Abstract
Compositions including polyaspartic acid and methods for preparing polyaspartic acid using a precondensate of aspartic acid and polyaspartimide are provided herein. Uses for such compositions are also described.
Claims23
A method for preparing polyaspartic acid, comprising the following steps:
- (a) precondensing aspartic acid at a temperature of 100 to 250° C. up to a degree of conversion of at least 2% to obtain a precondensate;
- (b) adding 1 to 25 mol % of an acidic catalyst to the precondensate to form a reaction mixture;
- (c) polycondensing the reaction mixture at 170 to 250° C. to obtain polycondensates;
- and
- (d) hydrolyzing the polycondensates with addition of a base.
2 more elements
A method for preparing polyaspartic acid, comprising the following steps:
- (i) contacting a mixture of:
- aspartic acid and 3 to 35 wt % polyaspartimide
- with
- 1 to 25 mol % of an acidic catalyst in a reactor;
- (ii) polycondensing the mixture at a temperature of 170 to 250° C. to obtain polycondensates;
- and
- (iii) hydrolyzing the polycondensates according to (ii) with addition of a base to obtain polyaspartic acid.
4 more elements
A composition comprising a polyaspartic acid obtained using a method selected from a group consisting of:
- (A) precondensing aspartic acid at a temperature of 100 to 250° C. up to a degree of conversion of at least 2% to obtain a precondensate, adding 1 to 25 mol % of an acidic catalyst to the precondensate to form a reaction mixture, polycondensing the reaction mixture at 170 to 250° C. to obtain polycondensates, and hydrolyzing the polycondensates with addition of a base;
- and
- (B) contacting a mixture of aspartic acid and 3 to 35 wt % polyaspartimide with 1 to 25 mol % of an acidic catalyst in a reactor, polycondensing the mixture at a temperature of 170 to 250° C. to obtain polycondensates, and hydrolyzing the polycondensates with addition of a base to obtain polyaspartic acid.
(canceled)
(canceled)
(canceled)
(canceled)
Dependencies are inferred from the claim text.