# US 2017/0319994 A1 · High efficiency and high capacity glass-free fuel filtration media and fuel filters and methods employing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0319994 A1
- Document ID: US20170319994A1
- Status: Published application
- Kind: A1
- Application number: 15/493,734
- Filed: 2017-04-21
- Published: 2017-11-09
- Earliest claimed: 2012-03-09
- Assignees: A. Ahlstrom Corporation
- Applicants: Ahlstrom Corporation
- Inventors: Ina PARKER
- Web page: https://patentgrep.com/patent/US20170319994A1

## CPC

- B01D 39/1623: {of synthetic origin}
- B01D 39/18: the material being cellulose or derivatives thereof ({cork or peat B01D39/1646} ; making filter paper D21F11/14)
- B01D 2239/064: The fibres being mixed
- B01D 2239/086: Binders between particles or fibres
- B01D 2239/1225: Fibre length
- B01D 2239/1233: Fibre diameter
- B01D 2239/1291: Other parameters
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)

## Abstract

High efficiency and high capacity glass-free filtration media include a blend of synthetic non-fibrillated staple fibers and fibrillated cellulosic staple fibers, wherein the fibrillated cellulosic fibers are present in the media in an amount to achieve an overall filtration efficiency at 4 microns of 95% or higher and a ratio of filtration capacity to media caliper of 0.5 mg/in2/mils and greater. The filtration media is made by forming a wet laid sheet from a fibrous slurry blend of the synthetic non-fibrillated staple fibers and fibrillated cellulosic staple fibers, followed by drying the sheet to obtain the filtration media. Optionally, the filtration media may be provided with a resin binder and may be grooved and/or pleated.

## Claims

### Claim 1

A method of making filtration media comprising:
(a) forming a wet laid sheet from a fibrous slurry comprised of a blend of synthetic non-fibrillated staple fibers and fibrillated cellulosic staple fibers, and
(b) drying the sheet to obtain the filtration media, wherein
the fibrillated cellulosic fibers are present in the filtration media in an amount to achieve an overall filtration efficiency at 4 microns of about 95% or higher and a ratio of filtration capacity to media caliper of 0.5 mg/in2/mils and greater.

### Claim 2 (depends on 1)

The method of claim 1, wherein the synthetic non-fibrillated stable fibers are formed of a thermoplastic polymer selected from the group consisting of polyesters, polyalkylenes, poyacrylonitriles, and polyamides.

### Claim 3 (depends on 1)

The method of claim 1, wherein the synthetic staple fibers are microfibers having an average fiber diameter of less than about 10 microns and an average length of less than about 25 millimeters.

### Claim 4 (depends on 3)

The method of claim 3, wherein the synthetic staple fibers are polyethylene terephthalate microfibers.

### Claim 5 (depends on 4)

The method of claim 4, wherein the polyethylene terephthalate microfibers are the water-washed residue of water non-dispersible sulfopolyester fibers having a glass transition temperature (Tg) of at least 25° C., the sulfopolyester comprising (i) about 50 to about 96 mole % of one or more residues of isophthalic acid or terephthalic acid; (ii) about 4 to about 30 mole %, based on the total acid residues, of a residue of sodiosulfoisophthalic acid; (iii) one or more diol residues wherein at least 25 mole %, based on the total diol residues, is a poly(ethylene glycol) having a structure H—(OCH2—CH2)n—OH, wherein n is an integer in the range of 2 to about 500; and (iv) 0 to about 20 mole %, based on the total repeating unites, of residues of a branching monomer having 3 or more hydroxyl, and/or carboxyl functional groups

### Claim 6 (depends on 1)

The method of claim 1, wherein the synthetic staple fibers are present in an amount between about 50 wt. % to about 99.5 wt. % ODW.

### Claim 7 (depends on 1)

The method of claim 1, wherein the fibrillated cellulosic staple fibers comprise fibrillated lyocell nanofibers.

### Claim 8 (depends on 7)

The method of claim 7, wherein the fibrillated lyocell nanofibers are present in an amount of between about 0.5 to about 50 wt. % ODW.

