: Borealis AG
- Inventors: Auli NUMMILA-PAKARINEN; Mikko PELTOVUORI
- Web page: https://patentgrep.com/patent/US20170321048A1

## CPC

- C08L 23/12: Polypropene
- C09D 123/12: Polypropene
- B29C 48/0021: {combined with joining, lining or laminating}
- B29C 48/022: {characterised by the choice of material}
- B29C 48/08: flexible, e.g. films
- B29C 48/15: incorporating preformed parts or layers, e.g. extrusion moulding around inserts
- B29K 2023/10: {Polymers of propylene}
- C08L 2205/02: containing two or more polymers of the same C08L -group
- C08L 2205/03: containing three or more polymers in a blend
- C08L 2314/06: Metallocene or single site catalysts
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

The present invention relates to a polymer composition (A) comprising a blend of i) 60 to 90 wt-% of propylene polymer composition (a) comprising a blend of (a-1) 55 to 95 wt-% of propylene polymer and (a-2) 5 to 45 wt-% of low density ethylene polymer and ii) 10 to 40 wt-% of a plastomer (b) of ethylene copolymer. The invention relates also to extrusion coating articles, comprising at least a substrate layer and a heat sealable layer, wherein composition (A) is used as said heat sealable layer, process for producing the extrusion coated articles as well use of the composition (A) as a heat sealable layer in an extrusion coated article.

## Claims

### Claim at position 1

1-17. (canceled)

### Claim 18

A polymer composition (A) comprising a blend of
i) 60 to 90 wt-% of propylene polymer composition (a) comprising a blend of
(a-1) 55 to 95 wt-% of propylene polymer and
(a-2) 5 to 45 wt-% of low density ethylene polymer (LDPE) which is a high pressure polyethylene,
where the amounts of (a-1) and (a-2) are based on the total weight of composition (a), and composition (a) has a melt flow rate MFR2 of from 10 to 50 g/10 min (230° C./2.16 kg) and the Vicat softening temperature in the range of 120 to 155° C. measured according to ISO 306,
and
ii) 10 to 40 wt-% of a plastomer (b) of ethylene copolymer with at least one α-olefin comonomer of 4 to 10 C-atoms, provided that at least one comonomer is a monomer with at least 6 C-atoms
where the amounts of (i) and (ii) are based on the total weight of the composition (A), and
wherein the plastomer b) has a density of 880 to 912 kg/m3.

### Claim 19 (depends on 18)

The polymer composition (A) according to claim 18, wherein the plastomer (b) is an ethylene-C6-C10 α-olefin copolymer.

### Claim 20 (depends on 18)

The polymer composition (A) according to claim 18, wherein the plastomer (b) is produced in a solution process in the presence of a metallocene catalyst.

### Claim 21 (depends on 18)

The polymer composition (A) according to claim 18, wherein the plastomer (b) has MFR2 (190° C./2.16 kg) in the range of 3 to 25 g/10 min.

### Claim 22 (depends on 18)

The polymer composition (A) according to claim 18, wherein the polymer composition comprises a blend of
i) 70 to 85 wt-% of propylene composition (a) and
ii) 15 to 30 wt-% of plastomer (b)
based on the total amount of composition (A).

### Claim 23 (depends on 18)

The polymer composition (A) according to claim 18, wherein the propylene polymer (a-1) of composition (a) is propylene homopolymer or propylene random or block copolymer with ethylene and/or α-olefin comonomers of 4 to 12 C-atoms.

### Claim 24 (depends on 18)

The polymer composition (A) according to claim 18, wherein the low density ethylene polymer (a-2) has a density from 860 to 940 kg/m3.

### Claim 25

A polymer layer structure (PL) comprising
1) Layer 1 of polymer composition (A) comprising a blend of
i) 60 to 90 wt-% of propylene polymer composition (a) comprising a blend of
(a-1) 55 to 95 wt-% of propylene polymer and
(a-2) 5 to 45 wt-% of low density ethylene polymer (LDPE) which is a high pressure polyethylene,
where the amounts of (a-1) and (a-2) are based on the total weight of composition (a), and composition (a) has a melt flow rate MFR2 of from 10 to 50 g/10 min (230° C./2.16 kg) and the Vicat softening temperature in the range of 120 to 155° C. measured according to ISO 306,
and
ii) 10 to 40 percent by weight of a plastomer (b) of ethylene copolymer with at least one α-olefin comonomer of 4 to 10 C-atoms, provided that at least one co-monomer is a monomer with at least 6 C-atoms,
where the amounts of (i) and (ii) are based on the total weight of the composition (A), and wherein the plastomer b) has a density of 880 to 912 kg/m3
and
2) Layer 2 of a polymer composition being different to composition (A).