### Claim 9 (depends on 8)

The method of claim 8, wherein the media has a basis weight of between about 15 gsm to about 300 gsm.

### Claim 10 (depends on 1)

The method of claim 1, wherein the fibrillated cellulosic staple fibers possess a Canadian Standard Freeness (CSF) of about 300 mL or less.

### Claim 11 (depends on 1)

The method of claim 1, wherein
the synthetic staple fibers are polyethylene terephthalate microfibers having an average fiber diameter of less than about 10 microns and an average length of less than about 25 millimeters which are present in an amount of between about 50 wt. % to about 99.5 wt. % ODW, and wherein
the fibrillated cellulosic staple fibers are fibrillated lyocell fibers having a Canadian Standard Freeness (CSF) of about 300 mL or less which are present in an amount of at least about 0.5 to about 50 wt. % ODW.

### Claim 12 (depends on 1)

The method of claim 1, wherein the fibrillated cellulosic fibers have an average diameter of about 1000 nanometers or less and an average length between about 1 mm to about 8 mm.

### Claim 13 (depends on 1)

The method of claim 1, further comprising blending natural wood pulp with the synthetic non-fibrillated staple fibers and fibrillated cellulosic staple fibers of the fibrous slurry.

### Claim 14 (depends on 13)

The method of claim 13, wherein the natural wood pulp is present in an amount of about 25 wt. % ODW or less.

### Claim 15 (depends on 14)

The method of claim 14, wherein the natural wood pulp is present in an amount of about 20 wt. % ODW or less.

### Claim 16 (depends on 1)

The method of claim 1, further comprising applying at least one resin binder to the filtration media.

### Claim 17 (depends on 16)

The filtration media of claim 16, wherein the resin binder is at least one selected from the group consisting of styrene acrylic, acrylic, polyethylene vinyl chloride, styrene butadiene rubber, polystyrene acrylate, polyacrylates, polyvinyl chloride, polynitriles, polyvinyl acetate, polyvinyl alcohol derivates, starch polymers, epoxy, phenolics and combinations thereof.

### Claim 18 (depends on 16)

The method of claim 16, wherein the resin binder is present in an amount of between about 2 to about 50 wt. % SDC.

### Claim 19 (depends on 1)

The method of claim 1, which further comprises blending with the fibrous slurry at least one additive selected from the group consisting of wet strength additives, optical brighteners, fiber retention agents, colorants, fuel-water separation aides.

### Claim 20 (depends on 1)

The method of claim 1, further comprising forming longitudinally extending and latitudinally separated grooves in the filtration media.

### Claim 21 (depends on 1)

The method of claim 1, further comprising laminating at least one additional filtration media layer to the filtration media.

### Claim 22 (depends on 1)

The method of claim 1, further comprising pleating the filtration media.

### Claim 23 (depends on 22)

The method of claim 22, further comprising co-pleating at least one supporting layer with the filtration media.

### Claim 24 (depends on 23)

The method of claim 23, wherein the supporting layer is a wire mesh layer.

### Claim 25

A method of making high efficiency and high capacity glass-free filtration media comprising:
(a) forming a wet laid sheet from a fibrous slurry comprised of a blend of synthetic non-fibrillated staple microfibers and fibrillated cellulosic staple fibers, wherein
(i) the synthetic non-fibrillated staple microfibers have an average fiber diameter of less than about 10 microns and an average fiber length of less than about 25 millimeters and are formed of a thermoplastic polymer selected from the group consisting of polyesters, polyalkylenes, polyacrylonitriles, and polyamides, and wherein
(ii) the fibrillated cellulosic fibers exhibit a Canadian Standard Freeness (CSF) of about 300 mL or less and are present in the media in an amount to achieve an overall filtration efficiency at 4 microns of about 95% or higher and a ratio of filtration capacity to media caliper of 0.5 mg/in2/mils and greater; and
(b) drying the sheet to obtain the filtration media.