### Claim 26

An extrusion coated article (EC) comprising
I. a substrate layer (S) and
II. a heat sealable polymer layer (H),
wherein the heat sealable polymer layer (H) comprises a composition (A) comprising a blend of
i) 60 to 90 percent by weight of propylene polymer composition (a) comprising a blend of
(a-1) 55 to 95 percent by weight of propylene polymer and
(a-2) 5 to 45 percent by weight of low density ethylene polymer (LDPE) which is a high pressure polyethylene,
where the amounts of (a-1) and (a-2) are based on the total weight of composition (a), and composition (a) has a melt flow rate MFR2 of from 10 to 50 g/10 min (230° C./2.16 kg) and the Vicat softening temperature is in the range of 120 to 155° C. measured according to ISO 306,
and
ii) 10 to 40 percent by weight of a plastomer (b) of ethylene copolymer with at least one α-olefin comonomer of 4 to 10 C-atoms, provided that at least one co-monomer is a monomer with at least 6 C-atoms,
where the amounts of (i) and (ii) are based on the total weight of the composition (A), and wherein the plastomer (b) has a density of 880 to 912 kg/m3.

### Claim 27 (depends on 26)

The extrusion coated article (EC) according to claim 26, wherein the article comprises a Layer 2 of a polymer composition being different to composition (A) located between the substrate layer (S) and the heat sealable polymer layer (H).

### Claim 28 (depends on 26)

The extrusion coated article (EC) according to claim 26 comprising I-i a substrate layer (S) and II-i a polymer layer structure (PL), said PL comprising
1) Layer 1 of polymer composition (A) comprising a blend of
i) 60 to 90 wt-% of propylene polymer composition (a) comprising a blend of
(a-1) 55 to 95 wt-% of propylene polymer and
(a-2) 5 to 45 wt-% of low density ethylene polymer (LDPE) which is a high pressure polyethylene,
where the amounts of (a-1) and (a-2) are based on the total weight of composition (a), and composition (a) has a melt flow rate MFR2 of from 10 to 50 g/10 min (230° C./2.16 kg) and the Vicat softening temperature in the range of 120 to 155° C. measured according to ISO 306, and
ii) 10 to 40 percent by weight of a plastomer (b) of ethylene copolymer with at least one α-olefin comonomer of 4 to 10 C-atoms, provided that at least one co-monomer is a monomer with at least 6 C-atoms,
where the amounts of (i) and (ii) are based on the total weight of the composition (A), and wherein the plastomer b) has a density of 880 to 912 kg/m3
and
2) Layer 2 of a polymer composition being different to composition (A).

### Claim 29 (depends on 26)

The extrusion coated article (EC) according to claim 26, wherein the plastomer (b) is produced in solution process in the presence of a metallocene catalyst.

### Claim 30 (depends on 26)

The extrusion coated article (EC) according to claim 26, wherein the plastomer b) is an ethylene-C6-C10 α-olefin copolymer.

### Claim 31 (depends on 26)

The extrusion coated article (EC) according to claim 26, wherein the substrate layer (S) is selected from the group consisting of paper, paperboard, kraft paper, a plastic film, metallised plastic film, a metal foil, woven fabric or plastic, and combinations thereof.

### Claim 32 (depends on 26)

The extrusion coated article (EC) according to claim 26, wherein the article comprises at least one layer (M) being of a polymeric film, metal foil, metallised polymeric film, layer of fibrous material or combinations thereof.

### Claim 33 (depends on 18)

A process for producing an extrusion coated article (EC) comprising
extrusion coating a substrate (S) with a draw-down speed of at least 150 m/min by extruding a heat sealable layer (H) or co-extruding at least the polymer layer structure (PL) in a molten state through a flat die onto said substrate at a temperature of from 240 to 320° C.,
wherein the heat sealable polymer layer (H) comprises composition (A) as defined in claim 18 or is part of a polymer layer structure (PL), said PL comprising
1) Layer 1 of polymer composition (A) comprising a blend of
i) 60 to 90 wt-% of propylene polymer composition (a) comprising a blend of
(a-1) 55 to 95 wt-% of propylene polymer and
(a-2) 5 to 45 wt-% of low density ethylene polymer (LDPE) which is a high pressure polyethylene,
where the amounts of (a-1) and (a-2) are based on the total weight of composition (a), and composition (a) has a melt flow rate MFR2 of from 10 to 50 g/10 min (230° C./2.16 kg) and the Vicat softening temperature in the range of 120 to 155° C. measured according to ISO 306, and
ii) 10 to 40 percent by weight of a plastomer (b) of ethylene copolymer with at least one α-olefin comonomer of 4 to 10 C-atoms, provided that at least one co-monomer is a monomer with at least 6 C-atoms,
where the amounts of (i) and (ii) are based on the total weight of the composition (A), and wherein the plastomer b) has a density of 880 to 912 kg/m3
and
2) Layer 2 of a polymer composition being different to composition (A).

### Claim 34 (depends on 18)

A heat sealable layer of an extrusion coated article, said heat sealable layer comprising the polymer composition (A) as defined in claim 18.